Method for fixating sludges and soils contaminated with mercury and other heavy metals

Assignee: ADA Technologies, Inc.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 6,911,570
App. No.
09/997,932
Granted
Jun 28, 2005
Kind
B2
Abstract

The invention relates to a method, composition and apparatus for stabilizing mercury and other heavy metals present in a particulate material such that the metals will not leach from the particulate material. The method generally involves the application of a metal reagent, a sulfur-containing compound, and the addition of oxygen to the particulate material, either through agitation, sparging or the addition of an oxygen-containing compound.

Claims (134)

1. A method for stabilizing metals an a particulate material comprising the steps of:

(a) contacting a metal reagent with the particulate material, said particulate material having a solids content of greater than about seventy-five weight percent;

(b) contacting a sulfur-containing compound with the particulate material; and

(c) agitating the particulate material to entrain oxygen in the particulate material, wherein the metal reagent is selected from the group consisting of metal based elements from Group 1B, Group 2B, Group 4B, Group 4A and combinations thereof of the Periodic Table of Elements.

2. A method according to claim 1 wherein the metals in the particulate material that are to be stabilized are selected from the group consisting of mercury, arsenic, lead, zinc, barium, cadmium, chromium, selenium, silver and mixtures thereof.

3. A method according to claim 1 wherein the particulate material has a mercury content of greater than about 260 ppm.

4. A method according to claim 1 wherein the particulate material is soil and further comprising the additional step of adding a dispersing agent to the soil.

5. A method according to claim 1 comprising the additional step of treating the metal reagent with an activator.

6. A method according to claim 1 comprising the additional step of adding an iron-containing compound to the particulate material to react with excess sulfides in the particulate material.

7. A method according to claim 1 wherein the sulfur-containing compound is a dimethylthiolcarbamate, diethylthiolcarbamate, sulfide, polysulfide or mixtures thereof.

8. A method according to claim 1 wherein the metal reagent is selected from the group consisting of zinc, tin, copper, titanium, lead and mixtures thereof.

9. A method according to claim 1 wherein the metal reagent is tin.

10. A method according to claim 5 wherein the activator is a mineral containing acid.

11. A method according to claim 5 wherein the activator is a sulfur-containing acid.

12. A method according to claim 5 wherein the activator is selected from the group consisting of sulfamic acid, sulfamidic acid, sulfonic acid, sulfinic acid, sulfenic acid, and mixtures thereof.

13. A method according to claim 5 wherein the activator is sulfamic acid.

14. A method according to claim 6 wherein a pH level of the particulate material is in a range of approximately pH 4 to pH 8.

15. A method according to claim 14 wherein the pH level of the particulate material is raised following the addition of the sulfur-containing compound.

16. A method according to claim 15 wherein the pH level of the particulate material is approximately neutral following the addition of the iron-containing compound.

17. A method according to claim 1 wherein approximately 0.4 to 2.0 weight percent of the metal reagent is added per kilogram of particulate material.

18. A method according to claim 1 wherein the sulfur-containing compound is added in an amount ranging from about 1.0 mole to about 2.0 mole of sulfur-containing compound per mole of mercury for a metals concentration in the range of about 300 ppm of metals to about 1000 ppm of metals.

19. A method according to claim 1 wherein the sulfur-containing compound is added in the an amount ranging from about 2.0 mole to about 3.0 mole of sulfur-containing compound per mole of mercury for a metals concentration in the range of about 1000 ppm of metals to about 3000 ppm of metals.

20. A method according to claim 1 wherein the particulate material is selected from the group consisting of soil, sand, dirt, sludge, solid wastes and mixtures thereof.

21. A method according to claim 6 wherein the iron-containing compound is selected from the group consisting of elemental iron, ferric chloride, ferric sulfate, ferrous sulfate and mixtures thereof.

22. A method according to claim 4 wherein the dispersing agent is a surfactant.

23. A method according to claim 4 wherein the dispersing agent is a detergent.

24. A method for stabilizing metals in a particulate material comprising the steps of:

a) treating a metal reagent with an activator;

b) adding a dispersing agent to the particulate material;

c) adding a metal reagent to the particulate material, said particulate material having a solids content of greater than about seventy-five weight percent;

d) adding a sulfur-containing compound to the particulate material;

e) agitating the particulate material to entrain oxygen in the particulate material;

f) adding an iron-containing compound to the particulate material to react with excess sulfides in the particulate material.

25. A method according to claim 24 wherein the metals in the particulate material that are to be stabilized are selected from the group consisting of mercury, arsenic, lead, zinc, barium, cadmium, chromium, selenium, silver and mixtures thereof.

26. A method according to claim 24 wherein the particulate material has a mercury content of greater than about 260 ppm.

27. A method according to claim 24 wherein the sulfur-containing compound is calcium sulfate, dithiolcarbomate, dimethylcarbomate, sulfide, polysulfide or and mixtures thereof.

28. A method according to claim 24 wherein the metal reagent is selected from the group consisting of metal based elements from Group 1B, Group 2B, Group 4B, Group 4A and combinations thereof of the Periodic Table of Elements.

29. A method according to claim 24 wherein the metal reagent is selected from the group consisting of zinc, tin, copper, titanium, lead and mixtures thereof.

30. A method according to claim 24 wherein the metal reagent is tin.

31. A method according to claim 24 wherein the activator is a mineral containing acid.

32. A method according to claim 24 wherein the activator is a sulfur-containing acid.

33. A method according to claim 24 wherein the activator is selected from the group consisting of sulfamic acid, sulfamidic acid, sulfonic acid, sulfinic acid, sulfenic acid and mixtures thereof.

34. A method according to claim 24 wherein the activator is sulfamic acid.

35. A method according to claim 24 wherein a pH level of the particulate material is in a range of approximately pH 4 to pH 8.

36. A method according to claim 35 wherein the pH level of the particulate material is raised following the addition of the sulfur-containing compound.

37. A method according to claim 36 wherein the pH level of the particulate material is approximately neutral following the addition of the iron-containing compound.

38. A method according to claim 24 wherein approximately 0.4 to 2.0 weight percent of the metal reagent is added per kilogram of particulate material.

39. A method according to claim 24 wherein the sulfur-containing compound is added in an amount ranging from about 1.0 mole to about 2.0 mole of sulfur-containing compound per mole of mercury for a metals concentration in the range of about 300 ppm of metals to about 1000 ppm of metals.

40. A method according to claim 24 wherein the sulfur-containing compound is added in the an amount ranging from about 2.0 mole to about 3.0 mol of sulfur-containing compound per mole of mercury for a metals concentration in the range of about 1000 ppm of metals to about 5000 ppm of metals.

41. A method according to claim 24 wherein the particulate material is selected from the group consisting of soil, sand, dirt, sludge, solid wastes and mixtures thereof.

42. A method according to claim 24 wherein the iron-containing compound is selected from the group consisting of elemental iron, ferric sulfate, ferric chloride, ferrous sulfate and mixtures thereof.

43. A method according to claim 24 wherein the dispersing agent is a surfactant.

44. A method according to claim 24 wherein the dispersing agent is a detergent.

45. A method for stabilizing metals in a particulate compound comprising the steps of:

(a) adding a metal reagent to the particulate material, said particulate material having a solids content of greater than about seventy-five weight percent;

(b) adding a sulfur-containing compound to the particulate material;

(c) impregnating the particulate material with oxygen;

(d) agitating the particulate material to entrain oxygen in the particulate material; and,

(e) adding an iron-containing compound to the particulate to remove excess sulfides from the particulate material.

46. A method for stabilizing metals in a particulate compound comprising the steps of:

(a) adding a metal reagent to the particulate material, said particulate material having a solid content of greater than about seventy-five weight percent;

(b) adding a sulfur-containing compound to the particulate material;

(c) agitating the particulate material to entrain oxygen in the particulate material; and,

(d) adding an iron-containing compound to the particulate to remove excess sulfides from the particulate material.

47. A method for stabilizing metals in a particulate material comprising the steps of:

(a) adding a dispersing agent to the particulate material;

(b) adding a metal reagent to the particulate material, said particulate material having a solids content of greater than about seventy-five weight percent;

(c) adding a sulfur-containing compound to the particulate material;

(d) agitating the particulate material to entrain oxygen in the particulate material; and,

(e) adding an iron-containing compound to the particulate material to remove excess sulfides from the particulate material.

48. A method for stabilizing metals in a particulate material comprising the steps of:

(a) adding a metal reagent to the particulate material, said particulate material having a solids content of greater than about seventy-five weight percent;

(b) adding a sulfur-containing compound to the particulate material; and,

(c) impregnating the particulate material with oxygen, wherein the metal reagent is selected from the group consisting of metal based elements from Group 1B, Group 2B, Group 4B, Group 4A and combinations thereof of Periodic Table of Elements.

49. A method for stabilizing metals in a particulate material comprising the steps of:

(a) contacting a metal reagent with the particulate material, said particulate material having a solids content of greater than about seventy-five weight percent;

(b) contacting a sulfur-containing compound with the particulate material;

(c) agitating the particulate material to entrain oxygen in the particulate material; and

(d) adding an iron-containing compound to the particulate material to react with excess sulfides in the particulate material.

50. A method according to claim 49 wherein a pH level of the particulate material is in a range of approximately pH 4 to pH 8.

51. A method according to claim 50 wherein the pH level of the particulate material is raised following the addition of the sulfur-containing compound.

52. A method according to claim 49 wherein the pH level of the particulate material is approximately neutral following the addition of the iron-containing compound.

53. A method according to claim 49 wherein the iron-containing compound is selected from the group consisting of elemental iron, ferric chloride, ferric sulfate, ferrous sulfate and mixtures thereof.

54. A method for stabilizing metals in a particulate material comprising the steps of:

(a) contacting a metal reagent with the particulate material, said particulate material having a solids content of greater than about seventy-five weight percent;

(b) contacting a sulfur-containing compound with the particulate material; and

(c) agitating the particulate material to entrain oxygen in the particulate material, wherein the metal reagent is selected from the group consisting of zinc, tin, copper, titanium, lead and mixtures thereof.

55. A method for stabilizing metals in a particulate material comprising the steps of:

(a) contacting a metal reagent with the particulate material, said particulate material having a solids content of greater than about seventy-five weight percent;

(b) contacting a sulfur-containing compound with the particulate material; and

(c) agitating the particulate material to entrain oxygen in the particulate material, wherein the metal reagent is tin.

56. A method for stabilizing metals in a particulate material comprising the steps of:

(a) contacting a metal reagent with the particulate material, said particulate material having a solids content of greater than about seventy-five weight percent;

(b) contacting a sulfur-containing compound with the particulate material;

(c) agitating the particulate material to entrain oxygen in the particulate material; and

(d) treating the metal reagent with an activator, wherein the activator is selected from the group consisting of sulfamic acid, sulfamidic acid, sulfonic acid, sulfinic acid, sulfenic acid, and mixtures thereof.

57. A method for stabilizing metals in a particulate material comprising the steps of:

(a) contacting a metal reagent with the particulate material, said particulate material having a solids content of greater than about seventy-five weight percent;

(b) contacting a sulfur-containing compound with the particulate material;

(c) agitating the particulate material to entrain oxygen in the particulate material; and

(d) treating the metal reagent with an activator, wherein the activator is sulfamic acid.

58. A method for stabilizing metals in a particulate material comprising the steps of:

(a) contacting a metal reagent with the particulate material, said particulate material having a solids content of greater than about seventy-five weight percent;

(b) contacting a sulfur-containing compound with the particulate material;

(c) agitating the particulate material to entrain oxygen in the particulate material, wherein the particulate material is soil; and

(d) adding a dispersing agent to the soil wherein the dispersing agent is a surfactant.

59. A method for stabilizing metals in a particulate material comprising the steps of:

(a) contacting a metal reagent with the particulate material, said particulate material having a solids content of greater than about seventy-five weight percent;

(b) contacting a sulfur-containing compound with the particulate material;

(c) agitating the particulate material to entrain oxygen in the particulate material, wherein the particulate material is soil; and

(d) adding a dispersing agent to the soil, wherein the dispersing agent is a detergent.

60. A method according to claim 48 wherein the particulate material is impregnated with oxygen by adding an oxygen-containing compound to the particulate material.

61. A method according to claim 48 wherein the metals in the particulate material that are to be stabilized are selected from the group consisting of mercury, arsenic, lead, zinc, barium, cadmium, chromium, selenium, silver and mixtures thereof.

62. A method according to claim 48 wherein the particulate material has a mercury content of greater than about 260 ppm.

63. A method according to claim 48 wherein the particulate material is soil and further comprising the additional step of adding a dispersing agent to the soil.

64. A method according to claim 48 comprising the additional step of treating the metal reagent with an activator.

65. A method according to claim 48 , comprising the additional step of adding an iron-containing compound to the particulate material to react with excess sulfides in the particulate material.

66. A method according to claim 48 wherein the sulfur-containing compound is a dimethylthiolcarbamate, diethylthiolcarbamate, sulfide, polysulfide or mixtures thereof.

67. A method according to claim 48 wherein the metal reagent is selected from the group consisting of zinc, tin, copper, titanium, lead and mixtures thereof.

68. A method according to claim 48 wherein the metal reagent is tin.

69. A method according to claim 64 wherein the activator is a mineral containing acid.

70. A method according to claim 64 wherein the activator is a sulfur-containing acid.

71. A method according to claim 64 wherein the activator is selected from the group consisting of sulfamic acid, sulfamidic acid, sulfonic acid, sulfinic acid, sulfenic acid, and mixtures thereof.

72. A method according to claim 64 wherein the activator is sulfamic acid.

73. A method according to claim 48 wherein a pH level of the particulate material is in a range of approximately pH 4 to pH 8.

74. A method according to claim 73 wherein the pH level of the particulate material is raised following the addition of the sulfur-containing compound.

75. A method according to claim 65 wherein the pH level of the particulate material is approximately neutral following the addition of the iron-containing compound.

76. A method according to claim 48 wherein approximately 0.4 to 2.0 weight percent of the metal reagent is added per kilogram of particulate material.

77. A method according to claim 48 wherein the sulfur-containing compound is added in an amount ranging from about 1.0 mole to about 2.0 mole of sulfur-containing compound per mole of mercury for a metals concentration in the range of about 300 ppm of metals to about 1000 ppm of metals.

78. A method according to claim 48 wherein the sulfur-containing compound is added in the an amount ranging from about 2.0 mole to about 3.0 mole of sulfur-containing compound per mole of mercury for a metals concentration in the range of about 1000 ppm of metals to about 3000 ppm of metals.

79. A method according to claim 48 wherein the particulate material is selected from the group consisting of soil, sand, dirt, sludge, solid wastes and mixtures thereof.

80. A method according to claim 65 wherein the iron-containing compound is selected from the group consisting of elemental iron, ferric chloride, ferric sulfate, ferrous sulfate and mixtures thereof.

81. A method according to claim 63 wherein the dispersing agent is a surfactant.

82. A method according to claim 63 wherein the dispersing agent is a detergent.

Assignments (4)
NOTICE OF GRANT OF SECURITY INTEREST IN PATENTS Recorded Nov 15, 2011
From: PERMA-FIX ENVIRONMENTAL SERVICES, INC.
To: PNC BANK, NATIONAL ASSOCIATION, AS AGENT
Reel/Frame 027229/0355 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 20, 2011
From: MERCURY CONTROL TECHNOLOGIES, LLC
To: PERMA-FIX ENVIRONMENTAL SERVICES, INC.
Reel/Frame 026157/0839 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 7, 2011
From: ADA TECHNOLOGIES, INC.
To: MERCURY CONTROL TECHNOLOGIES, LLC
Reel/Frame 026089/0891 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 28, 2001
From: BRODERICK, THOMAS E.; ROTH, RACHEL L.; CARLSON, ALLAN L.
To: ADA TECHNOLOGIES, INC.
Reel/Frame 012339/0049 →
Continuity (2)
Provisional Application 6025348200 · Nov 28, 2000
Related Publication 20020106317A1 · Aug 8, 2002