IP Library › Granted Patent US 7,183,145
Granted Patent B2
US 7,183,145 · App. 11/148,400 · Granted Feb 27, 2007

Semiconductor device and manufacturing method thereof

Assignee: Semiconductor Energy Laboratory Co., Ltd.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,183,145
App. No.
11/148,400
Granted
Feb 27, 2007
Kind
B2
Abstract

In a crystallization process of an amorphous semiconductor film, a first polycrystalline semiconductor film, in which amorphous regions are dotted within the continuous crystal region, is obtained by performing heat treatment after introducing a metallic element which promotes crystallization on the amorphous semiconductor film. At this point, the amorphous regions are kept within a predetermined range. A laser beam having a wave length region, which can give more energy to the amorphous region than to the crystal region, is irradiated to the first polycrystalline semiconductor film, it is possible to crystallize the amorphous region without destroying the crystal region. If a TFT is manufactured based on a second polycrystalline semiconductor film, which is obtained through the above-mentioned crystallization processes, the TFT with high electric characteristics and less fluctuation can be obtained.

Claims (23)

1. A method of manufacturing a semiconductor device, comprising:

a first step of introducing a metallic element for promoting crystallization of an amorphous semiconductor film introducing into the amorphous semiconductor film;

a second step of partially crystallizing the amorphous semiconductor film by heat treatment to form a first polycrystalline semiconductor film; and

a third step of irradiating a laser beam with a wave length from 360 to 650 nm to the first polycrystalline semiconductor film to form a second polycrystalline semiconductor film,

wherein the first polycrystalline semiconductor film is crystallized in the range from 92 to 99% in a region which becomes an active layer of a TFT.

2. A method of manufacturing a semiconductor device, comprising:

a first step of introducing a metallic element for promoting crystallization of an amorphous semiconductor film introducing into the amorphous semiconductor film;

a second step of partially crystallizing the amorphous semiconductor film by heat treatment to form a first polycrystalline semiconductor film; and

a third step of irradiating a laser beam with a wave length from 360 to 650 nm to the first polycrystalline semiconductor film to form a second polycrystalline semiconductor film,

wherein, in the first polycrystalline semiconductor film, the total area of amorphous regions in a region which becomes an active layer of a TFT is set from 1 to 8% of an area of the region which becomes the active layer of the TFT.

3. A method of manufacturing a semiconductor device according to claim 1 , wherein the metallic element is one kind or plural kinds of elements selected from the group consisting of Ni, Pd, Pt, Cu, Ag, Au, Al, In, Sn, Pb, P, As and Sb.

4. A method of manufacturing a semiconductor device according to claim 2 , wherein the metallic element is one kind or plural kinds of elements selected from the group consisting of Ni, Pd, Pt, Cu, Ag, Au, Al, In, Sn, Pb, P, As and Sb.

5. A method of manufacturing a semiconductor device according to claim 1 , wherein the laser beam is one kind selected from the group consisting of a second harmonic of a YAG laser, a second harmonic of a glass laser, an Ar laser, a second harmonic of a YLF laser, and a second harmonic of a YVO 4 laser.

6. A method of manufacturing a semiconductor device according to claim 2 , wherein the laser beam is one kind selected from the group consisting of a second harmonic of a YAG laser, a second harmonic of a glass laser, an Ar laser, a second harmonic of a YLF laser, and a second harmonic of a YVO 4 laser.

7. A method of manufacturing a semiconductor device according to claim 1 , wherein the semiconductor device is a liquid crystal display device or a light-emitting device.

8. A method of manufacturing a semiconductor device according to claim 2 , wherein the semiconductor device is a liquid crystal display device or a light-emitting device.

9. A method of manufacturing a semiconductor device according to claim 1 , wherein the semiconductor device is a portable telephone, a video camera, a digital camera, a projector, a goggle type display, a personal computer, a DVD player, an electronic book, or a portable information terminal.

10. A method of manufacturing a semiconductor device according to claim 2 , wherein the semiconductor device is a portable telephone, a video camera, a digital camera, a projector, a goggle type display, a personal computer, a DVD player, an electronic book, or a portable information terminal.

11. A method of manufacturing a semiconductor device according to claim 1 , wherein the laser beam has a wave length from 400 to 600 nm.

12. A method of manufacturing a semiconductor device according to claim 2 , wherein the laser beam has a wave length from 400 to 600 nm.

13. A method of manufacturing a semiconductor device according to claim 2 , wherein, in the first polycrystalline semiconductor film, the total area of amorphous regions in a region which becomes an active layer of a TFT is set from 1 to 6% of an area of the region which becomes the active layer of the TFT.

14. A method of manufacturing a semiconductor device according to claim 1 , wherein the second polycrystalline semiconductor film formed is crystallized in equal to or greater than 99% of the region which becomes the active layer of the TFT.

15. A method of manufacturing a semiconductor device according to claim 2 , wherein, in the second polycrystalline semiconductor film, the total area of amorphous regions in the region which becomes the active layer of the TFT is set equal to or less than 1% of the area of the region which becomes the active layer of the TFT.

Assignments (2)
SECURITY INTEREST Recorded Dec 1, 2021
From: TEKNI-PLEX, INC.
To: CREDIT SUISSE AG, CAYMAN ISLANDS BRANCH
Reel/Frame 058256/0186 →
SECURITY INTEREST Recorded Dec 1, 2021
From: TEKNI-PLEX, INC.
To: BMO HARRIS BANK N.A.
Reel/Frame 058256/0199 →
Priority Claims (2)
JP 2000-063000 · Mar 8, 2000 · national
JP 2000-064186 · Mar 8, 2000 · national
Continuity (2)
Division 0980062700 · Mar 7, 2001
Related Publication 20050233557A1 · Oct 20, 2005