IP Library › Granted Patent US 9,010,274
Granted Patent B2
US 9,010,274 · App. 13/443,695 · Granted Apr 21, 2015

Lightweight clumping animal litter and method thereof

Inventors: Ahmed Drief (Pleasanton, CA); David M. Gall (Pleasanton, CA); Elisa Calimano (Pleasanton, CA); Aram Garabedian (Pleasanton, CA); Dennis B. Jenkins (Pleasanton, CA); Roger V. Lee (Pleasanton, CA); Carrier Ripberger (Pleasanton, CA); Sean Gooby (Pleasanton, CA)
Assignee: The Clorox Company
A01K1/0154A01K1/0155
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,010,274
App. No.
13/443,695
Granted
Apr 21, 2015
Kind
B2
Abstract

Animal litter having up to a sixty percent reduction in bulk density can be produced by combining flat-shaped cellulosic materials and sodium bentonite clay. Not only is the resulting litter lighter, but it also maintains a high clump strength as compared to clay-based animal litters that contain greater than ninety percent by weight sodium bentonite clay.

Claims (28)

1. An animal litter comprising a dry blend of:

(i) composite particles comprising

(a) a flat-shaped cellulosic material component having a mean particle size ranging from 0.2-3 mm and having an aspect ratio of at least 2;

(b) a powdered sodium bentonite component having a mean particle size less than 0.25 mm, wherein the ratio of cellulosic material to sodium bentonite ranges from 1:4 to 4:1 and wherein the mean particle size of the composite particles ranges from 0.4-4 mm;

(c) optionally a spacer material, and

(d) optionally a binder;

(ii) granular sodium bentonite having a mean particle size in the range of 0.4-2 mm;

(iii) optionally granular calcium bentonite having a mean particle size in the range of 0.4-2 mm; and

(iv) at least 0.2% by weight powdered kaolinite having a particle size less than 0.25 mm; and

wherein the animal litter has a clump strength of at least 80% and is substantially free of a static charge.

2. The animal litter recited in claim 1 having a brightness of at least 52 as evaluated using a Minolta Chroma Meter CR-300.

3. The animal litter recited in claim 1 having a clump strength of at least 90% and a bulk density reduction of at least 25% as compared to pure sodium bentonite animal litter.

4. The animal litter recited in claim 1 having a clump strength of at least 95% and a bulk density reduction of at least 25% as compared to pure sodium bentonite animal litter.

5. The animal litter recited in claim 1 , wherein the spacer material is selected from the group consisting of PAC, silica gel, zeolite, calcium bentonite, limestone, gypsum, kaolinite, silica, hydrophobic silica, flow aid such as talk, starches and combinations thereof.

6. The animal litter recited in claim 1 , wherein the binder is selected from the group consisting of guar gum, modified starch, natural hydro-coloids, alginates, acrylates, poly vinyl acetate and combinations thereof.

7. The animal litter recited in claim 1 , wherein the binder is guar gum.

8. The animal litter recited in claim 1 , wherein the spacer material is powder activated carbon having a particle size less than 0.25 mm.

9. The animal litter recited in claim 1 , wherein the composite particles comprise 2 percent to 65 percent by weight of the animal litter, the granular sodium bentonite comprises between 35 percent to 98 percent by weight of the animal litter, and the granular calcium bentonite comprises between 0 to 15 percent by weight of the animal litter.

10. An animal litter comprising a dry blend of:

(i) 2 percent to 65 percent by weight composite particles comprising

(a) a flat-shaped cellulosic material component having a mean particle size ranging from 0.2-3 mm and having an aspect ratio of at least 2;

(b) a powdered sodium bentonite component having a mean particle size less than 0.25 mm, wherein the ratio of cellulosic material to sodium bentonite ranges from 1:4 to 4:1 and wherein the mean particle size of the composite particles ranges from 0.4-4 mm;

(c) a spacer material comprising powder activated carbon having a particle size less than 0.25 mm;

(ii) 35 percent to 98 percent by weight granular sodium bentonite having a mean particle size in the range of 0.4-2 mm;

(iii) 0 to 15 percent by weight granular calcium bentonite having a mean particle size in the range of 0.4-2 mm; and

(iv) at least 0.2% by weight powdered kaolinite having a particle size less than 0.25 mm; and wherein the animal litter has a clump strength of at least 80% and is substantially free of a static charge.

11. The animal litter recited in claim 10 , wherein the composite particles comprise 50-70 percent by weight powdered sodium bentonite, 30-50 percent by weight cellulosic particles and 0.3-1.5 percent powder activated carbon.

12. The animal litter recited in claim 10 , wherein the animal litter has a percent reflectance value as measured by compact tristimulus color analyzer of at least 52.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 10, 2012
From: DRIEF, AHMED; GALL, DAVID M.; CALIMANO, ELISA; GARABEDIAN, JR., ARAM; LEE, ROGER V.; RIPBERGER, CARRIER; GOOBY, SEAN; JENKINS, DENNIS B.
To: THE CLOROX COMPANY
Reel/Frame 028022/0448 →
Continuity (2)
Provisional Application 61474970 · Apr 13, 2011
Related Publication 20120260860A1 · Oct 18, 2012