Selective catalytic reduction system and process for control of NO
An exhaust gas treatment process, apparatus, and system for reducing the concentration of NOx, CO and hydrocarbons in a gas stream, such as an exhaust stream ( 29 ), via selective catalytic reduction with ammonia is provided. The process, apparatus and system include a catalytic bed ( 32 ) having a reducing only catalyst portion ( 34 ) and a downstream reducing-plus-oxidizing portion ( 36 ). Each portion ( 34, 36 ) includes an amount of tungsten. The reducing-plus-oxidizing catalyst portion ( 36 ) advantageously includes a greater amount of tungsten than the reducing catalyst portion ( 36 ) to markedly limit ammonia salt formation.
1. A process for selective catalytic reduction of nitrogen oxides (NOx) with effective suppression of ammonia salt formation in a gas stream comprising ammonia, the NOx, SO 2 and water, the process comprising:
reducing the NOx via the ammonia by passing the gas stream over a catalytic bed comprising a reducing only catalyst portion that comprises a first amount of tungsten; and
oxidizing remaining ammonia while simultaneously further reducing NOx by passing the gas stream over a reducing-plus-oxidizing catalyst portion downstream from the reducing only catalyst portion in the catalytic bed, the reducing-plus-oxidizing catalyst portion comprising a second amount of tungsten greater than the first amount of tungsten.
2. The process of claim 1 , wherein the reducing only catalyst portion and the reducing-plus-oxidizing catalyst portion each further comprise vanadium pentoxide and titanium dioxide.
3. The process of claim 1 , wherein the reducing-plus-oxidizing catalyst portion further comprises an amount of at least one platinum group metal effective to promote oxidizing reactions.
4. The process of claim 1 , wherein the second amount of tungsten is from 2-8 wt. % of the catalytic bed greater the first amount of tungsten.
5. The process of claim 4 , wherein the second amount of tungsten is from 3-6 wt. % of the catalytic bed greater than the first amount of tungsten.
6. The process of claim 1 , wherein a total amount of the first amount of tungsten and the second amount of tungsten is from 12-38 wt. % of the catalytic bed.
7. The process of claim 1 , wherein a total amount of the tungsten in the reducing-plus-oxidizing catalyst portion is 10-16 wt. % of the catalytic bed.
8. The process of claim 1 , wherein a ratio of the reducing catalyst portion to the reducing-plus-oxidizing catalyst portion is 60:40 by vol. % of the catalytic bed.
9. The process of claim 1 , further comprising providing the reducing only catalyst portion and the reducing-plus-oxidizing portion on a common monolithic substrate.
10. The process of claim 1 , wherein the gas stream comprises from 10-25 vol. % water, 5-18 vol. % O 2 and 5-20 ppm of SO 2 .
11. The process of claim 1 , wherein the first amount of tungsten and the second amount of tungsten are provided by tungsten oxide.
12. The process according to claim 1 , further comprising installing the catalytic bed in a flow path of an exhaust gas stream of a gas turbine, wherein the exhaust gas stream includes NO x , CO, hydrocarbons, H 2 O, O 2 , and SO 2 .
13. The process according to claim 9 , further comprising installing the catalytic bed in a flow path of an exhaust gas stream of a gas turbine in an integrated gasification combined cycle (IGCC) power generation plant that synthesizes a hydrogen-containing fuel for the gas turbine.
14. A catalytic bed for selective catalytic reduction of nitrogen oxides (NOx) with effective suppression of ammonia salt formation in a gas stream comprising at least ammonia, NO x , SO 2 and water, the catalytic bed comprising:
a reducing only catalyst portion that comprises a first amount of tungsten for reducing the NO in the gas stream; and
a reducing-plus-oxidizing catalyst portion downstream from the reducing only catalyst portion in the catalytic bed for oxidizing remaining ammonia while simultaneously further reducing NO x , the reducing-plus-oxidizing catalyst portion comprising a second amount of tungsten greater than the first amount of tungsten.
15. The catalytic bed of claim 14 , wherein the reducing-plus-oxidizing portion further comprises an amount of at least one platinum group metal effective to promote oxidizing reactions, wherein the second amount of tungsten is from 2-8 by wt. % of the catalytic bed greater the first amount of tungsten.
16. The catalytic bed of claim 14 , wherein the second amount of tungsten is from 3-6 by wt. % of the catalytic bed greater the first amount of tungsten.
17. The catalytic bed of claim 16 , wherein the first amount and the second amount of tungsten are from tungsten oxide.
18. The catalytic bed of claim 14 , wherein a total amount of the first amount of tungsten and the second amount of tungsten is from 12-38 wt. % of the catalytic bed.
19. The catalytic bed of claim 14 , wherein a ratio of the reducing only catalyst portion to the reducing-plus-oxidizing portion is 60:40 by vol. % of the catalytic bed.
20. A power generating apparatus comprising
a gas turbine engine for combusting a fuel in air to produce shaft power and a flow of an exhaust gas comprising oxides of nitrogen (NOx), carbon monoxide and hydrocarbons; and
a treatment apparatus for receiving the exhaust gas prior to passing the exhaust gas to the atmosphere, the treatment apparatus comprising the catalytic bed of claim 14 .