IP Library Granted Patent US 9,138,722
Granted Patent B2
US 9,138,722 · App. 14/372,161 · Granted Sep 22, 2015

Method for producing water-absorbent resin particles

Inventors: Kenji Tanimura (Himeji, JP); Hiroki Yabuguchi (Himeji, JP); Yuichi Onoda (Himeji, JP); Masayoshi Handa (Himeji, JP)
Assignee: Sumitomo Seika Chemicals Co., Ltd.
B01J20/3085A61L15/12B01J20/262C08F2/32C08F20/06C08F120/06C08L33/02
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,138,722
App. No.
14/372,161
Granted
Sep 22, 2015
Kind
B2
Abstract

There is disclosed a method for producing water-absorbent resin particles comprising a step that includes reversed-phase suspension polymerization of a water-soluble ethylenically unsaturated monomer in a suspension containing a surfactant that comprises a surfactant that comprises a fatty acid ester of sorbitan or sorbitol, or derivative thereof, and a hydrocarbon dispersion medium. The fatty acid ester includes a lauric acid ester and at least one kind of other ester selected from the group consisting of palmitic acid esters, stearic acid esters and behenic acid esters. The proportion of the peak area for lauric acid ester is 30-60%, based on the total peak area for fatty acid esters in the GPC chromatogram obtained from the fatty acid esters, and the proportion of the total peak area for other ester is 10-50%.

Claims (4)

1. A method for producing water-absorbent resin particles, comprising a step that includes carrying out reversed-phase suspension polymerization of a water-soluble ethylenically unsaturated monomer in a suspension containing a surfactant that comprises a fatty acid ester of sorbitan, sorbitol or a derivative thereof, and a hydrocarbon dispersion medium,

wherein the fatty acid ester includes a lauric acid ester and at least one kind of other ester selected from the group consisting of palmitic acid esters, stearic acid esters and behenic acid esters, and

in a GPC chromatogram obtained from the fatty acid ester, the proportion of the peak area due to the lauric acid ester is 30-60% and the proportion of the total peak area due to the other ester is 10-50%, based on the total peak area due to the fatty acid esters.

2. The method for producing water-absorbent resin particles according to claim 1 , wherein the fatty acid ester is at least one selected from the group consisting of sorbitan fatty acid esters, polyoxyethylene sorbitan fatty acid esters, sorbitol fatty acid esters and polyoxyethylene sorbitol fatty acid esters.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 14, 2014
From: TANIMURA, KENJI; YABUGUCHI, HIROKI; ONODA, YUICHI; HANDA, MASAYOSHI
To: SUMITOMO SEIKA CHEMICALS CO., LTD.
Reel/Frame 033307/0915 →
Priority Claims (1)
JP 2012-043571 · Feb 29, 2012 · national
Continuity (1)
Related Publication 20150158015A1 · Jun 11, 2015