Biodegradable bone plates and bonding systems
The invention relates to novel internal fixation devices, such as bone plates, generally and novel craniomaxillofacial bone plates more specifically and systems for bonding the same. More specifically, the invention relates to bone plates made of a polymer blend of (poly)lactic acid and Ecoflex as well as a novel hot-melt adhesive polymer blend of the same material.
1. A method for bonding an internal fixation device to tissue, comprising:
placing an internal fixation device in contact with tissue to be fixed;
applying energy to the internal fixation device to melt at least a portion thereof;
allowing the melted portion of the internal fixation device to harden such that the internal fixation device is affixed to the tissue without the use of a secondary fixation device,
wherein the internal fixation device is a porous, bioactive plate.
2. The method of claim 1 , wherein the internal fixation device is affixed to tissue without drilling or perforating through the tissue.
3. The method of claim 1 , wherein the portion of the internal fixation device that is melted has a melting point in the range of about 50 degrees Celsius and about 300 degrees Celsius.
4. The method of claim 1 , wherein the secondary fixation device includes a screw, pin, or an additional plate.
5. The method of claim 1 , wherein the plate further comprises a first polymer in a co-continuous phase with a second polymer.
6. The method of claim 5 , wherein the first polymer is a polymer or a co-polymer that includes polylactic acid and the second polymer is a polymer or a co-polymer that includes polyester.
7. The method of claim 6 , wherein the amount of polylactic acid is in the range of about 10% to about 80%.
8. A method for bonding tissue, comprising:
melting a bioabsorbable polymer adhesive;
applying the melted bioabsorbable polymer adhesive onto at least one bone tissue segment to be fixed such that the melted polymer contacts the at least one bone tissue segment; and
affixing the at least bone tissue segment to at least one other portion of bone tissue without the use of a secondary fixation device,
wherein the bioabsorbable polymer adhesive comprises a first polymer or co-polymer in a co-continuous phase with a second polymer or co-polymer, and
wherein the first polymer or co-polymer includes polylactic acid and the second polymer or co-polymer includes polyester.
9. The method of claim 8 , wherein the at least one bone tissue segment and the at least one other portion of bone tissue are bonded together without drilling or perforating through either of the at least one bone tissue segment and the at least one other portion of bone tissue.
10. The method of claim 8 , wherein the bioabsorbable polymer is part of a bone plate, and the step of melting a bioabsorbable polymer adhesive comprises melting at least a portion of the bone plate.
11. The method of claim 10 , wherein the secondary fixation device includes a screw, pin, or an additional bone plate.
12. The method of claim 8 , wherein the bioabsorbable polymer adhesive has a melting point in the range of about 50 degrees Celsius and about 300 degrees Celsius.
13. The method of claim 8 , wherein the amount of polylactic acid is in the range of about 10% to about 80%.
14. A method for bonding an internal fixation device to tissue, comprising:
placing an internal fixation device in contact with tissue to be fixed;
applying energy to the internal fixation device to melt at least a portion thereof;
allowing the melted portion of the internal fixation device to harden such that the internal fixation device is affixed to the tissue without drilling or perforating through the tissue,
wherein the internal fixation device is a porous, bioactive plate.
15. The method of claim 14 , wherein the portion of the internal fixation device that is melted has a melting point in the range of about 50 degrees Celsius and about 300 degrees Celsius.
16. The method of claim 14 , wherein the plate further comprises a first polymer in a co-continuous phase with a second polymer.
17. The method of claim 16 , wherein the first polymer is a polymer or a co-polymer that includes polylactic acid and the second polymer is a polymer or a co-polymer that includes polyester.
18. The method of claim 17 , wherein the amount of polylactic acid is in the range of about 10% to about 80%.