IP Library Granted Patent US 9,181,698
Granted Patent B2
US 9,181,698 · App. 14/151,973 · Granted Nov 10, 2015

Method of producing a building panel and a building panel

Inventors: Darko Pervan (Viken, SE); Niclas Håkansson (Viken, SE); Hans Persson (Perstorp, SE); Marcus Bergelin (Lerberget, SE)
Assignees: Valinge Innovation AB; Valinge Flooring Technology AB
E04C2/246B32B37/0038E04C2/40B32B2038/0056B32B2038/0076B32B2038/166B32B2317/125B32B2317/16B32B2471/00B32B2607/00Y10T428/31964
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,181,698
App. No.
14/151,973
Granted
Nov 10, 2015
Kind
B2
Abstract

A method of producing a building panel ( 1 ), including: providing a core ( 2 ), applying a balancing layer ( 6 ) having a first moisture content on a first surface ( 3 ) of the core ( 2 ), the balancing layer ( 6 ) comprising a sheet impregnated with a thermosetting binder, applying a surface layer ( 12 ) having a second moisture content on a second surface ( 4 ) of the core ( 2 ), the surface layer ( 12 ) comprising a thermosetting binder, adjusting the first moisture content of the balancing layer ( 6 ) such that the first moisture content of the balancing layer ( 6 ) is higher than the second moisture content of the surface layer ( 12 ) prior to curing, and curing the surface layer ( 12 ) and the balancing layer ( 6 ) by applying heat and pressure. Also, a semi-finished product adapted to be cured for forming a building panel ( 1 ).

Claims (20)

1. A method of producing a building panel, comprising:

providing a core,

applying a balancing layer on a first surface of the core, wherein the balancing layer has a first moisture content and comprises a sheet impregnated with a thermosetting binder,

applying a surface layer on a second surface of the core, wherein the surface layer has a second moisture content and comprises a thermosetting binder,

adjusting the first moisture content of the balancing layer such that the first moisture content of the balancing layer is higher than the second moisture content of the surface layer prior to curing by applying heat and pressure, and

curing the surface layer and the balancing layer by applying heat and pressure.

2. A method according to claim 1 , wherein the step of adjusting the first moisture content of the balancing layer comprises applying water or steam to the first surface of the core prior to applying the balancing layer.

3. A method according to claim 1 , wherein the step of adjusting the first moisture content of the balancing layer comprises applying water or steam to the balancing layer.

4. A method according to claim 1 , wherein the first moisture content of the balancing layer exceeds 10% of the total weight of the balancing layer prior to curing.

5. A method according to claim 1 , wherein the thermosetting binder is of the same type in the surface layer and in the balancing layer.

6. A method according to claim 1 , wherein the thermosetting binder of the surface layer and/or the balancing layer is melamine formaldehyde resin.

7. A method according to claim 1 , wherein the sheet is a paper sheet.

8. A method according to claim 1 , wherein the surface layer comprises a décor paper.

9. A method according to claim 1 , wherein the surface layer comprises a layer comprising a thermosetting binder and at least one pigment.

10. A method according to claim 1 , wherein the amount of the thermosetting binder in the balancing layer is lower than the amount of the thermosetting binder in the surface layer.

11. A method according to claim 2 , wherein the step of adjusting the first moisture content of the balancing layer comprises applying water or steam to the balancing layer.

12. A method according to claim 1 , wherein the first moisture content of the balancing layer exceeds 20% of the total weight of the balancing layer prior to curing.

13. A method according to claim 1 , wherein the first moisture content of the balancing layer exceeds 30% of the total weight of the balancing layer prior to curing.

14. A method according to claim 1 , wherein the surface layer comprises a resin impregnated décor paper.

15. A method according to claim 1 , wherein the surface layer comprises a melamine formaldehyde impregnated décor paper.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 27, 2016
From: VÄLINGE FLOORING TECHNOLOGY AB
To: VÄLINGE INNOVATION AB
Reel/Frame 038394/0401 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 25, 2015
From: BERGELIN, MARCUS
To: VALINGE INNOVATION AB; VALINGE FLOORING TECHNOLOGY AB
Reel/Frame 035906/0925 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 11, 2014
From: PERVAN, DARKO; HAKANSSON, NICLAS; PERSSON, HANS
To: VALINGE FLOORING TECHNOLOGY AB; VALINGE INNOVATION AB
Reel/Frame 032660/0222 →
Continuity (2)
Provisional Application 61751393 · Jan 11, 2013
Related Publication 20140199558A1 · Jul 17, 2014