IP Library Granted Patent US 9,506,202
Granted Patent B2
US 9,506,202 · App. 14/537,055 · Granted Nov 29, 2016

Furnish pretreatment to improve paper strength aid performance in papermaking

Inventors: Yulin Zhao (Shanghai, CN); Jun Li (Shanghai, CN); Qing Long Rao (Shanghai, CN); Weiguo Cheng (Naperville, IL)
Assignee: NALCO Company
D21H21/20D21H11/14D21H17/28D21H17/375D21H17/45D21H17/72D21H21/18D21H23/14
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,506,202
App. No.
14/537,055
Granted
Nov 29, 2016
Kind
B2
Abstract

The invention is directed towards methods, compositions, and apparatus for increasing the strength of paper made out of a furnish having a large proportion of OCC. The method involves the following steps: 1) Providing a paper furnish having a large amount of OCC in it, 2) adding strength promoter to the furnish prior to adding a strength agent to the furnish, 3) adding a strength agent to the furnish, and 4) making a paper product from the furnish. This method allows cheap OCC material to be used in a papermaking process without the quality problems that the anionic trash in OCC typically causes. Thus paper products having low costs and high quality can be produced.

Claims (7)

1. A method of increasing the strength of a paper product, the method comprising the steps of: a) adding a strength promoter to a furnish prior to adding a strength agent to the furnish, the strength promoter comprising a polymer having cationic monomer repeating structural units containing a carbonyl functional group, the fibers in the furnish made up of at least 10% fibers containing anionic trash, b) adding the strength agent to the furnish, wherein the strength agent is glyoxalated polyacrylamide, and c) making a paper product out of the furnish according to a papermaking process, wherein the strength promotor consists of an acrylamide diallyldimethylammonium chloride copolymer, wherein the strength promotor is added at a concentration of 0.1 kg/ton of furnish, and wherein the strength agent is added in an amount between 3.0 and 6.0 kg/ton of furnish.

2. The method of claim 1 wherein the strength promoter has a reduced specific viscosity (RSV) between 0.5 to 15.

3. The method of claim 2 wherein the strength promoter has RSV between 3 to 6.

4. The method of claim 1 wherein the anionic trash containing furnish is one selected from the list consisting of recycled fibers or mechanic fibers, and any combination thereof.

5. The method of claim 1 wherein the strength agent is a dry strength agent.

6. The method of claim 1 further comprising adding a flocculant after the step of adding the strength agent.

7. A method of increasing the strength of a paper product, the method consisting of adding a strength promoter to a furnish prior to adding a strength agent to the furnish, wherein the strength promoter does not comprise epichlorohydrin, adding the strength agent to the furnish, wherein the strength agent is glyoxalated polyacrylamide, and making a paper product out of the furnish according to a papermaking process.

Assignments (3)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 28, 2017
From: NALCO COMPANY LLC
To: ECOLAB USA INC.
Reel/Frame 043133/0837 →
CHANGE OF NAME Recorded Jun 21, 2017
From: NALCO COMPANY
To: NALCO COMPANY LLC
Reel/Frame 042939/0948 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 10, 2014
From: ZHAO, YULIN; LI, JUN; LONG RAO, QING; CHENG, WEIGUO
To: NALCO COMPANY
Reel/Frame 034195/0013 →
Priority Claims (1)
CN 2011 1 0382058 · Nov 25, 2011 · national
Continuity (2)
Continuation 13399253 · Feb 17, 2012