Suspensions for enhanced oil recovery
Embodiments of the present disclosure include suspensions for use in enhanced oil recovery, and methods of using the suspensions for recovering oil. Suspensions of the present disclosure include a nonionic surfactant that can dissolve in supercritical carbon dioxide, and a metal salt having a concentration of 200 to 1 parts-per-million.
1. A method, comprising:
supplying supercritical carbon dioxide through piping; and
introducing a suspension having a nonionic surfactant and a metal salt into the supercritical carbon dioxide in the piping, the suspension having a metal salt concentration of 200 to 1 parts-per-million, wherein the metal salt is produced in forming the nonionic surfactant.
2. The method of claim 1 , including depositing at least a portion of the metal salt on at least a portion of the piping; and
dissolving the metal salt from at least the portion of the piping with an aqueous solution.
3. The method of claim 1 , where the nonionic surfactant is selected from the group consisting of an alkylphenol alkoxylate, an alkyl alkoxylate and combinations thereof.
4. The method of claim 1 , where the metal salt is selected from the group consisting of a carboxylate, a boron salt, a titanium salt, a metal carbonate, a metal chloride, a metal sulfate, a metal phosphate, a metal sulphonate, a metal phosphonate, a metal-cyanide salt, and combinations thereof.
5. The method of claim 1 , including exposing the suspension to an oxidizing agent prior to introducing the suspension into the supercritical carbon dioxide.
6. The method of claim 1 , including forming a carboxylic acid in the suspension prior to introducing the suspension into the supercritical carbon dioxide.
7. A method, comprising:
supplying supercritical carbon dioxide through piping;
introducing a suspension having a nonionic surfactant and a metal salt into the supercritical carbon dioxide in the piping the suspension having a metal salt concentration of 200 to 1 parts-per-million, wherein the metal salt is produced in forming the nonionic surfactant;
depositing at least a portion of the metal salt on at least a portion of the piping; and
dissolving the metal salt from at least the portion of the piping with an aqueous solution.
8. The method of claim 7 , where the nonionic surfactant is selected from the group consisting of an alkylphenol alkoxylate, an alkyl alkoxylate and combinations thereof.
9. The method of claim 7 , where the metal salt is selected from the group consisting of a carboxylate, a boron salt, a titanium salt, a metal carbonate, a metal chloride, a metal sulfate, a metal phosphate, a metal sulphonate, a metal phosphonate, a metal-cyanide salt, and combinations thereof.
10. The method of claim 7 , including exposing the suspension to an oxidizing agent prior to introducing the suspension into the supercritical carbon dioxide.
11. The method of claim 7 , including forming a carboxylic acid in the suspension prior to introducing the suspension into the supercritical carbon dioxide.