Ink composition and recording method

Inventors: Takayoshi Kagata (Shiojiri, JP); Masahiro Yatake (Shiojiri, JP); Hiroshi Mukai (Shiojiri, JP)
Assignee: Seiko Epson Corporation
C09D11/107C09D11/033C09D11/10C09D11/322
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,657,187
App. No.
14/669,371
Granted
May 23, 2017
Kind
B2
Abstract

An ink composition includes a pigment; polymer particles; and a polar solvent with a boiling point of 150° C. or higher, in which the polymer particles include a core polymer and a shell polymer that covers at least a portion of the core polymer, a glass transition point of the polymer that configures the core polymer is more than 30° C. lower than the glass transition point of the polymer that configures the shell polymer, the polymer that configures the shell polymer includes a polymer having a (meth)acrylate monomer unit and a carboxylic acid monomer unit, the content (solid content conversion) of the polymer particles is 1.0 mass % to 10 mass % with respect to the total amount of the ink composition, and the content of the polar solvent is 10 mass % to 40 mass % of the total amount of the ink composition.

Claims (68)

1. An ink composition, comprising:

a pigment;

polymer particles; and

a polar solvent with a boiling point of 150° C. or higher,

wherein the polymer particles include a core polymer and a shell polymer that covers at least a portion of the core polymer,

a glass transition point of the polymer that configures the core polymer is more than 10° C. lower than the glass transition point of the polymer that configures the shell polymer,

the polymer that configures the shell polymer includes a polymer having a (meth)acrylate monomer unit and a carboxylic acid monomer unit,

the content (solid content conversion) of the polymer particles is 1.0 mass % to 10 mass % with respect to the total amount of the ink composition,

the content of the polar solvent is 10 mass % to 40 mass % of the total amount of the ink composition, and

the viscosity reduction rate from the viscosity at 20° C. to the viscosity at 50° C. is 40% to 80%.

2. The ink composition according to claim 1 ,

wherein the polar solvent includes 5.0 mass % or more of the polar solvent with a boiling point of 190° C. or higher and 220° C. or lower, with respect to the total amount of the ink composition.

3. A recording method, comprising:

a first heating step of heating a recording medium to a surface temperature of 30° C. to 70° C.;

discharging the ink composition of claim 2 from a nozzle, and attaching the ink composition on the heated recording medium; and

a second heating step of heating the recording medium to which the ink composition is attached to 40° C. to 120° C.

4. The ink composition according to claim 1 ,

wherein the content of the polar solvent with a boiling point of 260° C. or higher is 5.0 mass % or less with respect to the total amount of the ink composition.

5. A recording method, comprising:

a first heating step of heating a recording medium to a surface temperature of 30° C. to 70° C.;

discharging the ink composition of claim 4 from a nozzle, and attaching the ink composition on the heated recording medium; and

a second heating step of heating the recording medium to which the ink composition is attached to 40° C. to 120° C.

6. The ink composition according to claim 1 ,

wherein the polar solvent includes 5 mass % or more of a nitrogen-containing solvent with respect to the total amount of the ink composition.

7. A recording method, comprising:

a first heating step of heating a recording medium to a surface temperature of 30° C. to 70° C.;

discharging the ink composition of claim 6 from a nozzle, and attaching the ink composition on the heated recording medium; and

a second heating step of heating the recording medium to which the ink composition is attached to 40° C. to 120° C.

8. The ink composition according to claim 1 ,

wherein recording is performed on a heated recording medium.

9. A recording method, comprising:

a first heating step of heating a recording medium to a surface temperature of 30° C. to 70° C.;

discharging the ink composition of claim 8 from a nozzle, and attaching the ink composition on the heated recording medium; and

a second heating step of heating the recording medium to which the ink composition is attached to 40° C. to 120° C.

10. The ink composition according to claim 1 ,

wherein the glass transition point of the polymer that configures the core polymer is −10° C. or higher to 60° C. or lower.

11. A recording method, comprising:

a first heating step of heating a recording medium to a surface temperature of 30° C. to 70° C.;

discharging the ink composition of claim 10 from a nozzle, and attaching the ink composition on the heated recording medium; and

a second heating step of heating the recording medium to which the ink composition is attached to 40° C. to 120° C.

12. The ink composition according to claim 1 ,

wherein the glass transition point of the polymer that configures the shell polymer is 40° C. or higher.

13. A recording method, comprising:

a first heating step of heating a recording medium to a surface temperature of 30° C. to 70° C.;

discharging the ink composition of claim 12 from a nozzle, and attaching the ink composition on the heated recording medium; and

a second heating step of heating the recording medium to which the ink composition is attached to 40° C. to 120° C.

14. The ink composition according to claim 1 ,

wherein the polymer particles include 0.50 mass % to 20 mass % of specified polymer particles with respect to the total amount of the polymer particles,

the specified polymer particles have a mass ratio (c/s) of the mass of the core polymer (c) and the mass of the shell polymer (s) of 0.40 to 4.0, and a ratio ((c/s)/φ) between the average particle diameter φ (unit: nm) of the polymer particles and the mass ratio (c/s) of 0.010 or more.

15. The ink composition according to claim 1 ,

wherein the acid value of the polymer that configures the core polymer is 30 mgKOH/g or less, and the acid value of the polymer that configures the shell polymer is 20 to 400 mgKOH/g.

16. The ink composition according to claim 1 ,

wherein the polymer that configures the core polymer includes a polymer having a hydrophobic monomer unit, and

the polymer that configures the shell polymer includes a polymer having a methyl (meth)acrylate monomer unit or an ethyl (meth)acrylate monomer unit.

17. A recording method, comprising:

a first heating step of heating a recording medium to a surface temperature of 30° C. to 70° C.;

discharging the ink composition of claim 1 from a nozzle, and attaching the ink composition on the heated recording medium; and

a second heating step of heating the recording medium to which the ink composition is attached to 40° C. to 120° C.

18. An ink composition, comprising:

a pigment;

polymer particles; and

a polar solvent with a boiling point of 150° C. or higher,

wherein the polymer particles include a core polymer and a shell polymer that covers at least a portion of the core polymer,

a glass transition point of the polymer that configures the core polymer is more than 10° C. lower than the glass transition point of the polymer that configures the shell polymer,

the polymer that configures the shell polymer includes a polymer having a (meth)acrylate monomer unit and a carboxylic acid monomer unit,

the content (solid content conversion) of the polymer particles is 1.0 mass % to 10 mass % with respect to the total amount of the ink composition,

the content of the polar solvent is 10 mass % to 40 mass % of the total amount of the ink composition, and

the acid value of the polymer that configures the core polymer is 30 mgKOH/g or less, and the acid value of the polymer that configures the shell polymer is 20 to 400 mgKOH/g.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 26, 2015
From: KAGATA, TAKAYOSHI; YATAKE, MASAHIRO; MUKAI, HIROSHI
To: SEIKO EPSON CORPORATION
Reel/Frame 035263/0129 →
Priority Claims (1)
JP 2014-065433 · Mar 27, 2014 · national
Continuity (1)
Related Publication 20160244626A1 · Aug 25, 2016