IP Library › Granted Patent US 9,749,752
Granted Patent B2
US 9,749,752 · App. 14/883,527 · Granted Aug 29, 2017

Microphone and method of manufacturing the same

Inventor: Ilseon Yoo (Seoul, KR)
Assignee: HYUNDAI MOTOR COMPANY
H04R19/04H04R31/00H04R1/342H04R19/005H04R31/003H04R2201/003
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,749,752
App. No.
14/883,527
Granted
Aug 29, 2017
Kind
B2
Abstract

A microphone includes: a first substrate having one or more first penetration holes; a vibrating membrane disposed on the first substrate and covering the first penetration holes; a fixed membrane disposed at a predetermined distance over the vibration membrane and having a plurality of air intake holes; and a phase delay unit bonded by a bonding pad on the fixed membrane, having a plurality of second penetration holes connected to the one or more first penetration holes, and having a phase delay material in the second penetration holes. A method of manufacturing a microphone including a phase delay unit is also disclosed.

Claims (60)

1. A method of manufacturing a microphone, comprising:

preparing a first substrate having first and second opposing surfaces and then forming a vibrating membrane having an oxide film and a plurality of slots onto the first opposing surface of the first substrate;

forming a sacrificial layer and fixed membrane, each having first and second opposing surfaces, over the vibrating membrane and then forming a plurality of air intake holes through the fixed membrane;

depositing a first pad to be connected with the fixed membrane, a second pad to be connected with the vibrating membrane, and a bonding pad for bonding a phase delay unit;

forming a first penetration hole by etching the second opposing surface of the first substrate and forming an air layer between the fixed membrane and the vibrating membrane by partially etching the oxide film and the sacrificial layer; and

bonding the phase delay unit on the bonding pad,

wherein the phase delay unit is formed by:

preparing a second substrate having first and second opposing surfaces and then forming a groove by etching the second opposing surface of the second substrate;

forming a plurality of second penetration holes through the groove and the first opposing surface of the second substrate;

depositing a catalyst to the first opposing surface of the second substrate and the second penetration holes; and

synthesizing CNT (carbon nanotubes) using the catalyst.

2. The method of claim 1 , wherein the forming of air intake holes includes:

forming a plurality of first depressions on the first opposing surface of the sacrificial layer and a plurality of second depressions on the first opposing surface of the fixed membrane; and

forming a plurality of projections on the second opposing surface of the fixed membrane,

wherein the projections

are received in the first depressions of the sacrificial layer.

3. The method of claim 1 , wherein: the depositing of the first pad, the second pad, or the bonding pad is performed by eutectic bonding using metal.

4. The method of claim 1 , wherein the catalyst includes iron (Fe).

5. The method of claim 1 , wherein the synthesizing of CNT includes injecting ammonia gas (NH3) and acetylene gas (C2H2) into a quartz tube at a temperature of 700° C., using CVD (Chemical Vapor Deposition) equipment.

6. A method of manufacturing a microphone, comprising:

preparing a first substrate having first and second opposing surfaces and then forming a vibrating membrane having an oxide film and a plurality of slots onto the first opposing surface of the first substrate;

forming a sacrificial layer and fixed membrane, each having first and second opposing surfaces, over the vibrating membrane and then forming a plurality of air intake holes through the fixed membrane;

depositing a first pad to be connected with the fixed membrane, a second pad to be connected with the vibrating membrane, and a bonding pad for bonding a phase delay unit;

forming a first penetration hole by etching the second opposing surface of the first substrate and forming an air layer between the fixed membrane and the vibrating membrane by partially etching the oxide film and the sacrificial layer; and

bonding the phase delay unit on the bonding pad,

wherein the phase delay unit is formed by:

preparing a second substrate having first and second opposing surfaces and then forming a groove by etching the second opposing surface of the second substrate;

forming a plurality of second penetration holes through the groove and the first opposing surface of the second substrate;

depositing zinc oxide nanoparticles to the groove, the top, and the second penetration holes of the second substrate; and

growing a zinc oxide nanowire in the second substrate with the zinc oxide nanoparticles deposited, using hydrothermal synthesis.

7. The method of claim 6 , wherein in the depositing of zinc oxide nanoparticles, the zinc oxide nanoparticles are dissolved in ethanol.

8. The method of claim 6 , wherein in the hydrothermal synthesis, an aqueous solution composed of zinc nitrate, HMTA (hexamethylenetetramine), and PEI (polyethylenimine) is used.

9. A method of manufacturing a directional MEMS microphone, comprising:

preparing a first substrate having first and second opposing surfaces and then forming a vibrating membrane having an oxide film and a plurality of slots onto the first opposing surface of the first substrate;

forming a sacrificial layer and a fixed membrane, each having first and second opposing surfaces, over the vibrating membrane, and then forming air intake holes through the fixed membrane;

depositing a first pad to be connected with the fixed membrane, a second pad to be connected with the vibrating membrane, and a bonding pad for bonding a phase delay unit;

forming a first penetration hole by etching the second opposing surface of the first substrate and forming an air layer between the fixed membrane and the vibrating membrane by partially etching the oxide film and the sacrificial layer; and

bonding the phase delay unit on the bonding pad,

wherein the phase delay unit is formed by:

preparing a second substrate having first and second opposing surfaces and then forming a groove by etching the second opposing surface of the second substrate;

forming a plurality of second penetration holes through the groove and the first opposing surface of the second substrate;

coating the groove, the first opposing surface, and the second penetration holes of the second substrate with a polymer;

coating a portion of the polymer with a photoresist (PR);

etching the polymer at portions other than the portion coated with a PR by patterning the PR between the groove and the second penetration holes; and

removing the PR after the polymer has been etched.

10. The method of claim 9 , wherein the bonding pad includes a polymer-based bonding material.

11. The method of claim 9 , wherein the step of coating with the polymer includes spin coating or spray coating.

12. The method of claim 9 , wherein the polymer includes PE, PMMA, EMMAm PEEK, LCP, PDMS, Tefxel, a phenolic resin, or an epoxy resin.

13. A microphone comprising:

a first substrate having one or more first penetration holes;

a vibrating membrane disposed on the first substrate and covering the first penetration holes;

a fixed membrane disposed at a predetermined distance over the vibration membrane and having a plurality of air intake holes; and

a phase delay unit bonded by a bonding pad on the fixed membrane, having a plurality of second penetration holes connected to the one or more first penetration holes, and having a phase delay material in the second penetration holes.

14. The microphone of claim 13 , wherein the phase delay unit includes a second substrate having first and second opposing surfaces, the second opposing surface having a groove connected with the second penetration holes, and wherein CNTs (carbon nanotubes) are formed as a phase delay material.

15. The microphone of claim 14 , wherein the CNTs are formed on the first opposing surface of the second substrate and fill the second penetration holes.

16. The microphone of claim 13 , wherein the phase delay unit includes a second substrate having first and second opposing surfaces, the second opposing surface having a groove connected with the second penetration holes, and wherein a zinc oxide nanowire is formed as a phase delay material.

17. The microphone of claim 16 , wherein the zinc oxide nanowire is formed on the first opposing surface of the second substrate, fills the second penetration holes, and is formed within the groove.

18. The microphone of claim 13 , wherein the phase delay unit includes a second substrate having first and second opposing surfaces, the second opposing surface having a groove connected with the second penetration holes, and wherein a polymer is formed as a phase delay material.

19. The microphone of claim 18 , wherein the polymer is formed on the first opposing surface of the second substrate, fills the second penetration holes, and is formed a first portion of the groove.

20. The microphone of claim 19 , wherein the first portion of the groove is a portion closest to the first opposing surface of the second substrate.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 14, 2015
From: YOO, ILSEON
To: HYUNDAI MOTOR COMPANY
Reel/Frame 036795/0224 →
Priority Claims (1)
KR 10-2014-0166783 · Nov 26, 2014 · national
Continuity (1)
Related Publication 20160150324A1 · May 26, 2016