IP Library › Granted Patent US 9,840,896
Granted Patent B2
US 9,840,896 · App. 13/865,610 · Granted Dec 12, 2017

Acid soluble abrasive material and method of use

Inventors: Mark Britton (Carter, OK); Roger Schultz (Ninnekah, OK)
Assignee: Thru Tubing Solutions, Inc.
E21B43/26C09G1/02C09K8/426C09K8/72C09K8/74E21B43/114
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,840,896
App. No.
13/865,610
Granted
Dec 12, 2017
Kind
B2
Abstract

A method of treating a formation, a wellbore, or equipment in a wellbore is disclosed herein. The method includes introducing a soluble abrasive material into a wellbore for various oil and gas operations. The method also includes introducing an acidic solution into the wellbore to dissolve at least a portion of the soluble abrasive material to allow for more efficient removal of the soluble abrasive material from the wellbore.

Claims (14)

1. A method, the method comprising:

performing a perforation operation by introducing an abrasive slurry through a perforating tool with high velocity nozzles thereby perforating an oil and gas formation intersected by a wellbore and creating perforations in the oil and gas formation that are fractured by a separate fracturing operation;

wherein

the abrasive slurry is a mixture of a soluble abrasive material, a non-soluble abrasive material and a carrier fluid for transporting the abrasive materials down into the wellbore,

the soluble abrasive material is soluble in an acidic solution, the non-soluble abrasive material is not soluble in the acidic solution and the wellbore provides access to portions of the oil and gas formation, and

the ratio of the amount of non-soluble abrasive material to the soluble abrasive material in the abrasive slurry is in a range of from about 10.0 weight percent to about 20 weight percent; and

introducing the acidic solution into the wellbore to dissolve a portion of the soluble abrasive material introduced into the wellbore in the abrasive slurry.

2. The method of claim 1 wherein the soluble abrasive material is calcium carbonate.

3. The method of claim 1 wherein the acidic solution includes hydrochloric acid to dissolve a portion of the soluble abrasive material.

4. The method of claim 1 further comprising fracturing a portion of the formation with the abrasive slurry prior to introducing the acidic solution and introducing a second acidic solution to the wellbore to dissolve a further amount of the soluble abrasive material.

5. The method of claim 1 wherein the non-soluble abrasive material is selected from the group consisting of sand, gypsum, silica-based products, and a combination thereof.

6. The method of claim 1 further comprising a step of introducing a second abrasive slurry into the wellbore wherein the second abrasive slurry includes non-soluble abrasive material that is insoluble in the acidic solution.

7. The method of claim 1 wherein a second acidic solution is introduced into the wellbore to interact with the soluble abrasive material to convert a portion of the soluble abrasive material to a non-soluble abrasive material that is insoluble in the acidic solution.

8. The method of claim 7 wherein the soluble abrasive material is calcium carbonate and the second acidic solution is sulfuric acid, which converts the calcium carbonate to gypsum.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 18, 2013
From: BRITTON, MARK; SCHULTZ, ROGER
To: THRU TUBING SOLUTIONS, INC.
Reel/Frame 030244/0247 →
Continuity (3)
Provisional Application 61704150 · Sep 21, 2012
Provisional Application 61733947 · Dec 6, 2012
Related Publication 20140083709A1 · Mar 27, 2014