Composite flash-precipitated nanoparticles

Inventors: Robert K. Prud'homme (Lawrenceville, NJ); Marian Gindy (Haledon, NJ); Ying Liu (Chicago, IL)
Assignee: The Trustees of Princeton University
A61K9/5153A61K49/0019A61K49/0065A61K49/0093A61K49/1857Y10T428/2991
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,943,490
App. No.
12/265,206
Granted
Apr 17, 2018
Kind
B2
Abstract

The invention described herein relates to sterically stabilized colloidal constructs comprising preformed colloidal particles encapsulated within a polymeric shell. The constructs, which are controllably sized, are nanoparticles comprising hydrophobic elements, electrostatically charged particles with hydrophobic surfaces, hydrophobic inorganic nanostructures, and amphiphilic copolymers with hydrophobic domains and hydrophilic domains. The constructs are made by a process that allows for the simultaneous encapsulation of a preformed colloidal agent as well as a dissolved hydrophobic active within the core of the polymeric nanoparticle. Among the actives incorporated in various embodiments are organic fluorescent dyes, metal nanostructures and superparamagnetic materials for use in combined fluorescence, optical and magnetic resonance imaging applications, and hydrophobic drugs for therapeutic applications.

Claims (24)

1. A process for manufacturing composite nanoparticles, comprising:

a. providing;

i) a first water-miscible organic solvent comprising a hydrophobic organic compound;

ii) a second water-miscible organic solvent comprising a colloidal dispersion of a plurality of inorganic hydrophobic nanoparticles selected from the group consisting of metallic inorganic hydrophobic nanoparticles and metal oxide inorganic hydrophobic nanoparticles, wherein said inorganic hydrophobic nanoparticles comprise a metallic element;

iii) a third water-miscible organic solvent comprising an amphiphilic polymer; and

iv) an anti-solvent; and

b) micromixing said collodial dispersion of said plurality of inorganic hydrophobic nanoparticles in said second water-miscible organic solvent with said first and third water-miscible organic solvents to create a colloidal composite nanoparticle comprising said metallic element,

wherein said colloidal composite nanoparticle comprises a plurality of inorganic hydrophobic nanoparticle aggregates;

wherein said inorganic hydrophobic nanoparticle aggregates comprise a size that is determined by the number of said metallic elements; and

wherein said collodial composite nanoparticle comprises a hydrophilic shell and said hydrophobic organic compound.

2. The process of claim 1 wherein said hydrophobic organic compound is insoluble in water.

3. The process of claim 1 , wherein said first, second and third water-miscible solvents are selected from the group consisting of tetrahydrofuran, dimethyl sulfoxide, and ethanol.

4. The process of claim 1 , wherein said anti-solvent comprises water.

5. The process of claim 1 , wherein said amphiphilic polymer is selected from the group consisting of a polymer, a copolymer, block copolymer, graft copolymer, comb-graft copolymer, and a random copolymer.

6. The process of claim 1 , wherein said inorganic-hydrophobic colloidal particles are surface-modified.

7. The process of claim 6 , wherein said surface-modified inorganic hydrophobic colloidal particles comprise an electrostatic charge.

8. The process of claim 1 , wherein said hydrophobic organic compound comprises an electrostatic charge.

9. The process of claim 1 , wherein said micromixing is performed with a multi-inlet vortex mixer.

10. The process of claim 1 , wherein said micromixing is performed with an impinging jet mixer.

11. The process of claim 1 , wherein said first, second and third water-miscible organic solvents are the same.

12. The process of claim 1 , wherein said first, second and third water-miscible organic solvents are different.

13. The process of claim 1 , wherein said micromixing comprises flash-nano precipitation.

14. The process of claim 1 , wherein said inorganic hydrophobic nanoparticles are selected from the group consisting of gold particles, palladium particles, magnetic particles, paramagnetic particles, superparamagnetic metals and oxides thereof.

15. The process of claim 1 , wherein said inorganic hydrophobic nanoparticles are selected from the group consisting of Gd(III), Mn(II), Mn(III), Cr(II), Cr(III), Cu(II), Fe(III), Pr(III), Nd(III), Sm(III), Tb(III), Yb(III), Ho(III), Eu(II), Eu(III), Er(III), Indium (In), Technetium (Tc), barium particles and quantum dots.

Assignments (2)
CONFIRMATORY LICENSE Recorded Jul 29, 2009
From: PRINCETON UNIVERSITY
To: NATIONAL SCIENCE FOUNDATION
Reel/Frame 023019/0767 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 13, 2009
From: PRUD'HOMME, ROBERT K.; GINDY, MARIAN; LIU, YING
To: THE TRUSTEES OF PRINCETON UNIVERSITY
Reel/Frame 022393/0664 →
Continuity (1)
Related Publication 20100330368A1 · Dec 30, 2010