IP Library Granted Patent US 9,945,039
Granted Patent B2
US 9,945,039 · App. 13/156,230 · Granted Apr 17, 2018

Method for improving the efficiency and durability of electrical energy storage using solid oxide electrolysis cell

Inventors: Scott A. Barnett (Evanston, IL); David M. Blerschank (Evanston, IL); James R. Wilson (San Francisco, CA)
Assignee: Northwestern University
C25B1/02C25B3/04C25B15/02H01M8/0618H01M8/186H01M8/0662H01M2008/1293Y02E60/528
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,945,039
App. No.
13/156,230
Granted
Apr 17, 2018
Kind
B2
Abstract

A method for improving the efficiency and durability of reversible solid oxide cells during electrical energy storage is disclosed. The method utilizes a specific set of operating conditions that produces a storage chemistry where approximately thermal-neutral operation can be achieved at low cell over-potentials. Also disclosed are reversible solid oxide cell energy storage system configurations, including one that utilizes storage in natural gas and water storage/distribution networks, thereby reducing storage cost.

Claims (25)

1. A method for fuel production comprising

providing a reversible solid oxide cell energy storage system comprising: a) a solid oxide fuel cell comprising an electrolyte, an oxygen electrode and a fuel electrode to catalytically promote methane formation under operation, thereby producing sufficient heat in the solid oxide reversible fuel cell to reduce the thermo-neutral voltage below 1.3 V; b) one or more storage tanks attached to the solid oxide fuel cell to store liquid or gaseous reactants and products; and c) a heat exchanger, wherein the heat exchanger is located between the one or more storage tanks and the solid oxide fuel cell, said system absent a Sabatier reactor;

operating the solid oxide reversible fuel cell in electrolysis mode at a thermo-neutral voltage of from between 1.0-1.3 V and improve efficiency of said cell; and

generating a fuel mixture within the solid oxide reversible fuel cell, the fuel mixture comprising hydrogen and at least about 10% methane, said mixture sufficient for use in said cell without the Sabatier reactor.

2. A method according to claim 1 wherein electrolysis mode is operated at an operating pressure of 5-100 atmospheres, and at an operating temperature of 700-850° C.

3. A method according to claim 2 wherein the operating pressure is 10-20 atmospheres.

4. A method according to claim 1 wherein electrolysis mode is operated at an operating pressure of 1-5 atmospheres, and at an operating temperature of 500-700° C.

5. A method according to claim 1 wherein electrolysis mode is operated at an operating pressure of 5-100 atmospheres, and at an operating temperature of 500-700° C.

6. A method according to claim 1 wherein the generated fuel is catalytically converted to methane.

7. A method according to claim 1 wherein electrolysis mode is operated under conditions wherein the thermal-neutral voltage is approximately equal to the Nernst potential.

8. A method according to claim 1 further comprising providing the stored at least 10% methane-containing fuel mixture, and oxygen or air, to the solid oxide reversible cell, and operating the solid oxide reversible cell in a fuel cell mode using the provided fuel, and oxygen or air, to produce electricity.

9. A method according to claim 8 wherein fuel cell mode is operated at an operating pressure of 5-100 atmospheres, and at an operating temperature of 700-850° C.

10. A method according to claim 9 wherein the operating pressure is 10-20 atmospheres.

11. A method according to claim 8 wherein fuel cell mode is operated at an operating pressure of 1-5 atmospheres, and at an operating temperature of 500-700° C.

12. A method according to claim 8 wherein fuel cell mode is operated at an operating pressure of 5-100 atmospheres, and at an operating temperature of 500-700° C.

13. A method for electrical energy storage comprising: providing a reversible solid oxide cell energy storage system comprising a solid oxide fuel cell comprising an electrolyte, an oxygen electrode and a fuel electrode to catalytically promote methane formation under operation, thereby producing sufficient heat in the solid oxide reversible fuel cell to reduce the thermos-neutral voltage below 1.3 V;

One or more storage tanks attached to the solid oxide fuel cell to store liquid or gaseous reactants and products; and a heat exchanger, wherein the heat exchanger is located between the one or more storage tanks and the solid oxide fuel cell, said system absent a Sabatier reactor;

a) operating the solid oxide reversible fuel cell in electrolysis mode at a thermal-neutral voltage of from between 1.0-1.3 V, at a first operating temperature of 500-850° C., and a first operating pressure of 1-100 atmospheres to generate within the solid oxide reversible cell a fuel mixture comprising hydrogen and at least 10% methane;

b) providing the fuel mixture, and oxygen or air, to the solid oxide reversible fuel cell; and

c) operating the solid oxide reversible fuel cell in fuel cell mode using the provided fuel, and oxygen or air, at a second operating temperature of 500-850° C. and a second operating pressure of from between 1-100 atmospheres to produce electrical energy.

14. A method according to claim 13 wherein electrolysis mode is operated under conditions wherein the thermal-neutral voltage is approximately equal to the Nernst potential.

15. A method according to claim 13 wherein the first operating pressure and the second operating pressure are independently 5-100 atmospheres, and the first operating temperature and the second operating temperature are independently 700-850° C.

16. A method according to claim 15 wherein the first operating pressure and the second operating pressure are independently 10-20 atmospheres.

17. A method according to claim 13 wherein the first operating pressure and the second operating pressure are independently 1-5 atmospheres, and the first operating temperature and the second operating temperature are independently 500-700° C.

18. A method according to claim 13 wherein the first operating pressure and the second operating pressure are independently 5-100 atmospheres, and the first operating temperature and the second operating temperature are independently 500-700° C.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Sep 7, 2011
From: BARNETT, SCOTT A.; BIERSCHENK, DAVID M.; WILSON, JAMES R.
To: NORTHWESTERN UNIVERSITY
Reel/Frame 026864/0435 →
CONFIRMATORY LICENSE Recorded Jun 28, 2011
From: NORTHWESTERN UNIVERSITY
To: NATIONAL SCIENCE FOUNDATION
Reel/Frame 026510/0998 →
Continuity (2)
Provisional Application 61352656 · Jun 8, 2010
Related Publication 20120003552A1 · Jan 5, 2012