Method for selective etching
Disclosed is a method of selective etching a first material on a substrate with a high selectivity towards a second material by flowing a liquid etchant across a substrate surface at a flow sufficient fast to generate a minimum mean velocity v parallel to the substrate's surface.
1 . Method of selective etching comprising:
providing a first material selected from a group A on a substrate
providing a second material selected from a group B on a substrate
selectively etching said first material with a selectivity of at least 2:1 towards said second material by a liquid etchant flowing across the substrate surface at a flow sufficient fast to generate a mean velocity v parallel to the substrate's surface of minimum 0,1 m/s
2 . Method of claim 1 wherein said liquid is dispensed onto the substrate in a continuous flow and spread over the substrate's surface
3 . Method of claim 2 wherein the point of impact of the liquid stream is moved across the surface of the substrate in a time sequence.
4 . Method of claim 2 wherein said liquid is dispensed at a volume flow of at least 0,05 l/min (especially at least 0,5 l/min).
5 . Method of claim 1 wherein said substrate is rotated while exposed to said liquid etchant.
6 . Method of claim 1 wherein group A comprises materials with a high dielectric constant.
7 . Method of claim 1 wherein group B comprises silicon dioxide, silicon.
8 . Method of claim 1 wherein the second material is silicon dioxide and the liquid etchant comprises fluoride ions.
9 . Method of claim 1 wherein said first material is subjected a pretreatment in order to damage the material's structure.
10 . Method of claim 9 wherein said pretreatment is an energetic particle bombardment.
11 . Method of claim 1 wherein said liquid etchant is selected from a group comprising
a solution comprising fluoride ions and an additive for lowering dielectric constant of said solution,
an acidic, aqueous solution comprising fluoride ions.
an acidic, aqueous solution comprising fluoride ions and an additive for lowering dielectric number e.g. an alcohol.
12 . Method of claim 11 wherein said liquid etchant comprises an analytical concentration of less than 0,01 mol/l of fluoride ions, wherein said analytical concentration is calculated as F − .
13 . Method of claim 1 wherein said liquid etchant comprises fluoride ions and has a pH value of below 3.