IP Library Granted Patent US 8,287,623
Granted Patent B2
US 8,287,623 · App. 12/617,934 · Granted Oct 16, 2012

Method of heap or dump leaching of copper from copper sulfide ore

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,287,623
App. No.
12/617,934
Granted
Oct 16, 2012
Kind
B2
Abstract

Disclosed is a method of efficiently leaching copper not only from a readily-soluble copper ore but also a poorly-soluble copper sulfide ore partially containing or consisting of chalcopyrite and/or covellite by means of ore heap leaching under versatile conditions for actual operation. Also disclosed is a method of leaching copper from a copper sulfide ore, including leaching copper from an ore including a copper sulfide ore by heap or dump leaching with the use of a sulfuric acid solution containing ferric (III) ions and iodide ions at a total iodine concentration of 8 to 100 mg/L as a leaching solution.

Claims (10)

1. A method of leaching copper from a copper sulfide ore, comprising

leaching copper from an ore comprising a copper sulfide ore by means of heap or dump leaching with the use of a sulfuric acid solution containing ferric (III) ions and iodide ions at a total iodine concentration of 8 to 100 mg/L as a leaching solution,

wherein a ratio of a ferric (III) ion concentration to a total iodine concentration (Fe 3+ /I) by weight in the leaching solution is greater than or equal to 20:1.

2. The method according to claim 1 , wherein the ore comprising a copper sulfide ore contains chalcopyrite as a main constituent.

3. The method according to claim 1 , wherein ferric (III) ion is added to the leaching solution in a manner that a proportion of a ferrous (II) ion concentration relative to a total iron concentration (Fe 2+ /Fe) in a pregnant leach solution becomes 20% or more.

4. The method according to claim 2 , wherein ferric (III) ion is added to the leaching solution in a manner that a proportion of a ferrous (II) ion concentration relative to a total iron concentration (Fe 2+ /Fe) in a pregnant leach solution becomes 20% or more.

5. A method of leaching copper from a copper sulfide ore, comprising

leaching copper from an ore comprising a copper sulfide ore by means of heap or dump leaching with the use of a sulfuric acid solution containing ferric (III) ions and iodide ions at a total iodine concentration of 8 to 100 mg/L as a leaching solution,

wherein ferric (III) ion is added to the leaching solution in a manner that a proportion of a ferrous (II) ion concentration relative to a total iron concentration (Fe 2+ /Fe) in a pregnant leach solution becomes 20% or more.

6. The method according to claim 5 , wherein the ore comprising a copper sulfide ore contains chalcopyrite as a main constituent.

Assignments (5)
CHANGE OF ADDRESS Recorded Aug 11, 2021
From: JX NIPPON MINING & METALS CORPORATION
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 057160/0114 →
CHANGE OF ADDRESS Recorded Feb 7, 2017
From: JX NIPPON MINING & METALS CORPORATION
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 041649/0733 →
CHANGE OF NAME Recorded Oct 19, 2010
From: NIPPON MINING HOLDINGS, INC.
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 025163/0035 →
MERGER Recorded Oct 14, 2010
From: NIPPON MINING & METALS CO., LTD.
To: NIPPON MINING HOLDINGS, INC.
Reel/Frame 025141/0435 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 1, 2009
From: MANABE, MANABU
To: NIPPON MINING & METALS CO., LTD.
Reel/Frame 023583/0720 →