IP Library Granted Patent US 8,591,720
Granted Patent B2
US 8,591,720 · App. 13/208,418 · Granted Nov 26, 2013

Method and apparatus for achieving maximum yield in the electrolytic preparation of group IV and V hydrides

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,591,720
App. No.
13/208,418
Granted
Nov 26, 2013
Kind
B2
Abstract

A method for generating hydride gas of metal M 1 in electrochemical cell comprising cathode comprising metal M 1 , sacrificial anode comprising metal M 2 , an initial concentration of aqueous electrolyte solution comprising metal hydroxide M 3 OH, wherein the sacrificial metal anode electrochemically oxidizes in the presence of the aqueous electrolyte solution to form metal salt, and hydride gas of metal M 1 is formed by reducing the metal M 1 of the cathode. The method also comprises steps of determining solubility profile curves of metal salt as M 3 OH is consumed and metal oxide is formed by oxidation reaction at various concentrations of M 3 OH; determining the maximum concentration of M 3 OH that does not yield a concentration of metal salt that precipitates out of the electrolyte solution; and choosing a concentration of M 3 OH that is in the range of at and within 5% less than the maximum concentration of M 3 OH to be the initial concentration of M 3 OH.

Claims (10)

1. An electrochemical vessel for generating a hydride gas of arsenic metal comprising:

an electrolyte solution comprising from about 35 to about 39% by weight of KOH;

a cathode comprising at least 99.0% by weight arsenic; and

at least one anode comprising molybdenum;

wherein the cathode and the at least one anode are placed in the electrolyte solution.

2. A method of producing a hydride gas of arsenic metal, characterized by using an electrochemical reactor comprising:

an electrolyte solution comprising from 35% to 39% by weight of KOH,

a cathode comprising at least 99.0% by weight arsenic, and

at least one anode comprising molybdenum,

wherein the cathode and the at least one anode are placed in the electrolyte solution, and a hydride gas of arsenic metal is generated by electrochemically reducing the cathode in the presence of the electrolyte solution.

Assignments (3)
RELEASE OF SECURITY INTEREST Recorded Oct 7, 2019
From: CITIBANK, N.A., AS AGENT
To: VERSUM MATERIALS US, LLC
Reel/Frame 050647/0001 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 20, 2017
From: AIR PRODUCTS AND CHEMICALS, INC.
To: VERSUM MATERIALS US, LLC
Reel/Frame 041772/0733 →
PATENT SECURITY AGREEMENT Recorded Oct 27, 2016
From: VERSUM MATERIALS US, LLC
To: CITIBANK, N.A., AS COLLATERAL AGENT
Reel/Frame 040503/0442 →