IP Library Granted Patent US 9,290,827
Granted Patent B2
US 9,290,827 · App. 13/410,975 · Granted Mar 22, 2016

Method of leaching copper and gold from sulfide ores

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,290,827
App. No.
13/410,975
Granted
Mar 22, 2016
Kind
B2
Abstract

Disclosed is a method of leaching copper and gold from sulfide ores, which includes Process (1) of bringing a first aqueous acidic solution which contains chlorine ion, copper ion and iron ion, but no bromine ion, into contact with sulfide ores under supply of an oxidizing agent, so as to leach copper component contained in the sulfide ores; Process (2) of separating, by solid-liquid separation, a leaching reaction liquid obtained in Process (1), into a leaching residue and a leachate; and Process (3) of bringing a second aqueous acidic solution which contains chlorine ion, bromine ion, copper ion and iron ion, into contact with the leaching residue obtained in Process (2) under supply of an oxidizing agent, so as to leach gold contained in the leaching residue.

Claims (32)

1. A method of leaching copper and gold from sulfide ores, comprising:

Process (1) of bringing a first aqueous acidic solution which contains chlorine ion, copper ion and iron ion, but no bromine ion, into contact with sulfide ores under supply of an oxidizing agent, so as to leach copper component contained in the sulfide ores;

Process (2) of separating, by solid-liquid separation, a leaching reaction liquid obtained in Process (1), into a leaching residue and a leachate; and

Process (3) of bringing a second aqueous acidic solution which contains chlorine ion, bromine ion, copper ion and iron ion, into contact with the leaching residue obtained in Process (2) under supply of an oxidizing agent, so as to leach gold contained in the leaching residue;

wherein the redox potential (vs Ag/AgCl) of the first aqueous acidic solution at the start of Process (1) is 500 mV or above;

wherein Process (1) terminates when conditions stating a copper leach rate of 90% by mass or more, and a gold leach rate of 10% by mass or less, are satisfied;

wherein Process (1) terminates in the range of redox potential (vs Ag/AgCl) from 450 to 500 mV; and

wherein the redox potential (vs Ag/AgCl) of the second aqueous acidic solution at the start of Process (2) is 550 mV or above.

2. The method according to claim 1 ,

wherein the concentration ratio by weight of bromine ion to chlorine ion in the second aqueous acidic solution is 1 or larger.

3. The method according to claim 1 ,

wherein the oxidizing agent used in Process (1) and Process (2) is air.

4. The method according to claim 1 ,

wherein the oxidizing agent used in Process (1) and Process (2) is air.

5. The method according to claim 2 ,

wherein the oxidizing agent used in Process (1) and Process (2) is air.

6. A method of leaching copper and gold from sulfide ores, comprising:

Process (1) of bringing a first aqueous acidic solution which contains chlorine ion, copper ion and iron ion, but no bromine ion, into contact with sulfide ores under supply of an oxidizing agent, so as to leach copper component contained in the sulfide ores;

Process (2) of separating, by solid-liquid separation, a leaching reaction liquid obtained in Process (1), into a leaching residue and a leachate; and

Process (3) of bringing a second aqueous acidic solution which contains chlorine ion, bromine ion, copper ion and iron ion, into contact with the leaching residue obtained in Process (2) under supply of an oxidizing agent, so as to leach gold contained in the leaching residue,

wherein Process (1) terminates in the range of redox potential (vs Ag/AgCl) from 450 to 500 mV;

wherein the redox potential (vs Ag/AgCl) of the first aqueous acidic solution at the start of Process (1) is 500 mV or above; and

wherein the redox potential (vs Ag/AgCl) of the second aqueous acidic solution at the start of Process (2) is 550 mV or above.

7. A method of leaching copper and gold from sulfide ores, comprising:

Process (1) of bringing a first aqueous acidic solution which contains chlorine ion, copper ion and iron ion, but no bromine ion, into contact with sulfide ores under supply of an oxidizing agent, so as to leach copper component contained in the sulfide ores;

Process (2) of separating, by solid-liquid separation, a leaching reaction liquid obtained in Process (1), into a leaching residue and a leachate; and

Process (3) of bringing a second aqueous acidic solution which contains chlorine ion, bromine ion, copper ion and iron ion, into contact with the leaching residue obtained in Process (2) under supply of an oxidizing agent, so as to leach gold contained in the leaching residue,

wherein Process (1) terminates when conditions reach a copper leach rate of 90% by mass or more, and a gold leach rate of 10% by mass or less, are satisfied;

wherein the redox potential (vs Ag/AgCl) of the first aqueous acidic solution at the start of Process (1) is 500 mV or above; and

wherein the redox potential (vs Ag/AgCl) of the second aqueous acidic solution at the start of Process (2) is 550 mV or above.

8. The method according to claim 1 , wherein the redox potential (vs Ag/AgCl) of the first aqueous acidic solution at the start of Process (1) is 550 mV or above.

9. The method according to claim 1 , wherein Process (1) terminates in the range of redox potential (vs Ag/AgCl) from 450 to 475 mV.

Assignments (3)
CHANGE OF ADDRESS Recorded Aug 11, 2021
From: JX NIPPON MINING & METALS CORPORATION
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 057453/0937 →
CHANGE OF ADDRESS Recorded Aug 11, 2021
From: JX NIPPON MINING & METALS CORPORATION
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 057160/0114 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 4, 2012
From: HATANO, KAZUHIRO; ABE, YOSHIFUMI; KATSUKAWA, KOJI; ONO, EIKI
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 027985/0867 →