IP Library Granted Patent US 8,911,533
Granted Patent B2
US 8,911,533 · App. 13/422,505 · Granted Dec 16, 2014

Method of recovering gold from dilute gold solution

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,911,533
App. No.
13/422,505
Granted
Dec 16, 2014
Kind
B2
Abstract

Disclosed is a method of recovering gold from an aqueous solution having a gold concentration of 10 mg/L or lower, using a plurality of extraction apparatuses for bringing the aqueous solution into contact with an extraction agent, arranged to configure a multi-stage extraction process, the method allowing the aqueous solution to continuously flow from the first-stage extraction process to the next-stage extraction process, while recycling the extraction medium used in each stage twice or more times for the extraction process of the same stage, without back extraction and reduction.

Claims (17)

1. A method of recovering gold from an aqueous solution having a gold concentration of 10 mg/L or lower, employing a plurality of extraction apparatuses for bringing the aqueous solution into contact with an extraction solvent arranged to configure a multi-stage extraction process,

wherein the method allows the aqueous solution continuously flows from a first-stage extraction to a second-stage extraction, while recycling the extraction solvent used in each stage twice or more times within the same stage, without back extraction and reduction;

wherein in the first-stage extraction, the volume ratio (O/A) of the extraction solvent (Or) and the aqueous solution (Aq) is ⅕ or smaller, and the used extraction solvent is repeatedly used until the concentration of gold in the extraction solvent is 1 g/L or higher;

wherein in the second-stage extraction gold is repeatedly extracted until the concentration of gold in a post extraction liquid reaches to 0.5 mg/L or below; and

wherein the extraction solvent present in the first-stage is separately prepared and recycled principally within the first-stage of extraction and the extraction solvent present in the second-stage is separately prepared and recycled principally within the second-stage of extraction.

2. The method according to claim 1 , wherein the extraction solvent used in the second-stage process or thereafter is recycled, and then a part of which is fed back to the extraction apparatus in the previous stage.

3. The method according to claim 1 , implementing a reduction process for reducing a part of, or the whole of the extraction solvent after being recycled in the first-stage extraction process.

4. The method according to claim 3 ,

wherein the reduction process is implemented until the gold concentration in the extraction solvent decreases down to 0.5 g/L or below.

5. The method according to claim 1 ,

wherein the aqueous solution is a post-extraction liquid obtained after leaching of ore or concentrate which contains sulfide of copper.

6. The method according to claim 1 , wherein supplementation of the extraction solvent for use in each stage of extraction is implemented by using one of, or two or more solvent selected from the extraction solvent in the succeeding stage, the extraction solvent from which gold was deposited in the reduction process, and a fresh extraction solvent.

7. The method according to claim 1 ,

wherein the extraction solvent is dibutyl carbitol (DBC).

8. The method according to claim 1 , wherein the aqueous solution is a post-extraction liquid of copper concentrate which contains 120 to 200 g/L of chlorine, 0.1 to 30 g/L of copper, 0.01 to 10 g/L of iron, and has a pH value of 2.5 or lower.

9. The method according to claim 1 ,

removing a solid matter from the aqueous solution before the aqueous solution is brought into contact with the extraction solvent.

Assignments (3)
CHANGE OF ADDRESS Recorded Aug 11, 2021
From: JX NIPPON MINING & METALS CORPORATION
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 057453/0937 →
CHANGE OF ADDRESS Recorded Aug 11, 2021
From: JX NIPPON MINING & METALS CORPORATION
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 057160/0114 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 3, 2012
From: HATANO, KAZUHIRO; ABE, YOSHIFUMI; ONO, EIKI; KATSUKAWA, KOJI
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 027977/0283 →