IP Library Granted Patent US 8,333,834
Granted Patent B2
US 8,333,834 · App. 13/497,551 · Granted Dec 18, 2012

High-purity aqueous copper sulfonate solution and method of producing same

View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,333,834
App. No.
13/497,551
Granted
Dec 18, 2012
Kind
B2
Abstract

An object of the present invention is to provide a high-purity aqueous copper sulfonate solution and a simplified method of producing this solution. The aqueous copper sulfonate solution of the present invention is characterized in that the copper concentration therein is at least 90 g/L, the content of metal impurities is less than 10 mg/L as metal for each metal impurity, the content of chlorine is less than 10 mg/L, and the sulfonic acid is a sulfonic acid represented by the following general formula R—(SO 3 H) n (in the formula, R represents a lower alkyl group, lower alkylidene group, lower alkylene group, or hydroxyalkyl group and n represents 1 or 2).

Claims (7)

1. An aqueous copper sulfonate solution having a copper concentration of at least 90 g/L, content of metal impurities of less than 10 mg/L as metal for each metal impurity, content of chlorine of less than 10 mg/L, pH of 2 or more, and sulfonic acid represented by the following general formula

R—(SO 3 H) n

wherein R represents a lower alkyl group, lower alkylidene group, lower alkylene group, or hydroxyalkyl group and n represents 1 or 2.

2. The aqueous copper sulfonate solution according to claim 1 , characterized in that the metal impurities contain a metal selected from the group consisting of iron, nickel, silver, lead, magnesium, aluminum, chromium, cobalt, zinc, sodium, potassium, arsenic, antimony, cadmium, gold, indium, manganese, thallium, tin, and titanium.

3. The aqueous copper sulfonate solution according to claim 2 , characterized in that the iron, nickel, silver, lead, magnesium, aluminum, chromium, cobalt, zinc, cadmium, gold, manganese, tin, and titanium contents are each less than 1 mg/L.

4. The aqueous copper sulfonate solution according to claim 1 , produced by the oxidation and dissolution of copper metal in a sulfonic acid solution at a temperature of at least 60° C. but less than 100° C.

5. A method of producing the aqueous copper sulfonate solution according to claim 1 , comprising the steps of oxidizing and dissolving copper metal in a sulfonic acid solution at a temperature of at least 60° C. but less than 100° C.

Assignments (3)
CHANGE OF ADDRESS Recorded Aug 11, 2021
From: JX NIPPON MINING & METALS CORPORATION
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 057160/0114 →
CHANGE OF ADDRESS Recorded Feb 7, 2017
From: JX NIPPON MINING & METALS CORPORATION
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 041649/0733 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Mar 26, 2012
From: SEKIGUCHI, JUNNOSUKE; MURAKAMI, MASAOMI; IMORI, TORU
To: JX NIPPON MINING & METALS CORPORATION
Reel/Frame 027925/0976 →