Method of sintering a composition
View Patent ↗The present invention relates to a method of sintering at least two powdered compounds with different water activities and glass transition temperatures keeping the total water content constant. The method allows sintering of two materials in a closed environment wherein the structure of one material is kept intact.
1. A method of sintering a composition comprising two powdered components, wherein the water activity of the first powdered component is greater than the water activity of the second powdered component, and the glass transition temperature of the first powdered component is less than the glass transition temperature of the second powdered component, the method comprising: heat treating a mixture of the two powdered components at a temperature which is above the glass transition temperature of the first powdered component and less than 20° C. above the glass transition temperature of the second powdered component; and maintaining the total water content of the mixture constant during the heat treatment.
2. The method of claim 1 wherein the mixture of the two powdered components is heated to a temperature which is below the glass transition temperature of the second powdered component.
3. The method of claim 1 wherein the mixture of the two powdered components is heated to a temperature which is at least 10° C. above the glass transition temperature of the first powdered component.
4. The method of claim 1 wherein the mixture of the two powdered components is heated to a temperature which is less than 5° C. above the glass transition temperature of the second powdered component at the water activity reached after full equilibration of the water activities of all ingredients of the mixture being treated.
5. The method of claim 1 wherein the mixture of the two powdered components is heated to a temperature which is below the glass transition temperature of the first powdered component at the water activity reached after full equilibration of the water activities of all ingredients of the mixture being treated.
6. The method of claim 1 wherein the first and the second powdered components are water soluble.
7. The method of claim 1 wherein the first powdered component comprises maltodextrin.
8. The method of claim 1 wherein the second powdered component comprises milk powder.
9. The method of claim 1 wherein the second powdered component comprises soluble coffee.
10. The method of claim 1 wherein the mixture of the two powdered components is heated to a temperature between 45° C. and 75° C.