IP Library Granted Patent US 9,169,453
Granted Patent B2
US 9,169,453 · App. 14/254,379 · Granted Oct 27, 2015

Sorbents for coal combustion

Inventor: Douglas C. Comrie (Cape Coral, FL)
Assignee: NOx II, LTD.
C10L10/00B01D53/30B01D53/485B01D53/64B01J20/041B01J20/043B01J20/046B01J20/06B01J20/16C10L9/10F23J7/00F23J15/00F23K1/00B01D2257/602B01J2220/42F23K2201/505Y10S423/05
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,169,453
App. No.
14/254,379
Granted
Oct 27, 2015
Kind
B2
Abstract

Sorbent compositions containing halogen and calcium are added to coal to mitigate the release of sulfur and/or other harmful elements, including mercury, into the environment during combustion of coal containing natural levels of mercury.

Claims (8)

1. A method of reducing the level of mercury and/or sulfur emitted into the atmosphere upon burning of coal, comprising adding remediation materials onto the coal and delivering the coal with the sorbent composition applied into a furnace for combustion, wherein the remediation materials comprise calcium oxides, calcium halogens, oxides of silicon, oxides of aluminum, oxides of iron, oxides of magnesium, oxides of sodium, and oxides of potassium.

2. The method according to claim 1 , wherein the remediation materials comprise calcium bromide.

3. The method according to claim 1 , wherein the remediation materials comprise an aqueous solution of a bromine containing salt or an iodine containing salt.

4. The method according to claim 1 , wherein the remediation materials contain sufficient silica and alumina to form a refractory mixture with calcium sulfate, such that calcium sulfate is removed by a particle control system of the furnace.

5. The method according to claim 1 , wherein the remediation materials comprise calcium oxide, calcium bromide, calcium nitrite, Portland cement, calcium hydroxide, or calcium carbonate.

6. The method according to claim 1 , wherein adding the remediation materials reduces mercury emissions by at least 90%, measured against emissions observed without the use of the remediation materials.

7. The method according to claim 1 , wherein the remediation materials comprise calcium in a molar ratio of 1:1 to 3:1 with respect to the amount of sulfur in the coal being burned.

8. The method according to claim 1 , further comprising monitoring the level of mercury emitted from the furnace, and adjusting the addition of the remediation materials based on the measured mercury level.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jun 23, 2014
From: COMRIE, DOUGLAS C
To: NOX II, LTD.
Reel/Frame 033155/0789 →
Continuity (10)
Continuation 14036036 · Sep 25, 2013
Continuation 13679775 · Nov 16, 2012
Continuation 13343491 · Jan 4, 2012
Continuation 13169187 · Jun 27, 2011
Continuation 12839154 · Jul 19, 2010
Continuation 12705196 · Feb 12, 2010
Continuation 12351191 · Jan 9, 2009