IP Library Granted Patent US 9,878,486
Granted Patent B2
US 9,878,486 · App. 15/082,080 · Granted Jan 30, 2018

High flash point fluids for in situ plasticization of polymers

Inventors: Bairu Liu (Katy, TX); Anil Sadana (Houston, TX); James B. Crews (Willis, TX)
Assignee: Baker Hughes, a GE company, LLC
B29C61/04B29C61/06E21B33/12E21B33/1208
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,878,486
App. No.
15/082,080
Granted
Jan 30, 2018
Kind
B2
Abstract

An in situ method to deploy and/or plasticize a shape-memory material in order to change the material's physical dimensions and/or mechanical properties, includes a method for deploying a shape memory polymer having a deformed or compressed shape in an environment at a first temperature, the shape memory polymer having a first glass transition temperature which is greater than the first temperature. The method also includes contacting the shape memory polymer with an activation fluid in an amount effective to decrease the glass transition temperature of the shape memory polymer from the first glass transition temperature to a second glass transition temperature which is less than or equal to the first temperature, where the activation fluid comprises a sugar present in an amount effective to raise a flash point of the activation fluid.

Claims (22)

1. A method for deploying a shape memory polymer in a downhole environment, comprising:

disposing a shape memory polymer having a deformed shape in the downhole environment at a first temperature, the shape memory polymer having a first glass transition temperature that is greater than the first temperature;

contacting the shape memory polymer with an activation fluid in an amount effective to decrease the glass transition temperature of the shape memory polymer from the first glass transition temperature to a second glass transition temperature which is less than or equal to the first temperature where the activation fluid comprises acetyl acetone and methanol; where the activation fluid comprises a sugar present in an amount effective to raise a flash point of the activation fluid where the sugar is selected from the group consisting of fructose, sucrose, and combinations thereof, where the amount of sugar in the activation fluid ranges from about 0.5 to about 20 wt %; and

expanding the shape memory polymer to deploy the shape memory polymer in a deployed shape in the downhole environment.

2. The method of claim 1 where the flash point is raised by at least 2° F. (1.1° C.).

3. The method of claim 1 where the shape memory polymer is selected from the group consisting of a polyurethane, a polyurethane made by reacting a polycarbonate polyol with a polyisocyanate, a polystyrene, a polyethylene, an epoxy, a rubber, a fluoroelastomers, a nitrile, a polymer made from ethylene propylene diene monomers (EPDM), a polyamide, a polyurea, a polyvinyl alcohol, a vinyl alcohol-vinyl ester copolymer, a phenolic polymer, a polybenzimidazole, a polyethylene oxide/acrylic acid/methacrylic acid copolymer crosslinked with N,N′-methylene-bis-acrylamide, a polyethylene oxide/methacrylic acid/N-vinyl-2-pyrrolidone copolymer crosslinked with ethylene glycol dimethacrylate, a polyethylene oxide/poly(methyl methacrylate)/N-vinyl-2-pyrrolidone copolymer crosslinked with ethylene glycol dimethacrylate, combinations thereof.

4. The method of claim 1 where the first glass transition temperature ranges from about 100° C. to about 150° C., and where the second glass transition temperature ranges from about 40° C. to about 100° C.

5. The method of claim 1 where the second glass transition temperature is about 10° C. to about 60° C. less than the first glass transition temperature.

6. The method of claim 1 where the first temperature ranges from about 60° C. to about 100° C.

7. The method of claim 1 further comprising changing a mechanical property of the shape memory polymer, where the property is selected from the group consisting of lowering Young's modulus, increasing toughness, and both.

8. A method for deploying a shape memory polymer in a downhole environment, comprising:

disposing a shape memory polymer having a deformed shape in the downhole environment at a first temperature;

contacting the shape memory polymer with an activation fluid to decrease the glass transition temperature of the shape memory polymer below the first temperature, where the activation fluid is comprises acetyl acetone and methanol; where the activation fluid comprises a sugar present in an amount effective to raise a flash point of the activation fluid by at least 2° F. (1.1° C.) where the sugar is selected from the group consisting of fructose, sucrose, and combinations thereof, where the amount of sugar in the activation fluid ranges from about 0.5 to about 20 wt %;

expanding the shape memory polymer to a deployed shape; and

displacing the activation fluid to increase the glass transition temperature to greater than the first temperature and to maintain the shape memory polymer in the deployed shape.

9. The method of claim 8 where the shape memory polymer is selected from the group consisting of a polyurethane, a polyurethane made by reacting a polycarbonate polyol with a polyisocyanate, a polystyrene, a polyethylene, an epoxy, a rubber, a fluoroelastomers, a nitrile, a polymer made from ethylene propylene diene monomers (EPDM), a polyamide, a polyurea, a polyvinyl alcohol, a vinyl alcohol-vinyl ester copolymer, a phenolic polymer, a polybenzimidazole, a polyethylene oxide/acrylic acid/methacrylic acid copolymer crosslinked with N,N′-methylene-bis-acrylamide, a polyethylene oxide/methacrylic acid/N-vinyl-2-pyrrolidone copolymer crosslinked with ethylene glycol dimethacrylate, a polyethylene oxide/poly(methyl methacrylate)/N-vinyl-2-pyrrolidone copolymer crosslinked with ethylene glycol dimethacrylate, combinations thereof.

10. A system for deploying a shape memory polymer in a downhole environment, comprising:

an activation fluid comprising acetyl acetone and methanol; where the activation fluid comprises a sugar present in an amount effective to raise a flash point of the activation fluid where the sugar is selected from the group consisting of fructose, sucrose, and combinations thereof, where the amount of sugar in the activation fluid ranges from about 0.5 to about 20 wt %; and

a shape memory polymer configured to deploy in the downhole environment at a first temperature by a decrease in its glass transition temperature in response to contact with the activation fluid.

11. The system of claim 10 where the flash point is raised by at least 2° F. (1.1° C.).

12. The system of claim 10 where the shape memory polymer is selected from the group consisting of a polyurethane, a polyurethane made by reacting a polycarbonate polyol with a polyisocyanate, a polystyrene, a polyethylene, an epoxy, a rubber, a fluoroelastomers, a nitrile, a polymer made from ethylene propylene diene monomers (EPDM), a polyamide, a polyurea, a polyvinyl alcohol, a vinyl alcohol-vinyl ester copolymer, a phenolic polymer, a polybenzimidazole, a polyethylene oxide/acrylic acid/methacrylic acid copolymer crosslinked with N,N′-methylene-bis-acrylamide, a polyethylene oxide/methacrylic acid/N-vinyl-2-pyrrolidone copolymer crosslinked with ethylene glycol dimethacrylate, a polyethylene oxide/poly(methyl methacrylate)/N-vinyl-2-pyrrolidone copolymer crosslinked with ethylene glycol dimethacrylate, combinations thereof.

13. The system of claim 10 where the shape memory polymer has a first glass transition temperature, and the activation fluid is effective to decrease the first glass transition temperature to a second glass transition temperature, where the second glass transition temperature is about 10° C. to about 60° C. less than the first glass transition temperature.

Assignments (2)
CHANGE OF NAME Recorded Dec 21, 2017
From: BAKER HUGHES INCORPORATED
To: BAKER HUGHES, A GE COMPANY, LLC
Reel/Frame 044939/0467 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 5, 2016
From: LIU, BAIRU; SADANA, ANIL; CREWS, JAMES B.
To: BAKER HUGHES INCORPORATED
Reel/Frame 038475/0460 →
Continuity (3)
Continuation In Part 14033178 · Sep 20, 2013
Continuation In Part 13334394 · Dec 22, 2011
Related Publication 20160208574A1 · Jul 21, 2016