Vulcanization composition having reduced allergenic potential, and elastomeric articles formed therewith

Inventors: Seong Fong Chen (Gelugor, MY); Wei Cheong Wong (Kulim, MY); Chii Yih Low (Bayan Lepas, MY)
Assignee: ALLEGIANCE CORPORATION
C08K5/0091A61B42/10A61B42/20B29C41/14B29C41/22C08J5/02C08K3/06C08K3/22C08K5/0025C08K5/38C09D111/02C09D127/24A61B42/00A61B46/10A61B46/40B29K2011/00B29L2031/4864C08J2311/02C08K2003/2296C08K2201/019Y10T428/1386Y10T428/3183Y10T428/31569
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,125,239
App. No.
15/375,351
Granted
Nov 13, 2018
Kind
B2
Abstract

The present invention generally relates to vulcanization compositions used to vulcanize elastomeric articles, where the vulcanization compositions have reduced allergenic potential as compared to elastomeric articles formed using vulcanization compositions having non-fugitive accelerators. The present invention also relates to elastomeric articles formed using the vulcanization compositions. The invention further relates to methods for making a reduced-allergenicity vulcanization composition, and to methods for using the vulcanization compositions to vulcanize elastomeric articles.

Claims (32)

1. A vulcanization composition comprising:

a source of sulfur,

a single fugitive xanthate accelerator, and

a metal oxide,

where the composition does not include any additional compounds that function as accelerators for vulcanizing elastomers.

2. The vulcanization composition of claim 1 , wherein the sulfur is elemental sulfur and wherein the single fugitive xanthate accelerator is diisopropyl xanthogen polysulfide.

3. The vulcanization composition of claim 1 , wherein the vulcanization composition exhibits reduced allergenicity as compared to conventional vulcanization compositions.

4. The vulcanization composition of claim 1 , wherein the metal oxide is selected from the group consisting of zinc oxide, magnesium oxide, lead oxide, and combinations thereof.

5. The vulcanization composition of claim 1 , wherein the source of sulfur is selected from the group consisting of elemental sulfur and sulfur donors that have a low allergenic potential, and combinations thereof.

6. The vulcanization composition of claim 1 , wherein the single fugitive xanthate accelerator is selected from the group consisting of diisopropyl xanthogen polysulfide, dibutyl xanthogen disulfide, and diisopropyl xanthogen disulfide.

7. The vulcanization composition of claim 1 , wherein the composition does not contain any additional xanthate compounds.

8. An elastomeric article formed using the vulcanization composition of claim 1 , where the elastomeric article does not include any additional compounds that function as accelerators for vulcanizing elastomers.

9. The elastomeric article of claim 8 , wherein the elastomeric article exhibits reduced allergenicity as compared to elastomeric articles formed using conventional accelerators.

10. The elastomeric article of claim 8 , wherein the elastomeric article is selected from the group consisting of gloves, probe covers, finger cots, catheters, dental dams, and condoms.

11. The elastomeric article of claim 8 , wherein the elastomeric articles are powder free.

12. A vulcanization composition comprising:

a source of sulfur,

a single fugitive xanthate accelerators, and

a metal oxide,

wherein the composition does not include any non-fugitive accelerators; and

wherein the composition does not include any additional xanthate compounds.

13. The vulcanization composition of claim 12 wherein

the source of sulfur is elemental sulfur and

diisopropyl xanthogen polysulfide is the single fugitive xanthate accelerator.

14. The vulcanization composition of claim 12 , wherein the vulcanization composition exhibits reduced allergenicity as compared to conventional vulcanization compositions.

15. The vulcanization composition of claim 12 , wherein the metal oxide is selected from the group consisting of zinc oxide, magnesium oxide, lead oxide, and combinations thereof.

16. The vulcanization composition of claim 12 , wherein the source of sulfur is selected from the group consisting of elemental sulfur and sulfur donors that have a low allergenic potential, and combinations thereof.

17. The vulcanization composition of claim 12 , wherein the single fugitive xanthate accelerator is selected from the group consisting of diisopropyl xanthogen polysulfide, dibutyl xanthogen disulfide, and diisopropyl xanthogen disulfide.

18. An elastomeric article formed using the vulcanization composition of claim 12 , where the elastomeric article does not include any non-fugitive accelerators.

19. The elastomeric article of claim 18 , wherein the elastomeric article exhibits reduced allergenicity as compared to elastomeric articles formed using conventional accelerators.

20. The elastomeric article of claim 18 , wherein the elastomeric article is selected from the group consisting of gloves, probe covers, finger cots, catheters, dental dams, and condoms.

21. The elastomeric article of claim 18 , wherein the elastomeric articles are powder free.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 21, 2017
From: CHEN, SEONG FONG; WONG, WEI CHEONG; LOW, CHI YIH
To: ALLEGIANCE CORPORATION
Reel/Frame 041320/0486 →
Continuity (5)
Division 14993532 · Jan 12, 2016
Division 14617296 · Feb 9, 2015
Division 13169872 · Jun 27, 2011
Provisional Application 61358721 · Jun 25, 2010
Related Publication 20170145185A1 · May 25, 2017
Cited By (3)
US 12,415,908 US 12,509,572 US 12,528,936