Facile assembly of soft nanoarchitectures and co-loading of hydrophilic and hydrophobic molecules via flash nanoprecipitation
Described herein are flash nanoprecipitation methods capable of encapsulating hydrophobic molecules, hydrophilic molecules, bioactive protein therapeutics, or other target molecules in amphiphilic copolymer nanocarriers.
1. A method for preparing aqueous-core nanocarriers by flash precipitation comprising the steps of:
(i) providing an organic phase solution comprising poly(ethylene glycol)-bl-poly(propylene sulfide) (PEG-bl-PPS) and a process solvent, wherein the PEG-bl-PPS has a glass transition temperature below 0° C.,
(ii) providing an aqueous phase solution comprising an aqueous solvent,
(iii) mixing the organic phase solution and the aqueous phase solution by impingement to form a mixture, and
(iv) introducing the mixture into a reservoir to cause precipitation of the PEG-bl-PPS as an aqueous-core nanocarrier.
2. The method of claim 1 , wherein the process solvent is selected from the group consisting of tetrahydrofuran (THF), dimethylformamide (DMF), and dimethyl sulfoxide (DMSO).
3. The method of claim 1 , wherein the aqueous solvent is water.
4. The method of claim 1 , wherein the PEG-bl-PPS has a glass transition temperature between about −40° C. and about 0° C.
5. The method of claim 1 , wherein the PEG-bl-PPS is PEG17-bl-PPS 30 -Thiol.
6. The method of claim 1 , wherein the organic phase solution additionally comprises one or more target molecules.
7. The method of claim 1 , wherein the aqueous phase solution additionally comprises a target molecule.
8. The method of claim 7 , wherein the target molecule is selected from the group consisting of a DNA molecule, an RNA molecule, a plasmid, a peptide, a protein, and combinations thereof.
9. The method of claim 1 , wherein the reservoir comprises an aqueous nonsolvent.
10. The method of claim 1 , wherein the reservoir comprises a target molecule.
11. The method of claim 1 , wherein the mixing comprises at least 2 impingements.
12. A method for preparing aqueous-core nanocarriers by flash precipitation comprising the steps of:
(i) providing an organic phase solution comprising poly(ethylene glycol)-bl-poly(propylene sulfide) (PEG-bl-PPS) and a process solvent, wherein the PEG-bl-PPS has a glass transition temperature below 0° C.,
(ii) providing an aqueous phase solution comprising an aqueous solvent and an target molecule,
(iii) mixing the organic phase solution and the aqueous phase solution by impingement to form a mixture, and
(iv) introducing the mixture into a reservoir to cause precipitation of the PEG-bl-PPS as an aqueous-core nanocarrier loaded with the target molecule.
13. The method of claim 12 , wherein the target molecule is selected from the group consisting of a DNA molecule, an RNA molecule, a plasmid, a peptide, a protein, and combinations thereof.
14. The method of claim 12 , wherein the process solvent is selected from the group consisting of tetrahydrofuran (THF), dimethylformamide (DMF), and dimethyl sulfoxide (DMSO).
15. The method of claim 12 , wherein the aqueous solvent is water.
16. The method of claim 12 , wherein the PEG-bl-PPS has a glass transition temperature between about −40° C. and about 0° C.
17. The method of claim 12 , wherein the PEG-bl-PPS is PEG 17 -bl-PPS 30 -Thiol.
18. The method of claim 12 , wherein the organic phase solution additionally comprises a target molecule.
19. A method for preparing aqueous-core nanocarriers by flash precipitation comprising the steps of:
(i) providing an organic phase solution comprising poly(ethylene glycol)-bl-poly(propylene sulfide) (PEG-bl-PPS) and a process solvent, wherein the PEG-bl-PPS has a glass transition temperature below 0° C.,
(ii) providing an aqueous phase solution comprising an aqueous solvent and an target molecule,
(iii) mixing the organic phase solution and the first aqueous phase solution to form a mixture,
(iii) portioning the mixture into a first portion and a second portion,
(iv) mixing the first portion and the second portion by impingement to form a second mixture, and
(v) introducing the second mixture into a reservoir to cause precipitation of the PEG-bl-PPS as an aqueous-core nanocarrier loaded with the target molecule.
20. The method of claim 19 , wherein steps (iii) and (iv) are repeated at least one time.
21. The method of claim 19 , wherein the organic phase solution additionally comprises a second target molecule.
22. The method of claim 1 , wherein the aqueous-core nanocarrier is selected from the group consisting of tubular polymersomes, bicontinuous nanospheres, polymersomes, and multilamellar polymersomes.
23. The method of claim 12 , wherein the aqueous-core nanocarrier is selected from the group consisting of tubular polymersomes, bicontinuous nanospheres, polymersomes, and multilamellar polymersomes.
24. The method of claim 19 , wherein the aqueous-core nanocarrier is selected from the group consisting of tubular polymersomes, bicontinuous nanospheres, polymersomes, and multilamellar polymersomes.