Sizing method for making paper and paper prepared thereof
The present application discloses a sizing method for making paper. An alkenyl succinic anhydride (ASA) is added to a papermaking process. An aluminum salt is added in one or more process steps during the papermaking process. Preferably, the aluminum salt is an aluminum salt which can generate free aluminum ion in aqueous solution. The sizing method of the present application enhances the usage efficiency of a sizing agent and the aluminum salt, as well as provides paper having a high moisture content.
1. A sizing method for making paper, the method comprising:
adding alkenyl succinic anhydride to a papermaking furnish in a papermaking process, and
adding an aluminum salt to one or more process steps during the papermaking process via surface treatment,
wherein the surface treatment comprises spraying the aluminum salt onto a surface of a paper sheet in the one or more process steps during the papermaking process, wherein alkenyl succinic anhydride Is not added in the one or more process steps via a surface treatment,
wherein the one or more process steps during the papermaking process are selected from a process step at a forming section of the paper machine, a process step at a multilayer paperboard combining section, a process step at a press section, a process step at a drying section, a process step at a surface sizing section, and a combination thereof,
wherein the aluminum salt is added to the papermaking process in an amount greater than 0.3 kilograms per ton of paper, and the alkenyl succinic anhydride is added in an amount of at least 0.9 kilograms per ton of paper.
2. The sizing method of claim 1 , wherein the one or more process steps during the papermaking process is a process step at a surface sizing section.
3. The sizing method of claim 1 , wherein the alkenyl succinic anhydride has the following structure
wherein, R 1 and R 2 are alkyl.
4. The sizing method of claim 3 , wherein each of R 1 and R 2 is C 12 -C 22 alkyl.
5. The sizing method of claim 1 , wherein the alkenyl succinic anhydride is added to the papermaking furnish as an emulsion.
6. The sizing method of claim 1 , wherein the papermaking furnish has a pH of from 4 to 9 before the addition of alkenyl succinic anhydride.
7. The sizing method of claim 1 , wherein the aluminum salt is alum, aluminum chloride, polyaluminum chloride, or a combination thereof.
8. The sizing method of claim 1 , wherein the aluminum salt is added to the papermaking process in an amount of from 0.3 kilograms to 3 kilograms per ton of paper.
9. The sizing method of claim 1 , wherein the aluminum salt is added to the papermaking process in combination with an alkyl ketene dimer (“AKD”).
10. The sizing method of claim 9 , wherein the aluminum salt is alum, aluminum sulfate, aluminum chloride, polyaluminum chloride or a combination thereof.
11. The sizing method of claim 1 , wherein the aluminum salt is added to the papermaking process in combination with a starch.
12. The sizing method of claim 11 , wherein the aluminum salt is alum, aluminum sulfate, aluminum chloride, polyaluminum chloride or a combination thereof.
13. A sizing method for making paper, the method comprising:
adding alkenyl succinic anhydride to a papermaking furnish in a papermaking process, and
adding an aluminum salt to one or more process steps during the papermaking process via surface treatment,
wherein the surface treatment comprises spraying the aluminum salt onto a surface of a paper sheet in the one or more process steps during the papermaking process, wherein alkenyl succinic anhydride Is not added in the one or more process steps via a surface treatment,
wherein the one or more process steps during the papermaking process are selected from a process step at a forming section of the paper machine, a process step at a multilayer paperboard combining section, a process step at a press section, a process step at a drying section, a process step at a surface sizing section, and a combination thereof,
wherein the aluminum salt is added to the papermaking process in an amount of at least 10 kilograms per ton of paper, and the alkenyl succinic anhydride is added in an amount of up to and including 5 kilograms per ton of paper.