IP Library › Granted Patent US 10,889,939
Granted Patent B2
US 10,889,939 · App. 16/064,262 · Granted Jan 12, 2021

Sizing method for making paper and paper prepared thereof

Inventors: Zhi Chen (Shanghai, CN); Jinhai Xiao (Hubei, CN); Xiaofeng Zhang (Jiangsu, CN); Kun Hou (Shanghai, CN); James L. Thomas (Naperville, IL); Kaihong Huang (Fujian, CN)
Assignee: ECOLAB USA INC.
D21H21/16D21H17/14D21H17/15D21H17/17D21H17/28D21H17/62D21H17/66D21H17/70D21H17/74D21H23/24D21H23/26D21H23/28
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 10,889,939
App. No.
16/064,262
Granted
Jan 12, 2021
Kind
B2
Abstract

The present application discloses a sizing method for making paper. An alkenyl succinic anhydride (ASA) is added to a papermaking process. An aluminum salt is added in one or more process steps during the papermaking process. Preferably, the aluminum salt is an aluminum salt which can generate free aluminum ion in aqueous solution. The sizing method of the present application enhances the usage efficiency of a sizing agent and the aluminum salt, as well as provides paper having a high moisture content.

Claims (24)

1. A sizing method for making paper, the method comprising:

adding alkenyl succinic anhydride to a papermaking furnish in a papermaking process, and

adding an aluminum salt to one or more process steps during the papermaking process via surface treatment,

wherein the surface treatment comprises spraying the aluminum salt onto a surface of a paper sheet in the one or more process steps during the papermaking process, wherein alkenyl succinic anhydride Is not added in the one or more process steps via a surface treatment,

wherein the one or more process steps during the papermaking process are selected from a process step at a forming section of the paper machine, a process step at a multilayer paperboard combining section, a process step at a press section, a process step at a drying section, a process step at a surface sizing section, and a combination thereof,

wherein the aluminum salt is added to the papermaking process in an amount greater than 0.3 kilograms per ton of paper, and the alkenyl succinic anhydride is added in an amount of at least 0.9 kilograms per ton of paper.

2. The sizing method of claim 1 , wherein the one or more process steps during the papermaking process is a process step at a surface sizing section.

3. The sizing method of claim 1 , wherein the alkenyl succinic anhydride has the following structure

wherein, R 1 and R 2 are alkyl.

4. The sizing method of claim 3 , wherein each of R 1 and R 2 is C 12 -C 22 alkyl.

5. The sizing method of claim 1 , wherein the alkenyl succinic anhydride is added to the papermaking furnish as an emulsion.

6. The sizing method of claim 1 , wherein the papermaking furnish has a pH of from 4 to 9 before the addition of alkenyl succinic anhydride.

7. The sizing method of claim 1 , wherein the aluminum salt is alum, aluminum chloride, polyaluminum chloride, or a combination thereof.

8. The sizing method of claim 1 , wherein the aluminum salt is added to the papermaking process in an amount of from 0.3 kilograms to 3 kilograms per ton of paper.

9. The sizing method of claim 1 , wherein the aluminum salt is added to the papermaking process in combination with an alkyl ketene dimer (“AKD”).

10. The sizing method of claim 9 , wherein the aluminum salt is alum, aluminum sulfate, aluminum chloride, polyaluminum chloride or a combination thereof.

11. The sizing method of claim 1 , wherein the aluminum salt is added to the papermaking process in combination with a starch.

12. The sizing method of claim 11 , wherein the aluminum salt is alum, aluminum sulfate, aluminum chloride, polyaluminum chloride or a combination thereof.

13. A sizing method for making paper, the method comprising:

adding alkenyl succinic anhydride to a papermaking furnish in a papermaking process, and

adding an aluminum salt to one or more process steps during the papermaking process via surface treatment,

wherein the surface treatment comprises spraying the aluminum salt onto a surface of a paper sheet in the one or more process steps during the papermaking process, wherein alkenyl succinic anhydride Is not added in the one or more process steps via a surface treatment,

wherein the one or more process steps during the papermaking process are selected from a process step at a forming section of the paper machine, a process step at a multilayer paperboard combining section, a process step at a press section, a process step at a drying section, a process step at a surface sizing section, and a combination thereof,

wherein the aluminum salt is added to the papermaking process in an amount of at least 10 kilograms per ton of paper, and the alkenyl succinic anhydride is added in an amount of up to and including 5 kilograms per ton of paper.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 9, 2018
From: CHEN, ZHI; XIAO, JINHAI; ZHANG, XIAOFENG; HOU, KUN; THOMAS, JAMES L.; HUANG, KAIHONG
To: ECOLAB USA INC.
Reel/Frame 046599/0829 →
Priority Claims (1)
CN 2015 1 0994194 · Dec 25, 2015 · national
Continuity (1)
Related Publication 20190003125A1 · Jan 3, 2019