IP Library Granted Patent US 11,053,566
Granted Patent B2
US 11,053,566 · App. 16/671,323 · Granted Jul 6, 2021

System and method including multi-circuit solution extraction for recovery of metal values from metal-bearing materials

Inventors: Jason M Morgan (Morenci, AZ); Barbara J Savage (Silver City, NM); David G Meadows (Phoenix, AZ); Wayne W Hazen (Lakewood, CO)
Assignee: FREEPORT MINERALS CORPORATION
C22B3/02B01D11/028B01D11/0488C22B3/0005C22B3/20C22B3/44C25C7/00Y02P10/20
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,053,566
App. No.
16/671,323
Granted
Jul 6, 2021
Kind
B2
Abstract

The present disclosure relates to a metal recovery process comprising a solvent extraction process. In an exemplary embodiment, the solution extraction system comprises a plant with a first and second circuit. A high-grade pregnant leach solution (“HGPLS”) is provided to the first and second circuit, and a low-grade pregnant leach solution (“LGPLS”) is provided to the second circuit. The first circuit produces a rich electrolyte, which can be forwarded to a primary metal recovery, and a low-grade raffinate, which can be forwarded to a secondary metal recovery process. The second circuit produces a rich electrolyte, which can also be forwarded to the primary metal recovery process. The first and second circuits are in fluid communication with each other.

Claims (25)

1. A method of extracting a metal value comprising:

providing a first metal-bearing solution to a first circuit of a solution extraction plant;

providing a second metal-bearing solution to a second circuit of the solution extraction plant, wherein the first circuit comprises at least two first circuit extractors and at least one first circuit stripping unit, and wherein the second circuit comprises at least two second circuit extractors and at least one second circuit stripping unit, and wherein the first circuit and the second circuit are in fluid communication.

2. The method of claim 1 , wherein the first metal-bearing solution is a pregnant leach solution comprising a higher concentration of metal than the second metal-bearing solution.

3. The method of claim 1 , wherein a first portion of the first metal-bearing solution is provided to the first circuit, a second portion of the first metal-bearing solution is provided to the second circuit, and the second metal-bearing solution is provided to the second circuit.

4. The method of claim 1 , wherein the first metal-bearing solution and the second metal-bearing solution comprise copper.

5. The method of claim 1 , wherein the first circuit further comprises a third first circuit extractor.

6. The method of claim 1 , further comprising forwarding a second circuit raffinate to the first circuit by the second circuit.

7. The method of claim 1 , wherein an output of at least one of the first circuit extractors is a high-grade raffinate.

8. The method of claim 1 , further comprising forwarding a lean electrolyte to a second first circuit stripping unit.

9. The method of claim 1 , further comprising forming a first circuit electrolyte by a first circuit stripper and forming a second circuit electrolyte by a second circuit stripper.

10. A method of extracting a metal value comprising:

providing a first metal-bearing solution to a solution extraction plant comprising a first circuit and a second circuit, wherein the first circuit comprises at least two first circuit extractors and at least one first circuit stripping unit, and wherein the second circuit comprises at least two second circuit extractors and at least one second circuit stripping unit, and wherein the first circuit and the second circuit are in fluid communication with each other;

forwarding a first electrolyte to a primary electrowinning unit; and

forwarding a second electrolyte to a second electrowinning unit.

11. The method of claim 10 , further comprising forwarding a second metal-bearing solution to the solution extraction plant.

12. The method of claim 11 , wherein the first metal-bearing solution is provided to the first circuit and the second metal-bearing solution is provided to the second circuit.

13. The method of claim 12 , wherein a first portion of the first metal-bearing solution is provided to the first circuit, a second portion of the first metal-bearing solution is provided to the second circuit, and the second metal-bearing solution is provided to the second circuit.

14. The method of claim 13 , where the first portion of the first metal-bearing solution comprises a first barren organic stream.

15. The method of claim 14 , wherein the second portion of the first metal-bearing solution comprises a second barren organic stream.

16. The method of claim 10 , wherein the first metal-bearing solution is a high-grade pregnant leach solution.

17. The method of claim 11 , wherein the second metal-bearing solution is a low-grade pregnant leach solution.

18. The method of claim 10 , wherein the first electrolyte is a rich electrolyte.

19. The method of claim 10 , wherein the second electrolyte is a rich electrolyte.

20. The method of claim 11 , wherein the first metal-bearing solution and the second metal-bearing solution comprise copper.

Assignments (3)
CHANGE OF NAME Recorded Dec 3, 2019
From: FREEPORT-MCMORAN CORPORATION
To: FREEPORT MINERALS CORPORATION
Reel/Frame 051162/0747 →
MERGER Recorded Nov 26, 2019
From: FREEPORT-MCMORAN CORPORATION
To: FREEPORT-MCMORAN CORPORATION
Reel/Frame 051117/0592 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 25, 2019
From: MORGAN, JASON M; SAVAGE, BARBARA J; MEADOWS, DAVID G; HAZEN, WAYNE W
To: FREEPORT-MCMORAN CORPORATION
Reel/Frame 051102/0267 →
Continuity (4)
Continuation 16020405 · Jun 27, 2018
Continuation 14920768 · Oct 22, 2015
Division 13331717 · Dec 20, 2011
Related Publication 20200063236A1 · Feb 27, 2020