IP Library Granted Patent US 11,148,870
Granted Patent B2
US 11,148,870 · App. 17/123,676 · Granted Oct 19, 2021

Methods of forming repulpable containers

Inventors: Alan B. Collison (Pierce, NE); Reid Borgman (Norfolk, NE)
Assignee: Pratt Retail Specialties, LLC
B65D81/3823B32B7/14B32B27/32B32B29/005B32B29/02B32B29/08B65D5/0227B65D27/00B65D27/005B65D81/3858B32B2260/028B32B2260/046B32B2398/20B65D2565/384B65D2565/385Y02W30/80Y02W90/10
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 11,148,870
App. No.
17/123,676
Granted
Oct 19, 2021
Kind
B2
Abstract

A method of forming a shipping container includes mixing paper fibers with a binder fiber to form a mixture; disposing the mixture onto a surface to form a layer of the mixture; applying heat to form a paper fiber batt from the mixture having a fixed width and fixed length; and inserting the paper fiber batt within an interior of a corrugated box.

Claims (28)

1. A method of forming a shipping container comprising: mixing paper fibers with about 0.5% to 25% by weight meltable thermoplastic binder fiber to form a mixture, wherein the thermoplastic binder fiber has a length of between about 0.5 mm to about 16 mm; disposing the mixture onto a surface to form a layer of the mixture; applying heat to form a paper fiber batt from the mixture having a fixed width and fixed length; and coupling the paper fiber batt to a corrugated box, wherein subjecting the shipping container to a repulpability test produces a fiber yield of greater than 85%, wherein the repulpability test follows requirements set by Fibre Box Association of Elk Grove Village, Ill., and recited in Voluntary Standard For Repulping and Recycling Corrugated Fiberboard Treated to Improve Its Performance in the Presence of Water and Water Vapor as revised on Aug. 16, 2013.

2. The method according to claim 1 , wherein mixing the paper fibers with a binder fiber comprises mixing the paper fibers with a meltable PE/PP bi-component thermoplastic binder fiber.

3. The method according to claim 2 , wherein the thermoplastic binder fibers make up less than 10% by weight of the paper fiber batt.

4. The method according to claim 1 , wherein applying heat to form a paper fiber batt further comprises applying pressure with the heat to form the paper fiber batt.

5. The method according to claim 1 , wherein the step of coupling the paper fiber batt to a corrugated box comprises inserting the paper fiber batt in an interior of the box.

6. A method of forming a shipping container comprising: mixing paper fibers with about 0.5% to 25% by weight meltable PE/PP bi-component binder fiber to form a mixture, wherein the binder fiber has a length of between about 0.5 mm to about 16 mm; disposing the mixture onto a surface to form a layer of the mixture; applying heat to form a paper fiber batt from the mixture having a fixed width and fixed length; and inserting the paper fiber batt within an interior of a corrugated box, wherein subjecting the shipping container to a repulpability test produces a fiber yield of greater than 85%, wherein the repulpability test follows requirements set by Fibre Box Association of Elk Grove Village, Ill., and recited in Voluntary Standard For Repulping and Recycling Corrugated Fiberboard Treated to Improve Its Performance in the Presence of Water and Water Vapor as revised on Aug. 16, 2013.

7. The method according to claim 6 , wherein subjecting the binder fibers make up less than 10% by weight of the paper fiber batt.

8. The method according to claim 6 , wherein applying heat to form a paper fiber batt further comprises applying pressure with the heat to form the paper fiber batt.

9. The method according to claim 6 , further comprising the step of encapsulating the paper fiber batt within a paper layer.

10. The method according to claim 9 , further comprising the step of connecting a first paper layer to a second paper layer to form the paper layer encapsulating the paper fiber batt.

11. A method of forming a shipping container comprising:

mixing paper fibers with about 0.5% to 25% by weight meltable thermoplastic binder fiber to form a mixture;

disposing the mixture onto a surface to form a layer of the mixture, the mixture having a density of 1300 to 1600 grams per square meter;

applying heat to form a paper fiber batt from the mixture having a fixed width and fixed length;

encapsulating the paper fiber batt within a paper layer; and

folding the encapsulated paper fiber batt to form a bottom of the shipping container along the fold and also to define lateral edges adjacent to the bottom and a top arranged opposite to the bottom, the top defining an opening, wherein subjecting the shipping container to a repulpability test produces a fiber yield of greater than 85%.

12. The method according to claim 11 , further comprising the step of sealing at least two lateral edges of the paper layer.

13. The method according to claim 12 , wherein the lateral edges are sealed by heat sealing.

14. The method according to claim 11 , wherein the step of encapsulating the paper fiber batt within the paper layer comprises securing a first paper layer to a second paper layer with the paper fiber batt located between the first paper layer and the second paper layer.

15. The method according to claim 11 , wherein the thermoplastic binder fibers make up less than 10% by weight of the paper fiber batt.

16. A method of forming a shipping container, the method comprising: mixing paper fibers with about 0.5% to 25% by weight meltable PE/PP bi-component binder fiber to form a mixture, the binder fibers being of a length of less than about 24 millimeters; applying heat to form a paper fiber ball from the mixture having a fixed width and fixed length; forming a shipping container from a paper medium, the shipping container defining an interior; securing a paper layer to the paper fiber batt; and surrounding the interior of the shipping container with the paper fiber batt, wherein subjecting the shipping container to a repulpability test produces a fiber yield of greater than 85%, wherein the repulpability test follows requirements set by Fibre Box Association of Elk Grove Village, Ill., and recited in Voluntary Standard For Repulping and Recycling Corrugated Fiberboard Treated to Improve Its Performance in the Presence of Water and Water Vapor as revised on Aug. 16, 2013.

17. The method of claim 16 , wherein the step of securing the paper layer to the paper fiber batt comprises encapsulating the paper fiber batt within the paper layer.

18. The method of claim 17 , wherein the step of forming the shipping container from the paper medium comprises folding the encapsulated paper fiber batt to form a bottom of the shipping container along the fold and also to define lateral edges adjacent to the bottom and a top arranged opposite to the bottom, the top defining an opening.

19. The method of claim 16 , wherein the thermoplastic binder fiber has a length of between about 0.5 mm to about 16 mm.

20. The method of claim 16 , wherein the step of forming the shipping container from the paper medium comprises forming a corrugated box, and wherein the step of securing the paper layer to the paper fiber batt comprises coupling the paper fiber batt to the corrugated box.

21. The method of claim 16 , wherein the PE/PP bi-component binder fiber makes up less than 10% by weight of the paper fiber batt.

22. The method of claim 16 , wherein about 50% of the PE/PP bi-component binder fiber has a length of about 1 millimeter and about 50% of the PE/PP bi-component binder fiber has a length of about 6 millimeters.

23. The method according to claim 6 , wherein the paper fiber batt has a thickness that is at least 1/16 inch.

Assignments (1)
AMENDED AND RESTATED GRANT OF SECURITY INTEREST Recorded Dec 17, 2021
From: PRATT RETAIL SPECIALTIES, LLC
To: WELLS FARGO BANK, NATIONAL ASSOCIATION, AS ADMINISTRATIVE AGENT
Reel/Frame 058535/0927 →
Continuity (6)
Continuation 16414310 · May 16, 2019
Division 15677738 · Aug 15, 2017
Provisional Application 62375555 · Aug 16, 2016
Provisional Application 62419894 · Nov 9, 2016
Provisional Application 62437365 · Dec 21, 2016
Related Publication 20210101735A1 · Apr 8, 2021
Cited By (16)
US 12,195,266 US 12,270,153 US 12,286,285 US 12,286,286 US 12,297,016 US 12,298,060 US 12,305,911 US 12,344,454 US 12,365,529 US 12,415,649 US 12,504,220 US 12,515,870 US 12,565,371 US 12,656,050 US 12,668,412 US 12,709,453