Lubricant formulations
A composition for lubricant formulations is disclosed. The composition may include hypochlorite, dimethicone, and an emulsifier for improvement of lubricity. Methods of making and using the lubricant formulations are also disclosed.
1. A lubricant, comprising:
an electrolyzed saline solution;
a rheology modifier; and
a polymeric organosilicon compound; and wherein the rheology modifier comprises sodium magnesium silicate.
2. The lubricant of claim 1 , wherein the saline solution comprises sodium chloride present in an amount of about 0.1% to about 0.4% w/v.
3. The lubricant of claim 1 , wherein the sodium chloride is present in an amount of about 0.28% w/v.
4. The lubricant of claim 1 , wherein the electrolyzed saline solution comprises hypochlorite present in an amount of about 10 to about 300 ppm.
5. The lubricant of claim 1 , wherein the polymeric organosilicon compound is dimethicone.
6. The lubricant of claim 1 , wherein the polymeric organosilicon compound is present in an amount of about 0.5% to about 50% w/v.
7. The lubricant of claim 1 , wherein the polymeric organosilicon compound is present in an amount of about 10% w/v.
8. The lubricant of claim 1 , wherein the rheology modifier is present in an amount of about 0.1% to about 15% w/v.
9. The lubricant of claim 1 , wherein the rheology modifier is present in an amount of about 3.25% w/v.
10. The lubricant of claim 1 , further comprising a buffer or water.
11. The lubricant of claim 10 , wherein the buffer is present in an amount of about 0.05% to about 15% w/v.
12. A method of making a lubricant of claim 1 , comprising:
electrolyzing a saline solution to generate a solution comprising hypochlorite;
providing a polymeric organosilicon compound; and
mixing the solution comprising hypochlorite with the polymeric organosilicon compound to form a lubricant.
13. The method of claim 12 , wherein the saline solution comprises sodium chloride present in an amount of about 0.1% to about 0.4% w/v.
14. The method of claim 12 , wherein the polymeric organosilicon compound is present in an amount of about 0.5% to about 50% w/v.
15. The method of claim 12 , further comprising mixing the lubricant with a rheology modifier, and wherein the rheology modifier comprises sodium magnesium silicate.
16. The method of claim 12 , wherein the hypochlorite is present in an amount ranging from about 10 to about 300 ppm.
17. The method of claim 12 , further comprising mixing the lubricant with water.