IP Library › Granted Patent US 7,557,500
Granted Patent B2
US 7,557,500 · App. 10/513,229 · Granted Jul 7, 2009

Electroluminescent element and method for manufacturing the same

Assignee: Dai Nippon Printing Co., Ltd.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,557,500
App. No.
10/513,229
Granted
Jul 7, 2009
Kind
B2
Abstract

A main object of the present invention is to provide an EL element in which an inconvenience, resulting from uneven film thickness or generation of small clearances at a boundary in between layers due to a liquid repellent treatment, is prevented. In order to achieve the object, the present invention provides an electroluminescent element comprising: a substrate having at least a first electrode layer; an insulating layer formed so as to cover an edge portion of the first electrode layer; a liquid repellent portion provided on an upper surface of the insulating layer; alight emitting layer formed in a pattern on the first electrode layer; and a second electrode layer formed on the light emitting layer.

Claims (38)

1. An electroluminescent element comprising:

a substrate having at least a first electrode layer;

an insulating layer formed so as to cover an edge portion of the first electrode layer;

a liquid repellent portion provided only on an upper surface of the insulating layer;

a light emitting layer formed in a pattern on the first electrode layer; and

a second electrode layer formed on the light emitting layer, wherein the width of the liquid repellant portion is in a range of 0.2 times to 0.9 times the width of the insulating layer, and is formed at the center portion of the insulating layer, and further

wherein the light emitting layer is formed to creep up to end portions of an upper surface of the insulating layer.

2. The electroluminescent element according to claim 1 , wherein a contact angle difference, to a coating solution having a 30 mN/m surface tension, between the liquid repellent portion and the insulating layer is 10° or more.

3. An electroluminescent element comprising:

a substrate having at least a first electrode layer;

an insulating layer formed so as to cover an edge portion of the first electrode layer;

a photocatalyst containing layer, formed on the first electrode layer and the insulating layer, composed of at least a photocatalyst and a binder;

a light emitting layer formed in a pattern on the photocatalyst containing layer; and

a second electrode layer formed on the light emitting layer,

wherein only a portion of the phatocatalyst containing layer, which is located on an upper surface of the insulating layer, Is a liquid repellent portion having liquid repellency, and the remaining portion of the photocatalyst containing layer is a lyophilic portion having liophilicity, and

the light emitting layer is formed on the lyophilic portion, and

wherein the width of the liquid repellant portion is in a range of 0.2 times to 0.9 times the width of the insulating layer, and is formed at the center portion of the insulating layer, and further

wherein a contact angle difference, to a coating solution having a 30 mN/m surface tension, between the liquid repellent portion and the lyophillic portion is 10° or more.

4. The electroluminescent element according to claim 3 , wherein the photocatalyst is one kind or two or more kinds of substances selected from a titanium oxide (TiO 2 ), a zinc oxide (ZnO), a tin oxide (SnO 2 ), a strontium titanate (SrTiO 3 ), tungsten oxide (WO 3 ), bismuth oxide (Bi 2 O 3 ) and an iron oxide (Fe 2 O 3 ).

5. The electroluminescent element according to claim 4 , wherein the photocatalyst is the titanium oxide.

6. The electroluminescent element according to claim 3 , wherein the binder is an organo polysiloxane as a hydrolyzed condensate or a cohydrolyzed condensate of one kind or two or more kinds of silicon compounds represented by Y n SiX (4-n) (Here, Y is an alkyl group, a fluoro alkyl group, a vinyl group, an amino group, a phenyl group or an epoxy group, X is an alkoxyl group or a halogen, and n is an integer from 0 to 3.).

7. A method for manufacturing an electroluminescent element, at least comprising processes of:

forming an insulating layer in a pattern, on a substrate having at least a first electrode layer, so as to cover an edge portion of the first electrode layer;

forming a photocatalyst containing layer, on the substrate having the insulating layer provided thereon, comprising at least a photocatalyst and a binder, and whose wettability is varied by an energy irradiation;

forming a liquid repellent portion, which is a non-energy irradiated area, and a lyophilic portion, which is an energy iraddiated area, by irradiating the photocatalyst containing layer in a pattern so as only an upper surface of the insulating layer maintains liquid repellency;

forming a light emitting layer by coating the lyophilic portion with a light emitting layer forming coating solution; and

forming a second electrode layer on the light emitting layer,

wherein the pattern irradiation is carried out so as to form the width of the liquid repellant portion in a range of 0.2 times to 0.9 times the width of the insulating layer, and at the center portion of the insulating layer, and further

wherein a contact angle difference, to a coating solution having a 30 mN/m surface tension, between the liquid repellent portion and the lyophillic portion is 10° or more.

8. A method for manufacturing an electroluminescent element, comprising processes of;

forming an insulating layer in a pattern, on a substrate having at least a first electrode layer, so as to cover an edge portion of the first electrode layer;

forming a resist layer by coating the substrate, having at least the first electrode layer and the insulating layer, with a photosensitive resin containing fluorine;

forming a liquid repellent portion of the resist layer by forming the resist layer only on an upper surface of the insulating layer, irradiating the resist layer, in a pattern via a photomask, and developing;

forming a light emitting layer at least on the first electrode layer of the substrate having the first electrode layer, the insulating layer and the liquid repellent portion provided thereon; and

forming a second electrode layer on the light emitting layer,

wherein the pattern irradiation is carried out so as to form the width of the liquid repellant portion in a range of 0.2 times to 0.9 times the width of the insulating layer, and at the center portion of the insulating layer, and further

wherein the light emitting layer is formed to creep up to end portions of an upper surface of the insulating layer.

9. The method for manufacturing an electroluminescent element according to claim 8 , wherein a contact angle difference, to a coating solution having a 30 mN/m surface tension, between the liquid repellent portion and the insulating layer is 10° or more.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 2, 2004
From: NAKAMURA, NORIKATSU; KOBAYASHI, YOSHIHIRO
To: DAI NIPPON PRINTING CO., LTD.
Reel/Frame 016469/0016 →
Priority Claims (1)
JP 2002-131796 · May 7, 2002 · national
Continuity (1)
Related Publication 20050168140A1 · Aug 4, 2005