IP Library Granted Patent US 7,724,241
Granted Patent B2
US 7,724,241 · App. 11/133,270 · Granted May 25, 2010

Touch panel

Assignee: Panasonic Corporation
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,724,241
App. No.
11/133,270
Granted
May 25, 2010
Kind
B2
Abstract

The invention relates to touch panels for use in a variety of electronic apparatuses, and designed to prevent separation of a lower substrate and an antireflection layer, and to ensure reliable operation. An undercoat layer ( 9 ) made of any of silicon oxide and a compound having a principal ingredient of silicon oxide is disposed between the antireflection layer ( 5 ) and the lower substrate ( 2 ) made of glass having the same principal ingredient of silicon oxide, to improve strength of adhesion between the lower substrate ( 2 ) and the antireflection layer ( 5 ), thereby preventing separation of the antireflection layer ( 5 ) from the lower substrate ( 5 ), and providing the touch panel with reliable operation.

Claims (11)

1. A touch panel comprising:

an upper substrate having an upper conductive layer formed on one of main surfaces of the upper substrate,

a lower substrate having a lower conductive layer formed on one of main surfaces of the lower substrate in a manner to face the upper conductive layer with a predetermined space, the lower substrate being glass having silicon oxide as a main principal ingredient;

an antireflection layer formed between the lower conductive layer and the lower substrate; and

an undercoat layer, made of any of silicon oxide and a compound having silicon oxide as a principal ingredient, disposed between the antireflection layer and the lower substrate,

wherein the undercoat layer directly contacts both the antireflection layer and the lower substrate so as to enhance bonding strength between the antireflection layer and the lower substrate,

wherein surface roughness of a main surface of the lower conductive layer has an Ra value of 0.7 nm to 2 nm, and

wherein the undercoat layer has a thickness of 5 to 30 nm.

2. The touch panel according to claim 1 , wherein the undercoat layer has a thickness of 15 to 20 nm.

3. The touch panel according to claim 1 , wherein the antireflection layer comprises a plurality of layers, each having a different refractive index.

4. The touch panel according to claim 1 further comprising another antireflection layer disposed on another main surface of the lower substrate opposite the surface where the antireflection layer and the undercoat layer are formed.

Assignments (2)
CHANGE OF NAME Recorded Nov 24, 2008
From: MATSUSHITA ELECTRIC INDUSTRIAL CO., LTD.
To: PANASONIC CORPORATION
Reel/Frame 021897/0707 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 20, 2005
From: FUKUI, TOSHIHARU; YAMAUE, NOBUHIRO; TAKABATAKE, KENICHI
To: MATSUSHITA ELECTRIC INDUSTRIAL CO., LTD.
Reel/Frame 016588/0339 →
Priority Claims (1)
JP 2004-212719 · Jul 21, 2004 · national
Continuity (1)
Related Publication 20060017707A1 · Jan 26, 2006