IP Library › Granted Patent US 7,919,064
Granted Patent B2
US 7,919,064 · App. 12/366,993 · Granted Apr 5, 2011

Capture and sequestration of carbon dioxide in flue gases

Assignee: Michigan Technological University
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,919,064
App. No.
12/366,993
Granted
Apr 5, 2011
Kind
B2
Abstract

There is provided a process for the capture and sequestration of carbon dioxide that would otherwise enter the atmosphere and contribute to global warming and other problems. CO 2 capture is accomplished by reacting carbon dioxide in flue gas with an alkali metal carbonate, or a metal oxide, particularly containing an alkaline earth metal or iron, to form a carbonate salt. A preferred carbonate for CO 2 capture is a dilute aqueous solution of additive-free (Na 2 CO 3 ). Other carbonates include (K 2 CO 3 ) or other metal ion that can produce both a carbonate and a bicarbonate salt. Examples of suitable metal oxides include several alkaline earths including CaO and MgO. The captured CO 2 is preferably sequestered using any available mineral or industrial waste that contains calcium magnesium or iron in non-carbonate forms, or iron in the Fe +2 oxidation state.

Claims (22)

1. A method of capturing and sequestering carbon dioxide in carbon dioxide bearing gases of interest comprising:

(a) capturing carbon dioxide by reacting a gas of interest with an aqueous sodium carbonate solution to form a bicarbonate solution; and

(b) sequestering said captured CO 2 by reacting with a material selected from waste materials containing a metal selected from alkaline earth metals including calcium and magnesium, and iron in non-carbonate form or mixtures thereof.

2. A method as in claim 1 wherein said waste material is selected from the group consisting of cement kiln dust (CKD), fly-ash, iron slag, minerals and combinations thereof.

3. A method as in claim 2 wherein said waste material includes calcium oxide (CaO).

4. A method as in claim 2 wherein said waste material includes fly-ash.

5. A method as in claim 1 wherein said waste material includes calcium oxide (CaO).

6. A method as in claim 1 wherein said waste material includes fly-ash.

7. A method as in claim 1 wherein said carbon dioxide bearing gas of interest is selected from electric power plant and cement kiln effluent.

8. A method as in claim 1 wherein (b) involves a direct reaction of said bicarbonate solution with said waste material.

9. A method as in claim 8 including recycling a portion of said carbonate solution regenerated in said sequestering.

10. A method as in claim 8 wherein said waste material is selected from the group consisting of cement kiln dust (CKD), fly-ash, iron slag, minerals and combinations thereof.

11. A method as in claim 1 wherein said waste material includes material selected from the group consisting of wollastonite (CaSiO 3 ); any of the pyroxene minerals diopside (MgCaSi 2 O 6 ), hedenbergite (FeCaSi 2 O 6 ), augite ((Ca,Mg,Fe)SiO 3 ), pigeonite ((Ca,Mg,Fe)(Mg,Fe) Si 2 O 6 ), clinoenstatite (Mg 2 Si 2 O 6 ), or clinoferrosilite (Fe 2 Si 2 O 6 ) serpentine minerals ((Mg,Fe) 3 Si 2 O 5 (OH) 4 ); and epidote (Ca 2 Al 2 (Fe,Al)(SiO 4 )(Si 2 O 7 )O(OH)).

12. A method as in claim 1 wherein said carbonate solution is additive-free.

13. A method as in claim 1 wherein said aqueous carbonate solution contains from about 1% to 5% w/w sodium carbonate.

14. A method as in claim 13 wherein said aqueous carbonate solution contains from about 1.125% to 2.75% w/w sodium carbonate.

15. A method as in claim 1 wherein said aqueous carbonate solution contains about 2% w/w sodium carbonate.

16. A method as in claim 8 wherein said capture and said sequestration occur in the same vessel.

17. A method of capturing and sequestering carbon dioxide in carbon dioxide bearing gases of interest comprising:

(a) capturing carbon dioxide by reacting a gas of interest with an aqueous alkali metal carbonate solution to form a bicarbonate solution wherein said carbonate is selected from the group consisting of sodium carbonate and potassium carbonate; and

(b) releasing said CO 2 from said bicarbonate solution by heating said bicarbonate solution and storing said released CO 2 under stable conditions.

18. A method as in claim 17 wherein said aqueous alkali metal carbonate solution is a dilute solution of sodium carbonate.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 13, 2009
From: KAWATRA, SURENDRA KOMAR; EISELE, TIMOTHY C.; SIMMONS, JOHN J.
To: MICHIGAN TECHNOLOGICAL UNIVERSITY
Reel/Frame 022262/0828 →
Continuity (3)
Provisional Application 61065413 · Feb 12, 2008
Provisional Application 61124474 · Apr 17, 2008
Related Publication 20090202410A1 · Aug 13, 2009