IP Library › Granted Patent US 7,994,558
Granted Patent B2
US 7,994,558 · App. 11/510,709 · Granted Aug 9, 2011

Method for forming barrier metal layer of bit line in semiconductor memory device

Assignee: Hynix Semiconductor Inc.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 7,994,558
App. No.
11/510,709
Granted
Aug 9, 2011
Kind
B2
Abstract

A semiconductor memory device includes a titanium layer and a titanium nitride layer formed on a substrate, a thin layer formed on the titanium nitride layer, and a metal layer formed on the thin layer, wherein the thin layer increases a grain size of the metal layer.

Claims (9)

1. A method for fabricating a semiconductor memory device, comprising:

sequentially forming a titanium layer and a titanium nitride layer over a substrate;

forming a thin layer on the titanium nitride layer; and

forming a metal layer on the thin layer, wherein forming the thin layer increases a grain size of the metal layer;

wherein forming the thin layer comprises forming an amorphous layer by performing an atomic layer deposition (ALD) method and the amorphous layer has a thickness ranging from approximately 50 Å to approximately 200 Å and the amorphous layer remains as an amorphous layer in the semiconductor memory device.

2. The method of claim 1 , wherein forming the metal layer comprises forming a tungsten layer, and forming the amorphous layer comprises forming a tungsten silicide layer.

3. The method of claim 1 , wherein forming the amorphous layer comprises forming the amorphous layer from a material selected from a group consisting of tantalum silicide (TaSi x ), titanium silicide (TiSi x ), molybdenum silicide (MoSi x ), hafnium silicide (HfSi x ), zirconium silicide (ZrSi x ), cobalt silicide (CoSi x ), chrome silicide (CrSi x ), nickel silicide (NiSi x ), tungsten silicon nitride (W—Si—N), tantalum silicon nitride (Ta—Si—N), titanium silicon nitride (Ti—Si—N), molybdenum silicon nitride (Mo—Si—N), hafnium silicon nitride (Hf—Si—N), and zirconium silicon nitride (Zr—Si—N).

4. The method of claim 1 , wherein forming the metal layer comprises forming the metal layer from a material selected from a group consisting of tantalum (Ta), titanium (Ti), molybdenum (Mo), hafnium (HO, cobalt (Co), chrome (Cr), nickel (Ni), platinum (Pt), and ruthenium (Ru).

5. The method of claim 1 , further comprising forming an amorphous tungsten nitride (WN) layer between the amorphous layer and the metal layer.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 28, 2006
From: LIM, KWAN-YONG; SUNG, MIN-GYU; CHO, HEUNG-JAE
To: HYNIX SEMICONDUCTOR INC.
Reel/Frame 018252/0813 →
Priority Claims (1)
KR 10-2005-0079535 · Aug 29, 2005 · national
Continuity (1)
Related Publication 20070045854A1 · Mar 1, 2007