IP Library Granted Patent US 8,053,019
Granted Patent B2
US 8,053,019 · App. 12/699,127 · Granted Nov 8, 2011

Thermal treatment of a drug eluting implantable medical device

Assignee: Advanced Cardiovascular Systems, Inc.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,053,019
App. No.
12/699,127
Granted
Nov 8, 2011
Kind
B2
Abstract

A coating and a method of coating an implantable medical device, such as a stent, is disclosed. The method includes subjecting the coating to a thermal condition such as a temperature above the glass transition temperature of a polymer included in the coating.

Claims (33)

1. A method of manufacturing a drug delivery stent, the method comprising:

forming a dry polymeric coating on a stent having less than about 2% residual fluid content (w/w), the dry polymeric coating comprising a reservoir layer comprising a polymer and an active agent, and a barrier layer comprising a polymer covering a portion of the reservoir layer; and

subjecting the polymer of the barrier layer to a heat treatment at a temperature equal to or greater than the glass transition of the polymer of the barrier layer;

wherein the polymer of the barrier layer comprises an ethylene vinyl alcohol copolymer, an ethylene-vinyl acetate copolymer, poly(butylmethacrylate), or a combination thereof.

2. The method of claim 1 , wherein the active agent is rapamycin, 40-O-(2-hydroxy)ethyl-rapamycin, or a functional analog or structural derivative thereof.

3. The method of claim 1 , wherein the glass transition temperature of the polymer of the barrier layer is greater than the glass transition temperature of the polymer of the reservoir layer.

4. The method of claim 1 , wherein the glass transition temperature of the polymer of the barrier layer is lower than the glass transition temperature of the polymer of the reservoir layer.

5. The method of claim 1 , wherein the glass transition temperature of the polymer of the barrier layer is about the same as the glass transition temperature of the polymer of the reservoir layer.

6. The method of claim 1 , wherein the temperature of the heat treatment is less than the melting temperature of the polymer of the barrier layer.

7. The method of claim 1 , wherein the temperature of the heat treatment is less than the melting temperature of the polymer of the reservoir layer.

8. The method of claim 1 , wherein the temperature of the heat treatment is equal to the glass transition temperature of the polymer of the barrier layer plus the melting temperature of the polymer of the barrier layer, divided by 2.

9. The method of claim 1 , wherein the temperature of the heat treatment is equal to 0.9 times the melting temperature of the polymer of the barrier layer, wherein the melting temperature of the polymer of the barrier layer is expressed in Kelvin.

10. The method of claim 1 , wherein the glass transition temperature of the polymer of the barrier layer is above room temperature.

11. A method of manufacturing a drug delivery stent, the method comprising:

forming a polymeric coating on a stent, the polymeric coating comprising a reservoir layer comprising a polymer and an active agent, and a barrier layer comprising a semicrystalline polymer covering a portion of the reservoir layer; and

exposing the polymer of the barrier layer to the crystallization temperature of The polymer of the barrier layer.

12. The method of claim 11 , wherein the polymeric coating comprises less than about 2% residual fluid content (w/w).

13. The method of claim 11 , wherein the active agent is rapamycin, 40-O-(2-hydroxy)ethyl-rapamycin, or a functional analog or structural derivative thereof.

14. The method of claim 11 , wherein the polymer of the reservoir layer is a semicrystalline polymer and wherein the crystallization temperature of the polymer of the barrier layer is greater than the crystallization temperature of the polymer of the reservoir layer.

15. The method of claim 11 wherein the polymer of the reservoir layer is a semicrystalline polymer and wherein the crystallization temperature of the polymer of the barrier layer is less than the crystallization temperature of the polymer of the reservoir layer.

16. The method of claim 11 , wherein the polymer of the reservoir layer is a semicrystalline polymer and wherein the crystallization temperature of the polymer of the barrier layer is equal to the crystallization temperature of the polymer of the reservoir layer.

17. A method of manufacturing a drug delivery stent, the method comprising:

forming a dry polymeric coating on a stent having less than about 2% residual fluid content (w/w), the dry polymeric coating comprising a reservoir layer comprising a polymer and an active agent, and a barrier layer comprising a polymer covering a portion of the reservoir layer; and

subjecting the polymer of the barrier layer to a heat treatment at a temperature equal to or greater than the glass transition of the polymer of the barrier layer;

wherein the glass transition temperature of the polymer of the barrier layer is greater than the glass transition temperature of the polymer of the reservoir layer.

18. A method of manufacturing a drug delivery stent, the method comprising:

forming a dry polymeric coating on a stent having less than about 2% residual fluid content (w/w), the dry polymeric coating comprising a reservoir layer comprising a polymer and an active agent, and a barrier layer comprising a polymer covering a portion of the reservoir layer; and

subjecting the polymer of the barrier layer to a heat treatment at a temperature equal to or greater than the glass transition of the polymer of the barrier layer;

wherein the glass transition temperature of the polymer of the barrier layer is lower than the glass transition temperature of the polymer of the reservoir layer.

19. A method of manufacturing a drug delivery stent, the method comprising:

forming a dry polymeric coating on a stent having less than about 2% residual fluid content (w/w), the dry polymeric coating comprising a reservoir layer comprising a polymer and an active agent, and a barrier layer comprising a polymer covering a portion of the reservoir layer; and

subjecting the polymer of the barrier layer to a heat treatment at a temperature equal to or greater than the glass transition of the polymer of the barrier layer;

wherein the temperature is equal to 0.9 times the melting temperature of the polymer of the barrier layer, wherein the melting temperature of the polymer of the barrier layer is expressed in Kelvin.

Continuity (11)
Division 10603794 · Jun 25, 2003
Continuation In Part 10108004 · Mar 27, 2002
Continuation In Part 10304360 · Nov 25, 2002
Division 09751691 · Dec 28, 2000
Continuation In Part 09750595 · Dec 28, 2000
Continuation In Part 09470559 · Dec 23, 1999
Continuation In Part 09390855 · Sep 3, 1999
Continuation In Part 09390069 · Sep 3, 1999
Continuation In Part 09715510 · Nov 17, 2000
Continuation In Part 09540241 · Mar 31, 2000
Related Publication 20100136213A1 · Jun 3, 2010