IP Library Granted Patent US 8,075,806
Granted Patent B2
US 8,075,806 · App. 12/755,587 · Granted Dec 13, 2011

Solid composition having enhanced physical and electrical properties

Assignee: Kryron Global, LLC
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,075,806
App. No.
12/755,587
Granted
Dec 13, 2011
Kind
B2
Abstract

A method of making a treating wash includes mixing brass granules with acetone, mixing carbon nanotube material, iron pyrite granules and copper granules in the acetone brass mixture, and straining the liquid from the remaining solid material. Methods of treating materials such as brass granules, iron pyrite granules, carbon nanotube material, and brass granules comprises washing the materials in the treating wash, followed by straining and drying the materials.

Claims (11)

1. A method of making a treating wash comprising:

mixing brass granules with acetone;

mixing carbon nanotube material, iron pyrite granules and copper granules in the acetone brass mixture; and

straining the liquid from the remaining solid material.

2. The method of claim 1 further comprising storing the strained solid material.

3. The method of claim 1 wherein:

mixing brass granules with acetone comprises mixing about 454 grams of brass (about 100 mesh or finer) per gallon of acetone in a commercial blender at high speed for about 10 minutes or until a gold color appears at the surface of the acetone when the blender is stopped;

mixing carbon nanotube material comprises mixing about one gram of multi-walled carbon nanotube material per gallon of acetone at high speed for about 5 minutes;

mixing iron pyrite comprises mixing about 33.5 grams of iron pyrite per gallon of acetone, the iron pyrite having an average grain size of about 0.125 inch for a minimum of about 3 minutes at high speed; and

mixing copper comprises mixing about 517 grams of copper per gallon of acetone, the copper having a mesh size of about 35 mesh or finer for about 8 minutes until a slurry begins to form on the surface after the blender is turned off.

4. The method of claim 3 further comprising storing the strained solid material.

Assignments (2)
MERGER Recorded Jun 1, 2014
From: KRYRON GLOBAL, LLC
To: BOURQUE INDUSTRIES, INC.
Reel/Frame 033003/0106 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 22, 2014
From: BOURQUE, JOHN M.
To: KRYRON GLOBAL, LLC
Reel/Frame 032952/0702 →
Continuity (2)