Method for production of calcium compounds

Assignee: Elkem Solar AS
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,268,280
App. No.
12/744,803
Granted
Sep 18, 2012
Kind
B2
Abstract

The present invention relates to a method for production of calcium compounds having very low content of phosphorus and boron from an impure calcium chloride, solution containing phosphorus and boron, which method comprises the following steps: a) addition of a FeCl3-solution to the calcium chloride solution, b) adjusting the pH of the solution by addition of a base to between 3 and 9.5 for precipitation of iron hydroxide, iron phosphate and boron compounds, c) removal of the solid precipitate from the solution in step b) obtaining a purified calcium chloride solution, d) precipitation of a calcium compound from the solution from step c), and e) separation of the calcium compound from the solution in step d).

Claims (15)

1. A method for production of calcium compounds having very low content of phosphorus and boron from an impure calcium chloride solution containing phosphorus and boron, wherein the method comprises the following steps:

a) adding a FeCl 3 -solution to the impure calcium chloride solution;

b) adjusting the pH of the resulting solution from step a) by addition of a base to between 3 and 9.5 for precipitation of iron hydroxide, iron phosphate and boron compounds;

c) removing a solid precipitate of iron hydroxide, iron phosphate and boron compounds from the solution resulting from step b);

d) precipitating a calcium compound from the resulting solution from step c); and

e) separating the calcium compound from the solution resulting from step d), the calcium compound with very low phosphorus and boron content.

2. The method according to claim 1 , wherein the impure calcium chloride solution is produced by dissolving a calcium carbonate source in hydrochloric acid.

3. The method according to claim 1 , wherein the impure calcium chloride solution is waste solutions from chemical processes.

4. The method according to claim 1 , wherein the pH in step b) is adjusted to a value between 7 and 8.5.

5. The method according to claim 1 , wherein a flocculation agent is added to the impure calcium chloride solution in step b).

6. The method according to claim 1 , wherein calcium carbonate is precipitated in step d) by addition of CO 2 -gas and NH 3 to the solution resulting from step c).

7. Method according to claim 1 , characterized in that calcium hydroxide is precipitated in step d) by addition of NaOH to the solution from step c).

8. Method according to claim 1 , characterized in that calcium sulfate is precipitated in step d) by addition of sulfuric acid to the solution from step c).

9. Method according to claim 1 , characterized in that calcium oxalate is precipitated in step d) by addition of oxalic acid to the solution from c).

10. The method according to claim 1 , wherein the calcium compound from step e) is calcined to CaO.

Assignments (2)
CHANGE OF NAME Recorded Mar 20, 2019
From: ELKEM SOLAR AS
To: REC SOLAR NORWAY AS
Reel/Frame 048644/0251 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded May 26, 2010
From: BUSETH, TORFINN; EINAR, ANDERSEN
To: ELKEM SOLAR AS
Reel/Frame 024443/0656 →
Priority Claims (1)
NO 20080569 · Jan 30, 2008 · national
Continuity (1)
Related Publication 20100303707A1 · Dec 2, 2010