Reactive block copolymers

Inventors: Alfonso González Montiel (Atizapán de Zaragoza, MX); Leticia Flores Santos (Metepec, MX); Enrique Saldívar Guerra (Saltillo, MX)
Assignee: CID Centro de Investigación y Desarrollo Tecnológico S.A. de C.V.
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,357,759
App. No.
11/508,407
Granted
Jan 22, 2013
Kind
B2
Abstract

A process for making a block copolymer compatibilizer, comprising reacting an acrylic monomer that has functional groups with one or more vinyl monomers in the presence of a free radical initiator and a stable free radical to form a reaction product that includes residual unreacted acrylic monomer, and reacting one or more vinyl monomers with the reaction product to form a second block that incorporates the residual unreacted acrylic monomer. A blend composition comprising a first thermoplastic polymer, which has functional groups, a reactive block copolymer that has functional groups in two or more blocks, and a second thermoplastic polymer that is compatible with one block of the block copolymer, where the functional groups in the first thermoplastic react with the functional groups in the block copolymer.

Claims (4)

1. A process for making a block copolymer, comprising:

a) reacting an acrylic monomer (selected from the group consisting of glycidyl methacrylate, 2-hydroxyethyl methacrylate, 2-dimethylaminoethyl methacrylate and 2-diethylaminoethyl methacrylate), one or more vinyl monomers, a free radical initiator and a stable free radical to form a reaction product that includes a first block and residual unreacted acrylic monomer; and

b) reacting one or more vinyl monomers with the reaction product from the first step to form a second block that includes the residual unreacted acrylic monomer.

2. The process of claim 1 , wherein the block copolymer has a number average molecular weight between about 25,000 and about 350,000.

Assignments (2)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Apr 10, 2013
From: CID CENTRO DE INVESTIGACION Y DESARROLLO TECNOLOGICO S.A. DE C.V.
To: MACRO-M S.A. DE C.V.
Reel/Frame 030194/0159 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Aug 23, 2006
From: MONTIEL, ALFONSO GONZALEZ; SANTOS, LETICIA FLORES; GUERRA, ENRIQUE SALDIVAR
To: CID CENTRO DE INVESTIGACION DESARROLLO TECNOLOGICO SA
Reel/Frame 018241/0717 →
Continuity (2)
Provisional Application 60711890 · Aug 26, 2005
Related Publication 20070049696A1 · Mar 1, 2007