Process for hydrogenating butadiyne
In the process for hydrogenating butadiyne over a catalyst which comprises at least one platinum group metal on an inorganic metal oxide as a support, the hydrogenation is performed at a pressure in the range from 1 to 40 bar and a temperature in the range from 0 to 100° C., and from 0.05 to 5% by weight, based on the overall catalyst, of platinum group metal is present on the support.
1. A process for hydrogenating butadiyne to butane over a catalyst which comprises at least one platinum group metal on an inorganic metal oxide as a support, said process comprising:
fully hydrogenating butadiyne, via a one-stage process, over the catalyst, at a pressure of from 1 to 40 bar, at a temperature of from 0 to 100° C., and with a liquid circulation system with a weight ratio of recycle stream to feed stream of from 2 to 20,
wherein
from 0.05 to 5% by weight, based on the total weight of the catalyst, of the platinum group metal is present on the support,
the support has a porosity of from 0.2 to 1.0 ml/g,
the hydrogenation is performed on a stream obtained from gas scrubbing of acetylene,
the stream comprises an organic solvent other than hydrocarbons,
the stream comprises up to 20% by weight of vinylacetylene and up to 10% by weight of acetylene, based on the weight of butadiyne, and
the stream comprises from 1 to 10% by weight of butadiyne, based on the total weight of the stream.
2. The process according to claim 1 , wherein the platinum group metal is palladium and the inorganic metal oxide is one or more selected from the group consisting of aluminum oxide, titanium dioxide, zirconium oxide, and silicon dioxide.
3. The process according to claim 1 , wherein the butadiyne is present in an organic solvent other than hydrocarbons.
4. The process according to claim 3 , wherein the organic solvent is one or more selected from the group consisting of N-methylpyrrolidone, dimethylformamide, acetone, furfurol, acetonitrile, and dimethylacetamide.
5. The process according to claim 1 , wherein the hydrogenation of butadiyne is performed in a fixed bed.
6. The process according to claim 1 , wherein the support has a porosity of from 0.3 to 0.6 ml/g.
7. The process according to claim 1 , wherein the weight ratio of recycle stream to feed stream is from 3 to 10.
8. The process according to claim 1 , wherein the support has a median pore volume of from 5 to 20 nm.