Materials comprising deaggregated diamond nanoparticles
Heat-transfer fluids and lubricating fluids comprising deaggregated diamond nanoparticles are described herein. Also described are composites comprising deaggregated diamond nanoparticles, and methods of making such composites. Method of using deaggregated diamond nanoparticles, for example, to improve the properties of materials such as thermal conductivity and lubricity are also disclosed.
1. A heat-transfer fluid comprising deaggregated diamond nanoparticles, the deaggregated diamond nanoparticles having an average particle size of less than about 10 nm.
2. The heat-transfer fluid of claim 1 , wherein the deaggregated diamond nanoparticles are oxidized.
3. The heat-transfer fluid of claim 1 , wherein the heat transfer fluid comprises at least one of ethylene glycol, mineral oil, dimethyl polysiloxane, a biphenol, a triphenol, or a combination thereof.
4. The heat-transfer fluid of claim 1 , wherein the heat transfer fluid comprises greater than about 1% (wt/wt) deaggregated diamond nanoparticles.
5. The heat-transfer fluid of claim 3 , wherein the heat transfer fluid comprises greater than about 3% (wt/wt) deaggregated diamond nanoparticles.
6. The heat-transfer fluid of claim 1 , wherein the fluid is shelf-stable for at least about 30 days.
7. A lubricating fluid comprising deaggregated diamond nanoparticles, the deaggregated diamond nanoparticles having an average particle size of less than about 10 nm.
8. The lubricating fluid of claim 7 , wherein the deaggregated diamond nanoparticles are oxidized.
9. The lubricating fluid of claim 7 , wherein the lubricating fluid comprises at least one of ethylene glycol, mineral oil, dimethyl polysiloxane, hydrocarbons, or a combination thereof.
10. The lubricating fluid of claim 7 , comprising greater than about 1% (wt/wt) deaggregated diamond nanoparticles.
11. The lubricating fluid of claim 10 , comprising greater than about 3% (wt/wt) deaggregated diamond nanoparticles.
12. The lubricating fluid of claim 7 , wherein the fluid is shelf-stable for at least about 30 days.
13. A method of increasing the thermal conductivity of a fluid, comprising incorporating deaggregated diamond nanoparticles into the fluid, the deaggregated diamond nanoparticles having an average particle size of less than about 10 nm.
14. The method of claim 13 , wherein the deaggregated diamond nanoparticles are oxidized.
15. The method of claim 13 , wherein the thermal conductivity is increased by at least about 1% compared to the same fluid without deaggregated diamond nanoparticles.
16. The method of claim 13 , wherein the thermal conductivity is increased by at least about 5% compared to the same fluid without deaggregated diamond nanoparticles.
17. The method of claim 13 , wherein the thermal conductivity is increased by at least about 10% compared to the same fluid without deaggregated diamond nanoparticles.
18. A method of increasing the lubricity of a fluid, comprising incorporating deaggregated diamond nanoparticles into the fluid, the deaggregated diamond nanoparticles having an average particle size of less than about 10 nm.
19. The method of claim 18 , wherein the deaggregated diamond nanoparticles are oxidized.
20. The method of claim 18 , wherein the coefficient of friction of the fluid is reduced by at least about 10%.
21. The method of claim 18 , wherein the wear rate of the fluid is reduced by at least about 5%.
22. The method of claim 18 , wherein the seizure load of the fluid is increased by at least about 10%.
23. A liquid composite comprising deaggregated diamond nanoparticles, the deaggregated diamond nanoparticles having an average particle size of less than about 10 nm.