Method of forming a magnetoresistive random-access memory device

Inventor: Joydeep Guha (Fremont, CA)
Assignee: Lam Research Corporation
H01L43/12H01L29/82
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,895,323
App. No.
13/715,971
Granted
Nov 25, 2014
Kind
B2
Abstract

A method for forming MRAM (magnetoresistive random access memory) devices is provided. A bottom electrode assembly is formed. A magnetic junction assembly is formed, comprising, depositing a magnetic junction assembly layer over the bottom electrode assembly, forming a patterned mask over the magnetic junction assembly layer, etching the magnetic junction assembly layer to form the magnetic junction assembly with gaps, gap filling the magnetic junction assembly, and planarizing the magnetic junction assembly. A top electrode assembly is formed.

Claims (74)

1. A method for forming MRAM (magnetoresistive random access memory) devices, comprising:

forming a bottom electrode assembly;

forming a magnetic junction assembly, wherein the forming the magnetic junction assembly comprises:

depositing a magnetic junction assembly layer over the bottom electrode assembly, wherein the depositing the magnetic junction assembly layer comprises:

depositing a bottom magnetic layer over the bottom electrode assembly;

depositing a tunnel oxide layer over the bottom magnetic layer; and

depositing a top magnetic layer over the tunnel oxide layer;

forming a patterned mask over the magnetic junction assembly layer;

etching the magnetic junction assembly layer to form the magnetic junction assembly with gaps;

gap filling the magnetic junction assembly; and

planarizing the magnetic junction assembly; and

forming a top electrode assembly.

2. The method, as recited in claim 1 , wherein the forming the bottom electrode assembly, comprises:

depositing a bottom electrode assembly layer over a substrate;

forming a patterned mask over the bottom electrode assembly layer;

etching the bottom electrode assembly layer to form the bottom electrode assembly with gaps;

gap filling the gaps in the bottom electrode assembly; and

planarizing the bottom electrode assembly.

3. The method, as recited in claim 2 , wherein the forming the top electrode assembly, comprises:

depositing a top electrode assembly layer over the planarized magnetic junction assembly;

forming a patterned mask over the top electrode assembly layer;

etching the top electrode assembly layer to form the top electrode assembly with gaps; and

gap filling the top electrode assembly.

4. The method, as recited in claim 3 , further comprising:

stripping the patterned mask over the bottom electrode assembly; and

stripping the patterned mask over the magnetic junction assembly.

5. The method, as recited in claim 4 , wherein the etching the bottom electrode assembly layer is performed by a dry etch.

6. The method, as recited in claim 5 , wherein the etching the magnetic junction assembly layer is performed by a dry etch.

7. The method, as recited in claim 6 , wherein the etching the top electrode assembly layer is performed by a dry etch.

8. The method, as recited in claim 7 , wherein the gap filling fills the gaps with a dielectric material.

9. The method, as recited in claim 2 , wherein the etching the bottom electrode assembly layer is performed by a dry etch.

10. The method, as recited in claim 1 , wherein the etching the magnetic junction assembly layer is performed by a dry etch.

11. The method, as recited in claim 1 , wherein the gap filling fills the gaps with a dielectric material.

12. The method, as recited in claim 1 , wherein the forming the top electrode assembly, comprises:

depositing a top electrode assembly layer over the magnetic junction assembly;

forming a patterned mask over the top electrode assembly layer;

etching the top electrode assembly layer to form the top electrode assembly with gaps; and

gap filling the top electrode assembly.

13. The method, as recited in claim 11 , wherein the etching the top electrode assembly layer is performed by a dry etch.

14. A method for forming MRAM (magnetoresistive random access memory) devices, comprising:

forming a bottom electrode assembly, comprising:

depositing a bottom electrode assembly layer over a substrate;

forming a patterned mask over the bottom electrode assembly layer;

etching the bottom electrode assembly layer to form the bottom electrode assembly with gaps;

gap filling the gaps in the bottom electrode assembly;

stripping the patterned mask over the bottom electrode assembly; and

planarizing the bottom electrode assembly;

forming a magnetic junction assembly, comprising

depositing a magnetic junction assembly layer over the planarized bottom electrode assembly, wherein the depositing the magnetic junction assembly layer comprises:

depositing a bottom magnetic layer over the bottom electrode assembly;

depositing a tunnel oxide layer over the bottom magnetic layer; and

depositing a top magnetic layer over the tunnel oxide layer;

forming a patterned mask over the magnetic junction assembly layer;

etching the magnetic junction assembly layer to form the magnetic junction assembly with gaps;

gap filling the magnetic junction assembly;

stripping the patterned mask over the magnetic junction assembly; and

planarizing the magnetic junction assembly; and

forming a top electrode assembly, comprising

depositing a top electrode assembly layer over the planarized magnetic junction assembly;

forming a patterned mask over the top electrode assembly layer;

etching the top electrode assembly layer to form the top electrode assembly with gaps; and

gap filling the top electrode assembly.

15. A magnetoresistive random access memory device formed by the method, comprising:

forming a bottom electrode assembly;

forming a magnetic junction assembly, wherein the forming the magnetic junction assembly comprises:

depositing a magnetic junction assembly layer over the bottom electrode assembly, wherein the depositing the magnetic junction assembly layer comprises:

depositing a bottom magnetic layer over the bottom electrode assembly;

depositing a tunnel oxide layer over the bottom magnetic layer; and

depositing a top magnetic layer over the tunnel oxide layer;

forming a patterned mask over the magnetic junction assembly layer;

etching the magnetic junction assembly layer to form the magnetic junction assembly with gaps;

gap filling the magnetic junction assembly; and

planarizing the magnetic junction assembly; and

forming a top electrode assembly.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Oct 18, 2013
From: GUHA, JOYDEEP
To: LAM RESEARCH CORPORATION
Reel/Frame 031439/0320 →
Continuity (2)
Provisional Application 61577377 · Dec 19, 2011
Related Publication 20130154037A1 · Jun 20, 2013