IP Library › Granted Patent US 8,951,600
Granted Patent B2
US 8,951,600 · App. 13/689,167 · Granted Feb 10, 2015

Method for producing electrode for solid battery

Inventors: Hiroki Kubo (Toyota, JP); Yuichi Hashimoto (Toyota, JP)
Assignee: Toyota Jidosha Kabushiki Kaisha
H01M4/1397Y02E60/122H01M10/052H01M10/0562H01M4/139
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 8,951,600
App. No.
13/689,167
Granted
Feb 10, 2015
Kind
B2
Abstract

The present invention provides a method for producing an electrode for a solid battery which can improve battery performance. The method for producing an electrode for a solid battery comprises the steps of: mixing an active material, a solid electrolyte, a binder, and a solvent to make a slurry-form electrode composition; applying the slurry-form electrode composition made; and drying the slurry-form electrode composition applied, wherein the solvent includes a good solvent for the binder and a poor solvent for the binder.

Claims (11)

1. A method for producing an electrode for a solid battery comprising the steps of:

mixing an active material, a solid electrolyte, a binder, and a solvent to make a slurry-form electrode composition;

applying the slurry-form electrode composition that has been made; and

drying the slurry-form electrode composition that has been applied,

wherein the solvent includes a good solvent for the binder and a poor solvent for the binder,

wherein the good solvent defines a solubility for the binder of 5% or more and the poor solvent defines a solubility for the binder of less than 0.1%, and

wherein the poor solvent is selected from a group consisting

of n-Butyl n-Butyrate and anisole.

2. The method for producing said electrode for the solid battery according to claim 1 , wherein the good solvent has a boiling point lower than that of the poor solvent.

3. The method for producing said electrode for the solid battery according to claim 2 , wherein the solid electrolyte is a sulfide solid electrolyte.

4. The method for producing an electrode for a solid battery according to claim 1 , wherein the solid electrolyte is a sulfide solid electrolyte.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Dec 14, 2012
From: KUBO, HIROKI; HASHIMOTO, YUICHI
To: TOYOTA JIDOSHA KABUSHIKI KAISHA
Reel/Frame 029470/0737 →
Priority Claims (1)
JP 2011-266035 · Dec 5, 2011 · national
Continuity (1)
Related Publication 20130142943A1 · Jun 6, 2013