IP Library › Granted Patent US 9,016,978
Granted Patent B2
US 9,016,978 · App. 13/770,342 · Granted Apr 28, 2015

Asphalt sealer for surface crack repair

Inventor: Jeff Konczak (Alpena, MI)
Assignee: SuperGrout Products LLC
C09D195/00E01C23/026C08L2555/34C08L2555/52E01C7/187E01C11/005
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,016,978
App. No.
13/770,342
Granted
Apr 28, 2015
Kind
B2
Abstract

A method of repairing cracks in a paved surface includes identifying at least one crack in the surface that needs to be repaired. The crack is then filled with an asphalt sealer including approximately 40-55% by weight of slag sand.

Claims (15)

1. A method of repairing cracks in a paved surface comprising:

Identifying at least one crack in a paved surface to be repaired;

Substantially filling said at least one crack with an asphalt sealer including approximately 40-55% by weight of an air cooled blast furnace sand; whereby said asphalt sealer can withstand large temperature deviations without failing;

partially filing said crack with a grout material; and placing said asphalt sealer on said grout material.

2. The method of claim 1 , wherein said asphalt sealer includes approximately 48% by weight of said air cooled blast furnace sand.

3. The method of claim 1 , wherein said grout material, includes class F fly ash in a range of approximately 0 to 30% by weight of said grout material and cement kiln dust in a range of approximately 50 to 90% by weight of said grout material.

4. The method of claim 1 , wherein said paved surface is an asphalt surface.

5. A method of repairing cracks in a paved surface, comprising:

identifying at least one crack in a paved surface to be repaired;

at least partially filling said at least one crack is an asphalt sealer including approximately 40-55% by weight of an air cooled blast furnace sand, whereby said asphalt sealer can withstand large temperature deviations without failing; and

partially filling said crack with a grout material; and

placing said asphalt sealer on said grout material.

6. The method of claim 5 , wherein said asphalt sealer includes approximately 48% by weight of said air cooled blast furnace sand.

7. The method of claim 5 , wherein said grout material includes class F fly ash in a range of approximately 0-30% by weight of said grout material and cement kiln dust in a range of approximately 50-90% by weight of said grout material.

8. The method of claim 5 , wherein said paved surface is an asphalt surface.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 22, 2013
From: KONCZAK, JEFF
To: SUPERGROUT PRODUCTS, LLC
Reel/Frame 029858/0421 →
Continuity (2)
Provisional Application 61600289 · Feb 17, 2012
Related Publication 20130216306A1 · Aug 22, 2013