Process to produce lithium carbonate directly from the aluminosilicate mineral
View Patent ↗Process for obtaining lithium carbonate directly from the mineral containing silicium, aluminum, lithium and other metal oxides without the need to dissolve previously all oxides in sulphuric acid or alkaline hydroxides at high temperatures and pressures, by using carbon dioxide and water at supercritical or near supercritical conditions acting directly on the fine powder of the mineral.
1. A process for obtaining lithium carbonate comprising reacting minerals selected from the group consisting of spodumene, petalite or lepidolite, with water and carbon dioxide at a pressure of 10 to 200 bar and a temperature of 100 to 200 C;
Separating after the reacting a solid portion from a liquid portion;
Evaporating the liquid portion; and
Obtaining as the residue of the evaporating lithium carbonate;
Wherein the minerals have been previously crushed to a particle size of less than 50 microns and the reacting is performed in the absence of sulfuric acid or sodium hydroxide.
2. The process of claim 1 wherein the temperature is 150 to 180 C.
3. The process of claim 1 wherein the pressure is 30 to 50 bar.
4. The process of claim 1 wherein the reacting is performed for 1 to 6 hours.
5. The process of claim 1 wherein a ratio of the minerals to water is 1-3:20.
6. The process of claim 1 wherein the pressure of carbon dioxide is kept constant during the reacting step by adding more carbon dioxide.
7. The process of claim 1 wherein prior to evaporating comprises cooling down the mixture, depressurizing, filtered or decanted and then evaporating to dryness.