Method and a system for gold extraction with halogens

Inventors: Jean-Marc Lalancette (Sherbrooke, CA); Bertrand Dubreuil (Trois-Rivieres, CA); David Lemieux (Thetford Mines, CA)
Assignee: DUNDEE, TECHNOLOGIES DURABLES INC.
C22B11/06
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,051,626
App. No.
13/418,863
Granted
Jun 9, 2015
Kind
B2
Abstract

The invention relates to a method for the extraction of precious metals, using halogens. It has been found that introducing halogens in the reactor in the form of hypohalites rather than free halogens simplified greatly the recycling of halogens by electrolysis. It increases the rate of addition of the halogens and significantly reduces secondary reactions with base metals such as iron. Operating under acidic conditions, the gold recovery has been found as high with hypochlorite as with elemental chlorine, with an active chlorine to ore ratio reduced by a factor of two to five.

Claims (11)

1. In a method for extracting precious metals from ore using halogens:

adding a mixture of hypohalites to an acidic slurry of the ore, a pH of the slurry being comprised in a range between 0.5 and 3, under an oxido-reduction potential in a range comprised between about 0.7 and about 1.2 V vs a Ag/AgCl reference electrode;

filtering to collect a pregnant solution;

treating the pregnant solution to separate the precious metals from a barren salt brine; and

recycling halogens from the barren salt brine in the form of hypohalites formed by electrolysis of the barren salt brine in a diaphragm-less cell.

2. The method of claim 1 , wherein the pH of the slurry is about 1.5.

3. The method of claim 2 , wherein the oxido-reduction potential is about 0.85 V.

4. The method of claim 1 , wherein said adding a mixture of hypohalites comprises adding a mixture of hypohalites in a range comprised between about 0.5 and about 2 weight percent of the ore.

5. The method of claim 1 , wherein the slurry of the ore has a temperature of about 40° C.

6. The method of claim 1 , comprising adding the hypohalites at a concentration of 1.5 weight % of the ore.

7. The method of claim 1 , wherein said precious metals are gold and silver.

Assignments (3)
CHANGE OF ADDRESS Recorded Oct 6, 2016
From: DUNDEE SUSTAINABLE TECHNOLOGIES INC./DUNDEE, TECHNOLOGIES DURABLES INC.
To: DUNDEE SUSTAINABLE TECHNOLOGIES INC./DUNDEE, TECHNOLOGIES DURABLES INC.
Reel/Frame 040332/0863 →
CHANGE OF NAME Recorded Feb 12, 2014
From: NICHROMET EXTRACTION INC.
To: DUNDEE, TECHNOLOGIES DURABLES INC.
Reel/Frame 032251/0040 →
NUNC PRO TUNC ASSIGNMENT Recorded Mar 13, 2012
From: LALANCETTE, JEAN-MARC; DUBREUIL, BERTRAND; LEMIEUX, DAVID
To: NICHROMET EXTRACTION INC.
Reel/Frame 027854/0836 →
Continuity (2)
Provisional Application 61539517 · Sep 27, 2011
Related Publication 20130074655A1 · Mar 28, 2013