Friction stir welding method

Inventors: Nobushiro Seo (Shizuoka, JP); Hisashi Hori (Shizuoka, JP)
Assignee: NIPPON LIGHT METAL COMPANY, LTD.
B23K20/1245B23K20/122B23K20/128B23K20/1265
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,095,927
App. No.
14/237,998
Granted
Aug 4, 2015
Kind
B2
Abstract

The invention aims at providing a friction stir welding method which can achieve joining a butting portion to a deep location therein by reducing the load on the friction stirring device. The friction stir welding method for joining two metal members ( 1 ) using a primary joining rotary tool (F) with a stirring pin (F 2 ) includes a primary joining process in which a rotating stirring pin (F 2 ) is moved to the butting portion formed by butting the metal members ( 1 ) against each other and friction stir welding is carried out. In the primary joining process, only the stirring pin (F 2 ) is brought into contact with the metal members ( 1 ).

Claims (26)

1. A method of friction stir welding for joining two metal members together using a rotary tool including a stirring pin, comprising

a butting step for butting the metal members against one another at corresponding flat surfaces to form a butting portion;

a primary joining step for inserting the stirring pin in a rotating state into the butting portion of the metal members and carrying out friction stir welding with only the stirring pin contacting with the metal members, wherein a depressed groove is formed on a front surface of a plasticized region during the primary joining step; and

a repairing step for reforming the depressed groove, disposing a refill member at the reformed depressed groove and joining the refill member to the metal members.

2. The method of friction stir welding according to claim 1 , comprising

a provisional joining step for joining the metal members together provisionally before carrying out the primary joining step.

3. The method of friction stir welding according to claim 1 , comprising

disposing a tab member in a vicinity of the butting portion and forming a pilot hole in the tab member, and then inserting the stirring pin into the pilot hole to carry out the primary joining step.

4. A method of friction stir welding for joining two metal members together using a rotary tool including a stirring pin, comprising:

a butting step for butting the metal members against one another with an angle to form a butting portion; and

a first primary joining step for inserting the stirring pin in a rotating state into an inner corner of the metal members and carrying out friction stir welding on the butting portion with only the stirring pin contacting with the both metal members,

wherein a spiral groove is formed on an outer circumferential surface of the stirring pin, and

a pin angle between a rotation center axis of the rotary tool and the outer circumferential surface is 9.5 to 27.6 degrees.

5. A method of friction stir welding for joining two metal members together using a rotary tool including a stirring pin, comprising:

a butting step for butting the metal members against one another with an angle to form a butting portion;

a first primary joining step for inserting the stirring pin in a rotating state into an inner corner of the metal members and carrying out friction stir welding on the butting portion with only the stirring pin contacting with the both metal members; and a second primary joining step for inserting the stirring pin in a rotating state into a surface forming an outer corner of the metal members and carrying out friction stir welding on the butting portion with only the stirring pin contacting with the both metal members.

6. The method of friction stir welding according to claim 5 , wherein a plasticized region formed in the first primary joining step and a plasticized region formed in the second primary joining step overlap each other.

7. The method of friction stir welding according to claim 5 , wherein

in the butting step, a side surface of one metal member is butted against an end surface of the other metal member, with an angle α at an inner corner formed by the side surface of the one metal member and a side surface of the other metal member, and

in the first primary joining step, a rotation center axis of the rotary tool inserted into an intersection line of the side surfaces is positioned between an imaginary reference surface and the side surface of the one metal member, the imaginary reference surface passing through the intersection line and forming an angle α/2 with the side surfaces.

8. A method of friction stir welding for joining two metal members together using a rotary tool including a stirring pin, comprising:

a butting step for butting the metal members against one another with an angle to form a butting portion;

a first primary joining step for inserting the stirring pin in a rotating state into an inner corner of the metal members and carrying out friction stir welding on the butting portion with only the stirring pin contacting with the both metal members; and a provisional joining step for, before the first primary joining step, inserting a rotary tool in a rotating state into a surface forming an outer corner of the metal members and joining the butting portion provisionally.

9. The method of friction stir welding according to claim 8 , wherein in the first primary joining step, the plasticized region formed in the first primary joining step overlaps the plasticized region formed in the provisional joining step.

10. The method of friction stir welding according to claim 4 , comprising

a step for carrying out buildup welding on a plasticized region formed in the first primary joining step.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Feb 10, 2014
From: SEO, NOBUSHIRO; HORI, HISASHI
To: NIPPON LIGHT METAL COMPANY, LTD.
Reel/Frame 032183/0108 →
Priority Claims (2)
JP 2011-179586 · Aug 19, 2011 · national
JP 2011-187916 · Aug 30, 2011 · national
Continuity (1)
Related Publication 20140166731A1 · Jun 19, 2014