Cement compositions for cementing in confined locales and methods for use thereof
When conducting cementing operations within confined locales, such as the annular space within a wellbore, it can sometimes be difficult to successfully deliver an uncured cement composition to a desired location. Cementing methods can comprise: providing a cement composition comprising a cement and a property control package, the property control package comprising: a filtration control agent; a friction reducer; and a setting accelerator; introducing the cement composition into a mineral exploration wellbore; and setting the cement composition in the wellbore.
1. A method comprising:
providing a cement composition comprising a cement and a property control package, the property control package comprising:
a filtration control agent;
a friction reducer; and
a setting accelerator;
introducing the cement composition into a mineral exploration wellbore, the mineral exploration wellbore penetrating a mineral formation containing a mineral deposit;
wherein the mineral deposit comprises a metal or a metal ore;
setting the cement composition in the wellbore; and
mapping the mineral deposit, or harvesting the mineral deposit from the mineral formation.
2. The method of claim 1 , wherein the wellbore comprises an annular structure having an annular space ranging between about 3 mm and about 10 mm.
3. The method of claim 2 , wherein the cement composition is set in the annular space.
4. The method of claim 1 , wherein the cement composition is set in a lost circulation zone.
5. The method of claim 1 , wherein the setting accelerator comprises a substance selected from the group consisting of a calcium salt, a sodium salt, an amine, and any combination thereof.
6. The method of claim 5 , wherein the setting accelerator comprises a calcium salt or a sodium salt selected from the group consisting of calcium chloride, calcium sulfate, calcium nitrate, calcium nitrite, calcium formate, sodium thiocyanate, sodium sulfate, sodium chloride, and any combination thereof.
7. The method of claim 1 , wherein the filtration control agent comprises a cellulose derivative, a latex polymer, or a copolymer of acrylamido-2-methyl-2-propanesulfonic acid and N,N-dimethylacrylamide.
8. The method of claim 1 , wherein the friction reducer comprises a friction reducing polymer.
9. The method of claim 8 , wherein the friction reducing polymer comprises a reaction product of acetone, formaldehyde, and sulfurous acid or a sulfurous acid salt.
10. The method of claim 1 , wherein the cement comprises at least one cement selected from the group consisting of Portland cement, blast furnace slag cement, fly ash cement, trass cement, Pozzolan-lime cement, slag-lime cement, supersulfated cement, gypsum cement, phosphate cement, silica cement, calcium aluminate cement, calcium sulfoaluminate cement, and any combination thereof.
11. The method of claim 1 , wherein providing the cement composition comprises combining a dry mixture of the property control package with water and then adding the cement, thereby forming a cement slurry.
12. The method of claim 1 , wherein the cement composition comprises about 0.3% to about 1% friction reducer by weight of cement.
13. The method of claim 1 , wherein the cement composition comprises about 0.3% to about 1% filtration control agent by weight of cement.
14. The method of claim 1 , wherein the cement composition comprises about 1% to about 4% setting accelerator by weight of cement.
15. A method comprising:
providing a cement composition comprising a cement and a property control package, the property control package comprising:
about 0.3% to about 1% filtration control agent by weight of cement;
about 0.3% to about 1% friction reducer by weight of cement; and
about 1% to about 4% setting accelerator by weight of cement;
introducing the cement composition into a mineral exploration wellbore penetrating a mineral formation containing a mineral deposit;
wherein the mineral deposit comprises a metal or a metal ore;
setting the cement composition in the wellbore; and
mapping the mineral deposit, or harvesting the mineral deposit from the mineral formation.
16. The method of claim 15 , wherein the wellbore comprises an annular structure having an annular space ranging between about 3 mm and about 10 mm.
17. The method of claim 15 , wherein the setting accelerator comprises a substance selected from the group consisting of a calcium salt, a sodium salt, an amine, and any combination thereof.
18. The method of claim 17 , wherein the setting accelerator comprises a calcium salt or a sodium salt selected from the group consisting of calcium chloride, calcium sulfate, calcium nitrate, calcium nitrite, calcium formate, sodium thiocyanate, sodium sulfate, sodium chloride, and any combination thereof.
19. The method of claim 15 , wherein the filtration control agent comprises a cellulose derivative, a latex polymer, or a copolymer of acrylamido-2-methyl-2-propanesulfonic acid and N,N-dimethylacrylamide.
20. The method of claim 15 , wherein the friction reducer comprises a friction reducing polymer.
21. The method of claim 20 , wherein the friction reducing polymer comprises a reaction product of acetone, formaldehyde, and sulfurous acid or a sulfurous acid salt.