IP Library Granted Patent US 9,117,788
Granted Patent B2
US 9,117,788 · App. 13/184,723 · Granted Aug 25, 2015

Heat sink device and method of repairing semiconductor device

Inventors: Tsuyoshi Yamamoto (Kawasaki, JP); Naoaki Nakamura (Kawasaki, JP); Rie Takada (Kawasaki, JP); Kenichiro Tsubone (Kawasaki, JP); Yasuhide Kuroda (Kawasaki, JP); Harumi Yagi (Kawasaki, JP)
Assignee: FUJITSU LIMITED
H01L23/36H01L2224/16225H01L2224/73253Y10T29/49721
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,117,788
App. No.
13/184,723
Granted
Aug 25, 2015
Kind
B2
Abstract

A method of repairing a semiconductor device includes turning a press member to apply pressure on an electronic component which is mounted on a substrate. A heat sink which is provided on the electronic component via a bonding layer is thus displaced with respect to the electronic component in a transverse direction. The heat sink is removed from the electronic component by shearing the bonding layer with the press member.

Claims (5)

1. A method of repairing a semiconductor device including an electronic component, a heat sink provided over the electronic component via a bonding layer, and a press member that moves in the heat sink towards the electronic component, the method comprising:

moving the press member, in a perpendicular or diagonal direction with respect to an upper end of the electronic component, towards the electronic component until a conical portion of the press member comes into contact with the upper end of the electronic component;

turning the press member to apply pressure and to move the heat sink in a horizontal direction across the bonding layer on the electronic component; and

removing the heat sink from the electronic component,

wherein the movement of the heat sink on the electronic component reduces a shearing force in the bonding layer and reduces a bonding force of the bonding layer to separate the heat sink from the electronic component.

Assignments (1)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Jul 18, 2011
From: YAMAMOTO, TSUYOSHI; NAKAMURA, NAOAKI; TAKADA, RIE; TSUBONE, KENICHIRO; KURODA, YASUHIDE; YAGI, HARUMI
To: FUJITSU LIMITED
Reel/Frame 026607/0975 →
Priority Claims (1)
JP 2010-169067 · Jul 28, 2010 · national
Continuity (1)
Related Publication 20120024512A1 · Feb 2, 2012