Multilayer coating for paper based substrate

Inventors: Julia F. Hartmann (Lachen, CH); Jouko T. Vyorykka (Richterswil, CH)
Assignee: Dow Global Technologies LLC
D21H19/82D21H19/385D21H19/40D21H19/50D21H19/54D21H21/16Y10T428/24942Y10T428/277
View Patent ↗
Loading inventors, assignments & file history…
Monitor This Case
Get email alerts when status or documents change.
Order Certified Copies
Most orders are placed with the USPTO same day — all within 24 business hours.
Order via The Patent Place →
Pre-filled with this patent's details
Quick Facts
Patent No.
US 9,200,409
App. No.
13/964,423
Granted
Dec 1, 2015
Kind
B2
Abstract

Embodiments include a coated paper or paperboard with a multilayer coating and methods of forming a coated paper or paperboard with the multilayer coating. The multilayer coating includes a first water vapor barrier layer, a biopolymer barrier layer, and a second water vapor barrier layer and provides the paperboard with improved oil and grease resistant properties, oxygen barrier properties, and water vapor barrier properties.

Claims (31)

1. A coated paper or paperboard, comprising:

a base paper having a first major surface;

a multilayer coating over the first major surface, where the multilayer coating has a total dry coat weight of 10 g/m 2 or less and includes:

a first water vapor barrier layer formed with a synthetic latex;

a biopolymer barrier layer on the first water vapor barrier layer, where the biopolymer barrier layer includes a first biopolymer barrier layer on the first vapor water barrier layer and a second biopolymer barrier layer on the first biopolymer barrier layer so that the first biopolymer barrier layer and the second biopolymer barrier layer are between the first barrier layer and the second barrier layer, and wherein each of the first biopolymer barrier layer and the second biopolymer barrier layer have a dry coat weight of 2 g/m 2 or less, and wherein the biopolymer barrier layer includes a biopolymer and 2.5 to about 50 weight parts of a plasticizer for every 100 dry weight parts of the biopolymer;

a second water vapor barrier layer on the biopolymer barrier layer, where the second water vapor barrier layer is formed with a latex, wherein the biopolymer barrier layer is positioned between the first water vapor barrier layer and the second water vapor barrier layer to protect the biopolymer barrier layer from water absorption; and

where the coated paper or paper board has a Kit Rating Number of at least 12 and prevents penetration of canola oil at 60° C. for 24 hours through the multilayer coating and the base paper after creasing and folding.

2. The coated paper or paperboard of claim 1 , where the plasticizer is an ethylene-acrylic acid copolymer.

3. The coated paper or paper board of claim 1 , where the first water vapor barrier layer and the second water vapor barrier layer has a combined dry coat weight of 6 g/m 2 or less and each of the first water vapor barrier layer and the second water vapor barrier layer is formed with a coating composition that consists of the latex, an emulsifier and about 0 to about 100 weight parts pigment for every 100 dry weight parts of latex.

4. The coated paper or paper board of claim 1 , where the coated paper or paper board has an oxygen permeability of not higher than 100 cm 3 /(m 2 *24 hours) at 23° C., 760 mmHg, and 50% relative humidity.

5. The coated paper or paperboard of claim 1 , where the synthetic latex of the first water vapor barrier layer is selected from a group including styrene-butadiene latexes, styrene-acrylate latexes, styrene-acrylic latexes, styrene maleic anhydrides, styrene-butadiene acrylonitrile latexes, styrene-acrylate-vinyl acrylonitrile latexes, vinyl acetate latexes, vinyl acetate-butyl acrylate latexes, vinyl acetate-ethylene latexes, acrylic latexes, vinyl acetate-acrylate latexes, acrylate copolymers, vinylidene-containing latexes, vinylidene chloride latexes, vinyl chloride containing latexes, and a mixtures thereof.

6. The coated paper or paperboard of claim 1 , where the second water vapor barrier layer is formed with a synthetic latex.

7. The coated paper or paperboard of claim 1 , where the biopolymer barrier layer includes

about 10 to about 100 weight parts of a pigment for every 100 dry weight parts of biopolymer.

8. The coated paper or paperboard of claim 7 , where the biopolymer is selected from the group consisting of a starch, a modified starch, a chitosan, a polysaccharide, a protein, a gelatin, a bio-polyesters and modifications and mixtures thereof.

9. The coated paper or paperboard of claim 7 , where the pigment is a selected from the group consisting of a clay, an exfoliated natural layered silicate, a partially exfoliated natural layered silicate, an exfoliated synthetic layered silicate, a partially exfoliated synthetic layered silicate, calcium carbonates, talc and mixtures thereof.

10. A method of forming a coated paper or paper board, comprising:

applying a multilayer coating to a first major surface of a base paper, where the multilayer coating has a total dry coat weight of 10 g/m 2 or less and includes:

a first water vapor barrier layer formed with a synthetic latex;

a biopolymer barrier layer on the first water vapor barrier layer, where the biopolymer barrier layer includes a first biopolymer barrier layer on the first vapor water barrier layer and a second biopolymer barrier layer on the first biopolymer barrier layer so that the first biopolymer barrier layer and the second biopolymer barrier layer are between the first barrier layer and the second barrier layer, and wherein each of the first biopolymer barrier layer and the second biopolymer barrier layer have a dry coat weight of 2 g/m 2 or less, and wherein the biopolymer barrier layer includes a biopolymer and 2.5 to about 50 weight parts of a plasticizer for every 100 dry weight parts of the biopolymer;

a second water vapor barrier layer on the biopolymer barrier layer, where the second water vapor barrier layer is formed with a latex, wherein the biopolymer barrier layer is positioned between the first water vapor barrier layer and the second water vapor barrier layer to protect the biopolymer barrier layer from water absorption; and

drying the multilayer coating on the first major surface of the base paper, where the coated paper or paper board has a Kit Rating Number of at least 12 and prevents penetration of canola oil at 60° C. for 24 hours through the multilayer coating and the base paper after creasing and folding.

11. The method of claim 10 , where applying a multilayer coating includes applying each of the first and second water vapor barrier layers to form the first barrier layer having a coat weigh of 3 g/m 2 or less, and to form the second water vapor barrier layer having a coat weigh of 3 g/m 2 or less, where each of the first water vapor barrier layer and the second water vapor barrier layer is formed with a coating composition that consists of the latex, an emulsifier and about 0 to about 100 weight parts pigment for every 100 dry weight parts of latex.

12. The method of claim 10 , where each of the at least one biopolymer barrier layer is formed from a second coating composition that includes:

about 10 to about 100 weight parts of a pigment for every 100 dry weight parts of biopolymer.

13. The method of claim 10 , where applying the multilayer coating to the first major surface of the base paper includes simultaneously applying the multilayer coating to the first major surface of the base paper.

14. A coated paper or paperboard formed by the method of claim 10 .

15. The method of claim 10 , where applying a multilayer coating includes applying the first and second water vapor barrier layers and at least one biopolymer barrier layer to form the multilayer coating having a total dry coat weight of 10 g/m 2 or less.

16. The method of claim 15 , where applying a multilayer coating includes applying at least one biopolymer barrier layer to form a biopolymer barrier layer having a total dry coat weigh of 4 g/m 2 or less.

17. The method of claim 10 , where applying the multilayer coating includes applying a first biopolymer barrier layer on a first water barrier layer, and a second biopolymer barrier layer on the first biopolymer barrier layer so that the first biopolymer barrier layer and the second biopolymer barrier layer are between the first barrier layer and the second barrier layer.

18. The method of claim 17 , where each of the first biopolymer barrier layer and the second biopolymer barrier layer have a dry coat weight of 2 g/m 2 or less.

Assignments (4)
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 4, 2014
From: HARTMANN, JULIA F.; VYORYKKA, JOUKO T.
To: DOW EUROPE GMBH
Reel/Frame 034098/0290 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 4, 2014
From: DOW EUROPE GMBH
To: THE DOW CHEMICAL COMPANY
Reel/Frame 034098/0318 →
ASSIGNMENT OF ASSIGNOR'S INTEREST Recorded Nov 4, 2014
From: THE DOW CHEMICAL COMPANY
To: DOW GLOBAL TECHNOLOGIES INC.
Reel/Frame 034098/0395 →
CHANGE OF NAME Recorded Nov 4, 2014
From: DOW GLOBAL TECHNOLOGIES INC.
To: DOW GLOBAL TECHNOLOGIES LLC
Reel/Frame 034151/0744 →
Continuity (3)
Continuation 12998309
Provisional Application 61195843 · Oct 10, 2008