Flakes of ester mixtures and methods for their production
There is provided flakes of an ester mixture comprising bis-(hydroxyethyl)-terephthalate, dimers, tamers, tetramers, pentamers and higher oligomers of ethane-1,2-diol and terephthalate acid.
1. A method for producing flakes of an ester mixture comprising bis-(hydroxyethyl)-terephthalate, dimers, trimers, tetramers, pentamers and higher oligomers of ethane-1,2-diol and terephthalate acid, the method comprising the steps of:
a) flash evaporating ethane-1,2-diol from an ester mixture obtained from the glycolysis of PET (polyethylene terephthalate); and
b) producing flakes of the ester mixture of step (a), wherein the flakes are crystalline, free-flowing non-sticky, stable, storable and reusable.
2. The method according to claim 1 , wherein step (b) is conducted by quenching and solidifying the ester mixture of step (a).
3. The method according to claim 2 , wherein the quenching and solidifying is conducted using a rotary drum flaker.
4. The method according to claim 3 , wherein the rotary drum flaker in step (b) has a cooling medium at a temperature in the range from 8° C. to 90° C.
5. The method according to claim 3 , wherein the rotary drum flaker in step (b) has a cooling medium at a temperature in the range from 70° C. to 80° C.
6. A method for producing PET products from an ester mixture comprising bis-(hydroxyethyl)-terephthalate, dimers, trimers, tetramers, pentamers and higher oligomers of ethane-1,2-diol and terephthalate acid, the method comprising the steps of:
a) flash evaporating ethane-1,2-diol from an ester mixture obtained from the glycolysis of PET; and
b) polymerising the ester mixture from step (a) ready to produce PET products.
7. The method according to claim 1 or 6 wherein the free glycol content of the ester mixture after step (a) is less than about 12%.
8. The method according to claim 1 or 6 , wherein the free glycol content of the ester mixture after step (a) is about 2% or less.
9. The method according to claim 1 or 6 , wherein the ester mixture from step (a) has a diethylene glycol (DEG) content of about 2.5% or less.
10. The method according claim 1 or 6 , wherein the ester mixture from step (a) has a melting point at or below about 150° C.
11. The method according to claim 1 or 6 , wherein the flash evaporating is conducted at a temperature at or below 220° C.
12. The method according to claim 1 or 6 , wherein the flash evaporating is conducted at a temperature at in the range from 190° C. to 220° C.
13. The method according to claim 1 or 6 , wherein the flash evaporating is conducted at reduced pressure.
14. The method according to claim 13 , wherein the flash evaporating is conducted at a pressure in the range from 100 to 300 mbar (10 to 30 kPa).
15. The method according to claim 13 , wherein the flash evaporating is conducted at about 200 mbar (20 kPa).
16. Flakes of an ester mixture comprising bis-(hydroxyethyl)-terephthalate, dimers, trimers, tetramers, pentamers and higher oligomers of ethane-1,2-diol and terephthalate acid, wherein the flakes are crystalline, free-flowing non-sticky, stable, storable and reusable.
17. The flakes according to claim 16 , wherein the flakes have a melting point at or below 150° C.
18. The flakes according to claim 16 or 17 , wherein the flakes have a diethylene glycol content of about 2.5% or less.
19. The flakes according to claim 16 or 17 , wherein the flakes comprise about 2.5% or less diethylene glycol, 45 to 55% bis (hydroxyethyl) terephthalate, 25 to 35% dimers, 10 to 15% trimers, 3 to 8% tetramers, 1 to 2% pentamers and the balance comprising higher oligomers.
20. The flakes according to claim 16 or 17 , wherein the ester mixture comprises recycled esters obtained from the glycolysis of PET waste.
21. The method according to claim 1 , wherein the flakes have a melting point at or below 150° C.
22. The method according to claim 1 , wherein the flakes have a diethylene glycol content of about 2.5% or less.
23. The method according to claim 1 , wherein the flakes comprise about 2.5% or less diethylene glycol, 45 to 55% bis (hydroxyethyl) terephthalate, 25 to 35% dimers, 10 to 15% trimers, 3 to 8% tetramers, 1 to 2% pentamers and the balance comprising higher oligomers.